Plasma-Enhanced Atomic Layer Deposition of Anatase TiO2 Using TiCl4
Source abstract
Abstract
Self-limiting deposition of anatase TiO 2 was accomplished by plasma-enhanced atomic layer deposition using TiCl 4 and O 2 . Film growth occurred at a rate of ∼1.35 Å/cycle, independent of temperature. The refractive index increased monotonically with temperature, and the presence of the anatase phase was confirmed by FTIR and XRD for T ≥ 110 °C. Films were free of impurities with respect to FTIR and XPS, and conformal coverage was confirmed by cross-section microscopy. These results show that OH groups, the most common surface termination in ALD, is not required for this process.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemical Engineering, Colorado School of Mines, Golden, Colorado 80401
References (30)
Show source-provided references
1. Bennett J. M. · Appl. Opt. · 1989 · 28 · 330310.1364/AO.28.003303 ↗
2. Chao S. · J. Opt. Soc. Am. A · 1999 · 16 · 147710.1364/JOSAA.16.001477 ↗
3. Wang R. · Nature · 1997 · 388 · 43110.1038/41233 ↗
4. Cheng H.-E. · J. Electrochem. Soc. · 2008 · 155 · D60410.1149/1.2952659 ↗
5. Lee J. K. · Appl. Phys. Lett. · 2008 · 92 · 24330810.1063/1.2937844 ↗
6. Wu S. · J. Power Sources · 2008 · 182 · 11910.1016/j.jpowsour.2008.03.054 ↗
7. Rausch N. · Microelectron. Eng. · 1992 · 19 · 72510.1016/0167-9317(92)90531-U ↗
8. Yang W. · J. Vac. Sci. Technol., A · 2007 · 25 · 129810.1116/1.2484649 ↗
9. Puurunen R. L. · J. Appl. Phys. · 2005 · 97 · 12130110.1063/1.1940727 ↗
10. Ritala M. · Thin Solid Films · 1993 · 225 · 28810.1016/0040-6090(93)90172-L ↗
11. Aarik J. · Appl. Surf. Sci. · 2001 · 172 · 14810.1016/S0169-4332(00)00842-4 ↗
12. Matero R. · Chem. Mater. · 2001 · 13 · 450610.1021/cm011046+ ↗
13. Ferguson J. D. · Appl. Surf. Sci. · 2004 · 226 · 39310.1016/j.apsusc.2003.10.053 ↗
14. Puurunen R. L. · Chem. Vap. Deposition · 2005 · 11 · 7910.1002/cvde.200400021 ↗
15. Lim J. W. · Electrochem. Solid-State Lett. · 2004 · 7 · F7310.1149/1.1805502 ↗
16. Niskanen A. · Chem. Vap. Deposition · 2007 · 13 · 15210.1002/cvde.200606546 ↗
17. Xie Q. · J. Electrochem. Soc. · 2008 · 155 · H68810.1149/1.2955724 ↗
18. Rai V. R. · J. Phys. Chem. C · 2009 · 113 · 1296210.1021/jp903669c ↗
19. Szymanski S. F. · Surf. Coat. Technol. · 2007 · 201 · 899110.1016/j.surfcoat.2007.04.076 ↗
20. Heil S. B. S. · J. Appl. Phys. · 2008 · 103 · 10330210.1063/1.2924406 ↗
21. Schuisky M. · Langmuir · 2001 · 17 · 550810.1021/la010174+ ↗
22. Szymanski S. F. · J. Vac. Sci. Technol., A · 2008 · 26 · 107910.1116/1.2891258 ↗
23. Kubala N. G. · Electrochem. Solid-State Lett. · 2009 · 12 · H25910.1149/1.3125287 ↗
24. Kinney J. B. · J. Phys. Chem. · 1983 · 87 · 373510.1021/j100242a033 ↗
25. Chen W. · Surf. Sci. · 1996 · 359 · 9310.1016/0039-6028(96)00579-1 ↗
26. Tiznado H. · J. Phys. Chem. B · 2006 · 110 · 1349110.1021/jp062019f ↗
27. Ghoshtagore R. N. · J. Electrochem. Soc. · 1970 · 117 · 52910.1149/1.2407561 ↗
28. Scarel G. · J. Appl. Phys. · 2002 · 91 · 111810.1063/1.1427430 ↗
29. Busani T. · Semicond. Sci. Technol. · 2005 · 20 · 87010.1088/0268-1242/20/8/043 ↗
30. McIntyre N. S. · 1983