journal article·2020-06-11

Change in the Pd Oxidation State during Light-Off of Three-Way Catalysis Analyzed by in situ Diffuse Reflectance Spectroscopy

Ayumi Fujiwara, Hiroshi Yoshida, Junya Ohyama, Masato Machida

The Journal of Physical Chemistry C· Volume 124· Issue 23
Publisher page

Abstract

The changes in the oxidation state of supported Pd catalysts during light-off of NO–CO–C 3 H 6 –O 2 reactions were evaluated during temperature ramp up and down cycles (10 °C min –1 ) under fuel-rich (air-to-fuel ratio, A / F = 14.1) and fuel-lean ( A / F = 15.0) conditions. Real-time analysis of the Pd oxidation state was carried out by acquiring a diffuse reflectance at a wavelength of 450 nm every second. The correlation between the Kubelka–Munk function and the Pd oxidation state was confirmed by Pd 3d X-ray photoelectron spectroscopy. At the onset of the catalytic reaction, the oxidized Pd species (PdO) supported on Al 2 O 3 was converted to metallic Pd to a varying extent, depending on whether the provided gas feed was rich or lean. Under the rich conditions, >70% of Pd was reduced during light-off, which remained unchanged following the completion of the reaction and the subsequent temperature ramp down. Even under lean conditions, >40% of Pd on the surface was temporally reduced to the metallic state at 300 °C, although the thermodynamic estimation revealed that Pd should be stable in the oxide form. The obtained outcomes suggest that the real catalyst surface at the onset of light-off should be in a more reductive environment than that estimated from the equilibrium O 2 concentration in the gas phase. This is because the Pd surface site was predominantly occupied by the adsorbed CO and/or C 3 H 6 . Nevertheless, following the completion of light-off at ≥400 °C, the Pd surface was immediately reoxidized, as the surface concentration of CO/C 3 H 6 became negligible. The Pd reduction during light-off under lean conditions was determined to be considerably less pronounced when using the oxygen storage CeO 2 –ZrO 2 support. Because of its oxygen storage and release abilities, the reductive atmosphere of the Pd surface was mitigated, and the three-phase boundary formed at the interface with CeO 2 –ZrO 2 provided suitable active sites for the CO/C 3 H 6 light-off at the lowest possible temperatures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Catalytic Processes in Materials Science · Catalysis and Oxidation Reactions · Catalysts for Methane Reforming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Applied Chemistry, Graduate School of Science and Technology, Kumamoto University, 2-39-1 Kurokami, Chuo, Kumamoto 860-8555, Japan

Division of Materials Science and Chemistry, Faculty of Advanced Science and Technology, Kumamoto University, 2-39-1 Kurokami, Chuo, Kumamoto 860-8555, Japan

Elements Strategy Initiative for Catalysts & Batteries (ESICB), Kyoto University, 1-30 Goryo-Ohara, Nishikyo, Kyoto 615-8245, Japan

Funding

Ministry of Education, Culture, Sports, Science and Technology

References (46)

Show source-provided references
1. 10.1080/0161494750807998010.1080/01614947508079980 ↗
2. Heck R. M. · 1995
3. 10.1080/0161494940800946810.1080/01614949408009468 ↗
4. 10.1016/s0920-5861(99)00024-310.1016/s0920-5861(99)00024-3 ↗
5. 10.1016/s0920-5861(00)00407-710.1016/s0920-5861(00)00407-7 ↗
6. 10.1038/s41929-019-0312-910.1038/s41929-019-0312-9 ↗
7. 10.1016/0021-9517(73)90166-810.1016/0021-9517(73)90166-8 ↗
8. Heck R. M. · 1995
9. Barin I. · 199510.1002/9783527619825 ↗
10. 10.1016/s0920-5861(99)00024-310.1016/s0920-5861(99)00024-3 ↗
11. 10.1016/s0920-5861(00)00407-710.1016/s0920-5861(00)00407-7 ↗
12. 10.1021/acs.jpcc.7b0526010.1021/acs.jpcc.7b05260 ↗
13. 10.1016/j.cattod.2016.05.02010.1016/j.cattod.2016.05.020 ↗
14. 10.1021/acs.jpcc.8b0954310.1021/acs.jpcc.8b09543 ↗
15. 10.1006/jcat.1993.123810.1006/jcat.1993.1238 ↗
16. 10.1016/0920-5861(95)00241-310.1016/0920-5861(95)00241-3 ↗
17. 10.1016/s0021-9517(02)00145-810.1016/s0021-9517(02)00145-8 ↗
18. 10.1016/s0021-9517(03)00277-x10.1016/s0021-9517(03)00277-x ↗
19. 10.1016/j.apsusc.2014.03.15310.1016/j.apsusc.2014.03.153 ↗
20. 10.1021/acscatal.9b0166910.1021/acscatal.9b01669 ↗
21. 10.1007/s11244-018-1100-510.1007/s11244-018-1100-5 ↗
22. 10.1021/jacs.7b0711410.1021/jacs.7b07114 ↗
23. 10.1002/anie.20140309410.1002/anie.201403094 ↗
24. 10.1021/acs.jpcc.6b1158310.1021/acs.jpcc.6b11583 ↗
25. 10.1021/acscatal.8b0318010.1021/acscatal.8b03180 ↗
26. 10.1021/acs.jpcc.7b1112910.1021/acs.jpcc.7b11129 ↗
27. 10.1016/j.apcata.2005.07.01310.1016/j.apcata.2005.07.013 ↗
28. Tanaka, H.; Fujiwara, H.; Takahashi, I. Excellent Oxygen Storage Capacity of Perovskite-Pd Three-Way Catalysts. SAE Technical Paper Series, 1995; p 950256.10.4271/950256 ↗
29. 10.1016/j.cattod.2010.10.01510.1016/j.cattod.2010.10.015 ↗
30. 10.1016/j.apcatb.2016.09.03410.1016/j.apcatb.2016.09.034 ↗
31. 10.1016/j.apcatb.2019.04.00110.1016/j.apcatb.2019.04.001 ↗
32. Engel, T.; Ertl, G. Advances in Catalysis; Eley, D. D., Pines, H., Weez, P. B., Eds. Academic Press: New York, 1979; Vol. 28, pp 1–78.
33. 10.1016/0021-9517(91)90319-y10.1016/0021-9517(91)90319-y ↗
34. 10.1021/j100131a04710.1021/j100131a047 ↗
35. 10.1016/s0009-2509(01)00409-210.1016/s0009-2509(01)00409-2 ↗
36. 10.1006/jcat.2000.298510.1006/jcat.2000.2985 ↗
37. 10.1006/jcat.2001.337910.1006/jcat.2001.3379 ↗
38. 10.1016/s0926-3373(02)00033-410.1016/s0926-3373(02)00033-4 ↗
39. 10.1016/j.jcat.2003.07.01010.1016/j.jcat.2003.07.010 ↗
40. 10.1016/j.apcatb.2009.07.01610.1016/j.apcatb.2009.07.016 ↗
41. 10.1021/cs300620410.1021/cs3006204 ↗
42. 10.1039/c3cp44293d10.1039/c3cp44293d ↗
43. 10.1021/acs.jpcc.6b0865610.1021/acs.jpcc.6b08656 ↗
44. 10.1039/c4cy00291a10.1039/c4cy00291a ↗
45. 10.1006/jcat.1998.233410.1006/jcat.1998.2334 ↗
46. 10.1016/s0926-860x(01)00765-710.1016/s0926-860x(01)00765-7 ↗