Analysis of the Irreversible Capacity in an All-Solid-State Lithium Battery with a Porous Current Collector Using Soft X-ray Emission Spectroscopy
Source abstract
Abstract
Dendritic Li metal growth and low Coulombic efficiency (CE) have hindered the application of high energy density Li metal negative electrodes to rechargeable batteries. High mechanical strength of solid electrolyte (SE) in all-solid-state batteries was expected to inhibit Li metal penetration into the SE. However, the increased mechanical stress of Li metal during the deposition reaction pushed the Li metal into voids and cracks of SE, resulting in internal short circuits. We have previously demonstrated that a current collector with many microsized pores reduced the mechanical stress of the Li metal electrode to prevent internal short circuits. However, the low CE during the initial cycle resulted in significantly low capacity retention. Here, to clarify the cause of the low CE, the electronic state of Li accumulated inside the pores of the current collector was first analyzed using soft X-ray emission spectroscopy (SXES). SXES measurements revealed that the deactivated lithium was lithium nitride or lithium oxide. Nitrogen and oxygen gases remaining in the electrochemical cell are considered to be the reactants. Therefore, by keeping a vacuum state inside the electrochemical cell, we succeeded in significantly improving the CE of the initial cycle.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Applied Chemistry, Graduate School of Engineering, Osaka Metropolitan University, Sakai, Osaka 599-8531, Japan
Funding
Advanced Low Carbon Technology Research and Development Program
References (36)
Show source-provided references
1. 10.1038/3510464410.1038/35104644 ↗
2. 10.1002/aenm.20200268910.1002/aenm.202002689 ↗
3. 10.1016/j.jpowsour.2017.01.03710.1016/j.jpowsour.2017.01.037 ↗
4. 10.1002/aenm.20170100310.1002/aenm.201701003 ↗
5. 10.1149/2.0221902jes10.1149/2.0221902jes ↗
6. 10.1021/acsami.9b0253710.1021/acsami.9b02537 ↗
7. 10.1149/1.211979510.1149/1.2119795 ↗
8. 10.1038/s41563-019-0438-910.1038/s41563-019-0438-9 ↗
9. 10.1021/acs.chemmater.7b0300210.1021/acs.chemmater.7b03002 ↗
10. 10.1016/j.joule.2019.06.01310.1016/j.joule.2019.06.013 ↗
11. 10.1021/acsaem.9b0119310.1021/acsaem.9b01193 ↗
12. 10.1021/acsami.6b0083110.1021/acsami.6b00831 ↗
13. 10.1039/C8TA02276C10.1039/C8TA02276C ↗
14. 10.1002/adma.20160604210.1002/adma.201606042 ↗
15. 10.1002/aenm.20170196310.1002/aenm.201701963 ↗
16. 10.1038/nmat482110.1038/nmat4821 ↗
17. 10.1021/acs.nanolett.6b0469510.1021/acs.nanolett.6b04695 ↗
18. 10.1038/s41467-020-20463-y10.1038/s41467-020-20463-y ↗
19. 10.1021/acs.chemmater.6b0061010.1021/acs.chemmater.6b00610 ↗
20. 10.1021/acsami.5b0751710.1021/acsami.5b07517 ↗
21. 10.1021/acsami.8b0886010.1021/acsami.8b08860 ↗
22. 10.1126/sciadv.aau924510.1126/sciadv.aau9245 ↗
23. 10.1016/j.electacta.2018.07.22710.1016/j.electacta.2018.07.227 ↗
24. 10.1016/j.nanoen.2018.09.06110.1016/j.nanoen.2018.09.061 ↗
25. 10.1021/acsami.7b1617610.1021/acsami.7b16176 ↗
26. 10.1002/aenm.20170364410.1002/aenm.201703644 ↗
27. 10.1073/pnas.171975811510.1073/pnas.1719758115 ↗
28. 10.1038/s41586-020-1972-y10.1038/s41586-020-1972-y ↗
29. 10.1021/acsami.0c0175910.1021/acsami.0c01759 ↗
30. 10.1021/acsaem.1c0237810.1021/acsaem.1c02378 ↗
31. 10.1038/ncomms736210.1038/ncomms7362 ↗
32. 10.1021/acs.jpcc.0c0288510.1021/acs.jpcc.0c02885 ↗
33. 10.1021/acsaem.0c0123810.1021/acsaem.0c01238 ↗
34. 10.1016/j.jechem.2022.04.00910.1016/j.jechem.2022.04.009 ↗
35. 10.1080/21663831.2022.214158610.1080/21663831.2022.2141586 ↗
36. 10.1016/j.elecom.2007.02.00810.1016/j.elecom.2007.02.008 ↗