Facile Route Toward Mechanically Stable Superhydrophobic Copper Using Oxidation–Reduction Induced Morphology Changes
Source abstract
Abstract
We present that the morphological change induced by an oxidation–reduction reaction can be effectively employed for easily producing superhydrophobic copper without any use of hydrophobic agents. By thermal oxidation of copper, needle-shaped copper oxide nanowires (NWs) were grown on the copper substrate. Subsequent reduction led to wavy copper NW structures, which exhibited superhydrophobic properties (contact angle of over 160° and sliding angle of less than 2°). We found that the water adhesion behavior on a surface could markedly vary with the shape of miniature structures of the surface, presumably due to the pinning effect. Microstructure, element, and surface analyses indicated that the outermost layer (∼Å) of the resulting copper NWs is mainly composed of Cu 2 O. Furthermore, the resulting superhydrophobic copper structures were observed to have good mechanical stability as well as chemical stability. This simple and scalable method could potentially be adopted in industry or academia where research on anticorrosion, antibiofouling, or drag reduction of copper-based objects is performed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Surface Modification and Superhydrophobicity · Advanced Sensor and Energy Harvesting Materials · Nanomaterials and Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Nano-Mechanical Systems Research Division, Korea Institute of Machinery & Materials (KIMM), 156 Gajungbukno, Yuseong-gu, Daejeon, 305-343, Korea
Max Planck Institute of Microstructure Physics, Weinberg 2, D-06120 Halle, Germany
References (40)
Show source-provided references
1. Emsley, J.InNature’s building blocks: an A-Z guide to the elements;Oxford University Press:New York, NY, 2003; pp121–125.
2. Berntsson K. M. · Biofouling · 2003 · 19 · 18710.1080/08927014.2003.10382981 ↗
3. Barthlott W. · Planta · 1997 · 202 · 110.1007/s004250050096 ↗
4. Barkhudarov P. M. · Corros. Sci. · 2008 · 50 · 89710.1016/j.corsci.2007.10.005 ↗
5. Zhang F. · Angew. Chem., Int. Ed. · 2008 · 47 · 246610.1002/anie.200704694 ↗
6. Liu T. · Electrochim. Acta · 2007 · 52 · 370910.1016/j.electacta.2006.10.059 ↗
7. Genzer J. · Biofouling · 2006 · 22 · 33910.1080/08927010600980223 ↗
8. Shirtcliffe N. J. · ACS Appl. Mater. Interfaces · 2009 · 1 · 131610.1021/am9001937 ↗
9. Qian B. · Langmuir · 2005 · 21 · 900710.1021/la051308c ↗
10. Rao A. V. · Appl. Surf. Sci. · 2011 · 257 · 577210.1016/j.apsusc.2011.01.099 ↗
11. Li Y. · Chem. Mater. · 2007 · 19 · 575810.1021/cm071738j ↗
12. Chen X. · J. Phys. Chem. C · 2009 · 113 · 539610.1021/jp809616d ↗
13. Guo Z. · Langmuir · 2011 · 27 · 619310.1021/la104979x ↗
14. Li J. · J. Phys. Chem. C · 2011 · 115 · 1693410.1021/jp2058063 ↗
15. Callies M. · Soft Matter · 2005 · 1 · 5510.1039/b501657f ↗
16. Zimmermann J. · Colloids Surf. A · 2007 · 302 · 23410.1016/j.colsurfa.2007.02.033 ↗
17. Xiu Y. · Nanotechnology · 2010 · 21 · 15570510.1088/0957-4484/21/15/155705 ↗
18. Verho T. · Adv. Mater. · 2011 · 23 · 67310.1002/adma.201003129 ↗
19. Jiang X. · Nano Lett. · 2002 · 2 · 133310.1021/nl0257519 ↗
20. Han J.-W. · Mater. Express · 2011 · 1 · 17610.1166/mex.2011.1022 ↗
21. Wright C. R. A. · J. Chem. Soc., Trans. · 1879 · 35 · 47510.1039/CT8793500475 ↗
22. Pease R. N. · J. Am. Chem. Soc. · 1921 · 43 · 217910.1021/ja01443a007 ↗
23. Wenzel R. N. · Ind. Eng. Chem. · 1936 · 28 · 98810.1021/ie50320a024 ↗
24. Wenzel R. N. · J. Phys. Chem. · 1949 · 53 · 146610.1021/j150474a015 ↗
25. Cassie A. B. D. · Trans. Faraday Soc. · 1944 · 40 · 54610.1039/tf9444000546 ↗
26. Lee S.-M. · J. Micromech. Microeng. · 2007 · 17 · 68710.1088/0960-1317/17/4/003 ↗
27. Inorganic Crystal Structure Database (ICSD). ICSD #: 026963, 026715, 064699.
28. Rodrigeuz J. A. · Catal. Lett. · 2003 · 85 · 24710.1023/A:1022110200942 ↗
29. Knotkova, D; Krieslova, K.Atmospheric corrosion and conservation of copper and bronze In Environmental Deterioration of Materials;Moncmanová, A., Eds.WIT Press:Billerica, MA, USA, 2007; pp111–117.10.2495/978-1-84564-032-3/04 ↗
30. Xu J. F. · J. Raman Spectrosc. · 1999 · 30 · 41310.1002/(SICI)1097-4555(199905)30:5<413::AID-JRS387>3.0.CO;2-N ↗
31. Balkanski M. · Solid State Commun. · 1969 · 7 · 81510.1016/0038-1098(69)90768-6 ↗
32. Moulder, J. F.; Stickle, W. F.; Sobol, P. E.; Bomben, K. D.Handbook of X-ray Photoelectron Spectroscopy;Chastain, J., Eds.Perkin-Elmer:Eden Prairie, MN, USA, 1992; p87.
33. Chang F.-M. · Appl. Phys. Lett. · 2010 · 96 · 11410110.1063/1.3360847 ↗
34. Bhushan B. · J. Phys.: Condens. Matter · 2008 · 20 · 225010
35. He. B. · Langmuir · 2003 · 19 · 499910.1021/la0268348 ↗
36. Zhao Y · Langmuir · 2007 · 23 · 621210.1021/la0702077 ↗
37. Lin F. · Langmuir · 2008 · 24 · 411410.1021/la703821h ↗
38. Kim K.-S. · ACS Nano · 2011 · 5 · 510710.1021/nn2011865 ↗
39. Gao X. · Nature · 2004 · 432 · 3610.1038/432036a ↗
40. Lyon S. · Nature · 2004 · 427 · 40610.1038/427406a ↗