Abstract

Continuous destruction of the solid electrolyte interphase (SEI) on the graphite-based negative electrode during cycling operation is a significant degradation mechanism that raises safety concerns and limits the cycle life of LiNi 0.5 Mn 1.5 O 4 (LNMO)/graphite full-cells. Herein, we report on gassing phenomena which are typically concomitant with SEI destruction processes. Abrupt H 2 evolution is observed by differential electrochemical mass spectrometry and pressure measurements at the end of discharge. Using a lithium reference electrode reveals that the gassing, which intensifies with cycling, is caused by an increase in the anode potential. Lithium is irreversibly consumed upon SEI formation, but this loss is not compensated for by the intrinsic degradation of LNMO in the first cycle. When the potential of the anode on discharge increases above approximately 0.9 V, the SEI is instantly damaged, causing gas generation, and eventually capacity fade. We show that this (“mediator-free”) cross-talk phenomenon can be suppressed to various degrees by either using a precycled graphite electrode or an LNMO material having a higher initial irreversible capacity loss.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Battery and Electrochemistry Laboratory, Institute of Nanotechnology, Karlsruhe Institute of Technology, Hermann-von-Helmholtz-Platz 1, 76344 Eggenstein-Leopoldshafen, Germany

BASF SE, 67056 Ludwigshafen, Germany

Institute of Physical Chemistry, Justus-Liebig-University Giessen, Heinrich-Buff-Ring 17, 35392 Giessen, Germany

Funding

BASF International Network for Batteries and Electrochemistry

References (29)

Show source-provided references
1. 10.1016/j.elecom.2004.06.00510.1016/j.elecom.2004.06.005 ↗
2. 10.1149/1.183738610.1149/1.1837386 ↗
3. 10.1016/j.electacta.2012.12.06910.1016/j.electacta.2012.12.069 ↗
4. 10.1039/c3ee42981d10.1039/c3ee42981d ↗
5. 10.1149/2.0291510jes10.1149/2.0291510jes ↗
6. 10.1016/j.jpowsour.2014.12.13010.1016/j.jpowsour.2014.12.130 ↗
7. 10.1021/jp405158m10.1021/jp405158m ↗
8. Peled, E.; Golodnitsky, D.SEI on Lithium, Graphite, Disordered Carbons and Tin-Based Alloys. In Lithium-Ion Batteries: Solid-Electrolyte Interphase;Balbuena, P. B.; Wang, Y., Eds.Imperial College Press:London, 2004.10.1142/9781860946448_0001 ↗
9. 10.1016/j.jpowsour.2005.01.00610.1016/j.jpowsour.2005.01.006 ↗
10. 10.1002/(SICI)1521-4095(199807)10:10<725::AID-ADMA725>3.0.CO;2-Z10.1002/(SICI)1521-4095(199807)10:10<725::AID-ADMA725>3.0.CO;2-Z ↗
11. 10.1016/j.jpowsour.2005.07.05110.1016/j.jpowsour.2005.07.051 ↗
12. 10.1016/j.elecom.2014.04.00610.1016/j.elecom.2014.04.006 ↗
13. 10.1016/j.jpowsour.2014.10.19910.1016/j.jpowsour.2014.10.199 ↗
14. 10.1149/1.183842010.1149/1.1838420 ↗
15. 10.1149/1.296994710.1149/1.2969947 ↗
16. 10.1021/ac403317d10.1021/ac403317d ↗
17. 10.1021/jp501970j10.1021/jp501970j ↗
18. 10.1038/srep1562710.1038/srep15627 ↗
19. 10.1021/acs.analchem.5b0469610.1021/acs.analchem.5b04696 ↗
20. 10.1149/2.0191510jes10.1149/2.0191510jes ↗
21. 10.1149/1.183823510.1149/1.1838235 ↗
22. 10.1016/j.jpowsour.2016.03.04910.1016/j.jpowsour.2016.03.049 ↗
23. 10.1016/j.jpowsour.2014.09.18610.1016/j.jpowsour.2014.09.186 ↗
24. 10.1149/1.183834310.1149/1.1838343 ↗
25. 10.1021/acs.analchem.5b0123710.1021/acs.analchem.5b01237 ↗
26. 10.1006/jssc.2000.899010.1006/jssc.2000.8990 ↗
27. 10.1007/s10008-016-3362-910.1007/s10008-016-3362-9 ↗
28. 10.1149/2.1151605jes10.1149/2.1151605jes ↗
29. 10.1016/S0378-7753(01)00479-710.1016/S0378-7753(01)00479-7 ↗