Abstract

Commercially available polyaniline emeraldine base (PANI-EB) powder was protonated by simple mixing with camphorsulfonic acid (CSA) to form the CSA-doped emeraldine salt form of PANI (PANI-ES). The PANI-ES state was dissolved in m -cresol at various concentrations (4, 2, 1 wt %) and spin-coated onto fluorine-doped tin oxide (FTO) glass to use as counter electrodes (CEs) in dye-sensitized solar cells (DSSCs). The PANI-based CE exhibited a maximum transmittance of 72.9% in the visible wavelength range, which is equivalent to bare FTO glass. The surface resistivity of CE samples spin-coated with insulating PANI-EB was greater than 10 9 Ω/square, but the value steeply decreased to 1.3 kΩ/square when the CE was spin-coated with CSA-doped PANI-ES. Although the surface resistivity increased, and therefore fill factor ( ff ) gradually decreased, with decreasing solid content of the PANI-based coating solution, the charge-transfer resistance ( R ct ) and short-circuit current ( J sc ) conversely improved due to increased surface roughness, affording enhanced DSSC performance. Furthermore, the overall power conversion efficiency of a DSSC could be enhanced to a maximum of ∼6.3% by optimizing cell parameters through controlling the preparation conditions of the CE.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Conducting polymers and applications · TiO2 Photocatalysis and Solar Cells · Electrochemical sensors and biosensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Advanced Functional Materials Research Team, Automotive R&D Division, Hyundai Motor Company, Jangduk-dong, 366, Hwaseong-si, Gyeonggi-do, 445−706, Republic of Korea

Department of Advanced Material Chemistry, Korea University, Jochiwon, Chungnam, 339-700 Korea

Department of Fiber and Polymer Engineering, Hanyang University, 17 Haengdang-dong, Seoul, 133-791, Korea

References (42)

Show source-provided references
1. Kamat P. V. · J. Phys. Chem. C · 2007 · 111 · 283410.1021/jp066952u ↗
2. Dresslhaus M, S. · Nature · 2001 · 414 · 33210.1038/35104599 ↗
3. O’regan B. · Nature · 1991 · 353 · 73710.1038/353737a0 ↗
4. Grätzel M. · Nature · 2001 · 414 · 33810.1038/35104607 ↗
5. Yella A · Science · 2011 · 334 · 62910.1126/science.1209688 ↗
6. Hamann W. · Energy Environ. Sci. · 2008 · 1 · 6610.1039/b809672d ↗
7. Choi H. · Chem.—Eur. J. · 2010 · 16 · 119310.1002/chem.200902197 ↗
8. Yanagida S. · Acc. Chem. Res. · 2009 · 42 · 182710.1021/ar900069p ↗
9. Choi H. · Angew. Chem., Int. Ed. · 2009 · 48 · 593810.1002/anie.200902013 ↗
10. Choi H. · Angew. Chem., Int. Ed. · 2008 · 47 · 32710.1002/anie.200703852 ↗
11. Koo H. J. · Adv. Mater. · 2008 · 20 · 19510.1002/adma.200700840 ↗
12. Luo Y. · Adv. Mater. · 2009 · 21 · 464710.1002/adma.200901078 ↗
13. Dürr M. · Nat. Mater. · 2005 · 4 · 60710.1038/nmat1433 ↗
14. Hamann T. W. · Energy Environ. Sci. · 2011 · 4 · 37010.1039/C0EE00251H ↗
15. Kim M. J. · J. Phys. Chem. · 2010 · 114 · 19849
16. Lai X. · Energy Environ. Sci · 2012 · 5 · 560410.1039/C1EE02426D ↗
17. Murakami T. N. · Inorg. Chim. Acta · 2008 · 361 · 57210.1016/j.ica.2007.09.025 ↗
18. Papageorgiou N. · Coord. Chem. Rev. · 2004 · 248 · 142110.1016/j.ccr.2004.03.028 ↗
19. Yen M. · Compos. Sci. Technol. · 2009 · 69 · 219310.1016/j.compscitech.2009.06.003 ↗
20. Tai Q. · ACS Nano · 2011 · 5 · 379510.1021/nn200133g ↗
21. Huang K. · J. Mater. Chem. · 2011 · 21 · 1038410.1039/c1jm10576k ↗
22. Li Q. · Electrochem. Commun. · 2008 · 10 · 129910.1016/j.elecom.2008.06.029 ↗
23. Li Z. · Electrochem. Commun. · 2009 · 11 · 176810.1016/j.elecom.2009.07.018 ↗
24. Ameen S. · J. Phys. Chem. C · 2010 · 114 · 476010.1021/jp912037w ↗
25. Jeon S. S. · J. Mater. Chem. · 2011 · 21 · 814610.1039/c1jm10112a ↗
26. Jeon S. S. · J. Phys. Chem. C · 2011 · 115 · 2203510.1021/jp206535c ↗
27. Peng S. · ACS Appl. Mater. Interfaces · 2012 · 4 · 39710.1021/am201461c ↗
28. Xia J. · J. Mater. Chem. · 2011 · 21 · 464410.1039/c0jm04116e ↗
29. Shin H. · Synth. Met. · 2011 · 161 · 128410.1016/j.synthmet.2011.04.024 ↗
30. Ahmad S. · J. Mater. Chem. · 2010 · 20 · 165410.1039/b920210b ↗
31. Xia J. · J. Mater. Chem. · 2007 · 17 · 284510.1039/b703062b ↗
32. Lee K. S. · Chem. Commun. · 2010 · 46 · 450510.1039/c0cc00432d ↗
33. Pringle J. M. · Chem. Commun. · 2010 · 46 · 536710.1039/c0cc01400a ↗
34. Lee K. · Polymer · 2009 · 50 · 437210.1016/j.polymer.2009.07.009 ↗
35. MacDiarmid A. G. · Synth. Met. · 1995 · 69 · 8510.1016/0379-6779(94)02374-8 ↗
36. Lee K. · Phys. Rev. B · 1993 · 48 · 1488410.1103/PhysRevB.48.14884 ↗
37. Stejskal J. · Macromolecules · 1998 · 31 · 221810.1021/ma970823h ↗
38. Lee K. · Nature · 2006 · 441 · 6510.1038/nature04705 ↗
39. Sim S. Y. · Polym. Degrad. Stab. · 2009 · 94 · 20810.1016/j.polymdegradstab.2008.11.002 ↗
40. Qin Q. · Synth. Met. · 2010 · 160 · 116710.1016/j.synthmet.2010.03.003 ↗
41. Han L. · Appl. Phys. Lett. · 2004 · 84 · 243310.1063/1.1690495 ↗
42. Imoto K. · Sol. Energy Mater. Sol. Cell · 2003 · 79 · 45910.1016/S0927-0248(03)00021-7 ↗