Abstract

We examined the structural reconfiguration after intercalating foreign additives, that is, tetramethoxysilane (TMOS), within already formed supramolecular nanolayers of hexadecyltrimethoxysilane (HDTMS). Our experiments indicated that the newly formed interdigitated structure is a thermodynamically more stable configuration. Even after the HDTMS formed initial bilayer-by-bilayer structures, mixing of these aggregates with foreign additives at room temperature can change the original structure to a more compact configuration (i.e., interdigitated). Our MD simulations further revealed that the most favorable organization for this interdigitated stacking appears to be a formation of relatively small domains of HDTMS and TMOS molecules, supporting our proposal of a heterogeneous mixing before reorganization. Although the coassembly of binary or multiple building blocks has previously been used to modify a supramolecule or to produce a supramolecular composite, the modification of already formed supramolecules via molecular intercalation, examined here, provides a flexible path for decorating more advanced supramolecules without disturbing their complex assembly conditions.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Supramolecular Self-Assembly in Materials · Mesoporous Materials and Catalysis · Block Copolymer Self-Assembly

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Advanced Mechanics and Materials Engineering (AMME) International Laboratory, A-TEAM, Department of Engineering Mechanics and Nebraska Center for Materials and Nanoscience, University of Nebraska, Lincoln, Nebraska 68588, United States

Advanced Mechanics and Materials Engineering (AMME) International Laboratory, LECAP, Institut des Matériaux de Rouen, Faculté des Sciences, Université de Rouen, Site du Madrillet, 76801 Saint Etienne du Rouvray Cedex, France

Department of Chemistry, University of Nebraska, Lincoln, Nebraska 68588, United States

Institut National des Sciences Appliquées de Rouen (INSA), Avenue de l’Université − BP 08, 76801 Saint Etienne du Rouvray Cedex, France

References (32)

Show source-provided references
1. Lehn J. M. · Angew. Chem., Int. Ed. · 1990 · 29 · 130410.1002/anie.199013041 ↗
2. Lehn J. M. · Science · 1993 · 260 · 176210.1126/science.8511582 ↗
3. Matile S. · Chem. Soc. Rev. · 2001 · 30 · 15810.1039/b008101i ↗
4. Ganjali M. R. · Sensors · 2006 · 6 · 101810.3390/s6081018 ↗
5. Kim Y. H. · J. Nanosci. Nanotechnol. · 2008 · 8 · 459310.1166/jnn.2008.IC01 ↗
6. Chen B. L. · Acc. Chem. Res. · 2010 · 43 · 111510.1021/ar100023y ↗
7. Tan J. C. · Proc. Natl. Acad. Sci. U.S.A. · 2010 · 107 · 993810.1073/pnas.1003205107 ↗
8. Yu C. · Adv. Mater. · 2010 · 22 · 445710.1002/adma.201000546 ↗
9. Mattu J. · J. Phys. Chem. B · 2006 · 110 · 1532810.1021/jp057346m ↗
10. Stephenson B. C. · J. Phys. Chem. B · 2007 · 111 · 102510.1021/jp065696i ↗
11. Parikh A. N. · J. Am. Chem. Soc. · 1997 · 119 · 313510.1021/ja963284p ↗
12. Shimojima A. · Bull. Chem. Soc. Jpn. · 1997 · 70 · 284710.1246/bcsj.70.2847 ↗
13. Jiang J. · ACS Nano · 2010 · 4 · 377310.1021/nn100273m ↗
14. Jiang J. · J. Am. Chem. Soc. · 2009 · 131 · 90010.1021/ja808103h ↗
15. Brinker C. J. · J. Non. Cryst. Solids · 1988 · 100 · 3110.1016/0022-3093(88)90005-1 ↗
16. Kim H. K. · J. Phys. Chem. B · 2003 · 107 · 434810.1021/jp022377s ↗
17. Shimojima A. · Langmuir · 2002 · 18 · 114410.1021/la011016l ↗
18. Brand M. · Z. Naturforsch. · 1999 · 54 · 15510.1515/znb-1999-0202 ↗
19. bSince HCl was mostly dispersed in water, a pH value of 4 can be estimated if we take into account the total volume of water as 0.11 mL. At such a low pH value, the hydrolysis rate constant for HDTMS is 1.04 h–1(ref17a), suggesting 96% of the molecules becoming silanols at the end of 3 h. (c) The relative increase in the intensity of the α structure fromti= 1 min to 6 h is qualitative. While the films were prepared with exactly the same procedure, the final film thickness and surface area of the specimen probed by the X-ray beam cannot be accurately controlled and may have contributed to the change in intensity.
20. Tímár-Balázsy Á. · 1998
21. Bourlinos A. B. · Small · 2005 · 1 · 8010.1002/smll.200400027 ↗
22. Osman M. A. · J. Phys. Chem. B · 2000 · 104 · 443310.1021/jp993448z ↗
23. Beari F. · J. Organomet. Chem. · 2001 · 625 · 20810.1016/S0022-328X(01)00650-7 ↗
24. Ang T. P. · J. Phys. Chem. B · 2004 · 108 · 1100110.1021/jp049006r ↗
25. Yilgor I. · Polym. Bull. · 1998 · 40 · 52510.1007/s002890050286 ↗
26. Badia A. · Acc. Chem. Res. · 2000 · 33 · 47510.1021/ar9702841 ↗
27. Daoud W. A. · Appl. Surf. Sci. · 2006 · 252 · 536810.1016/j.apsusc.2005.12.020 ↗
28. Jursic B. S. · J. Chem. Soc., Perkin Trans. II · 1999 · 36910.1039/a803744b ↗
29. Walsh, R.Bond Dissociation Energies in Organosilicon Compounds.http://www.gelest.com /Library/10BondDiss.pdf(accessed 06/13/ 10) .
31. , 2002.
32. De Prado L. A. S. A. · J. Polym. Sci., Part A: Polym. Chem. · 2010 · 48 · 122010.1002/pola.23885 ↗