Abstract

Spectroscopic and electrochemical techniques were used to examine the benefits of adding small amounts of aluminum titanate (Al 2 TiO 5 or ALT) to standard NiO–yttria-stabilized zirconia (YSZ)-based solid oxide fuel cell anodes operating with methane at 800 °C. Combining small amounts (4% by mass) of ALT with NiO–YSZ leads to the formation of secondary phases that improve anode carbon tolerance via multiple reaction mechanisms. Raman data show that carbon forms on both ALT-doped and undoped anodes at open-circuit voltage and with applied bias as evidenced by the vibrational band of highly ordered graphite at 1560 cm –1 . However, ALT-doped anodes limited the amount of carbon that forms on both the surface and within the bulk, resulting in improved performance for up to 12 h of exposure to CH 4 . Results show that ALT-enhanced anodes accumulate ∼25% less carbon on the surface under open-circuit conditions and that increasing polarizations to 50% of the maximum current and beyond results in no observable carbon accumulation. These observations are used to deduce possible mechanisms that describe how secondary phases suppress carbon accumulation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Catalysis and Oxidation Reactions · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Montana Materials Science University, Bozeman MT 59715, United States

Funding

U.S. Department of Energy

References (60)

Show source-provided references
1. 10.1016/j.apcata.2006.10.04010.1016/j.apcata.2006.10.040 ↗
2. 10.1016/j.jpowsour.2010.08.07310.1016/j.jpowsour.2010.08.073 ↗
3. 10.1016/j.jpowsour.2009.09.01410.1016/j.jpowsour.2009.09.014 ↗
4. 10.1021/jp511304x10.1021/jp511304x ↗
5. 10.1149/05701.1267ecst10.1149/05701.1267ecst ↗
6. 10.1021/cm902640j10.1021/cm902640j ↗
7. 10.1016/j.pecs.2013.10.00110.1016/j.pecs.2013.10.001 ↗
8. 10.1149/2.051302jes10.1149/2.051302jes ↗
9. 10.1016/s0920-5861(97)00014-x10.1016/s0920-5861(97)00014-x ↗
10. 10.1016/s0920-5861(02)00209-210.1016/s0920-5861(02)00209-2 ↗
11. 10.1039/c3cp53278j10.1039/c3cp53278j ↗
12. 10.1021/jp711312p10.1021/jp711312p ↗
13. 10.1021/acs.chemrev.6b0028410.1021/acs.chemrev.6b00284 ↗
14. 10.1016/j.jpowsour.2010.11.09510.1016/j.jpowsour.2010.11.095 ↗
15. 10.1149/1.139395810.1149/1.1393958 ↗
16. 10.1016/j.matchemphys.2016.02.04610.1016/j.matchemphys.2016.02.046 ↗
17. 10.1149/1.157733710.1149/1.1577337 ↗
18. 10.1111/j.1551-2916.2009.02980.x10.1111/j.1551-2916.2009.02980.x ↗
19. 10.1016/j.ijhydene.2014.01.09210.1016/j.ijhydene.2014.01.092 ↗
20. 10.1016/j.jpowsour.2005.09.06010.1016/j.jpowsour.2005.09.060 ↗
21. 10.1038/3500504010.1038/35005040 ↗
22. 10.1016/s0167-2738(99)00111-310.1016/s0167-2738(99)00111-3 ↗
23. 10.1002/1521-4095(200010)12:19<1465::aid-adma1465>3.0.co;2-910.1002/1521-4095(200010)12:19<1465::aid-adma1465>3.0.co;2-9 ↗
24. 10.1126/science.112587710.1126/science.1125877 ↗
25. 10.1039/c2ra01256a10.1039/c2ra01256a ↗
26. 10.1016/j.jpowsour.2014.02.00810.1016/j.jpowsour.2014.02.008 ↗
27. 10.1016/j.materresbull.2013.11.03410.1016/j.materresbull.2013.11.034 ↗
28. 10.1021/acs.jpcc.5b0134510.1021/acs.jpcc.5b01345 ↗
29. 10.1149/1.361022610.1149/1.3610226 ↗
30. Sofie, S. W.; Taylor, D. R. In Advances in Solid Oxide Fuel Cells III: Ceramic and Engineering Science Proceedings; Bansal, P. N., Salem, J., Zhu, D., Eds. Wiley-Blackwell, 2009; Vol. 28, pp 215–223.10.1002/9780470339534.ch21 ↗
31. 10.1016/j.jpowsour.2016.01.07010.1016/j.jpowsour.2016.01.070 ↗
32. 10.1016/j.apcata.2016.08.02010.1016/j.apcata.2016.08.020 ↗
33. 10.1149/2.0531803jes10.1149/2.0531803jes ↗
34. 10.1002/fuce.20170007310.1002/fuce.201700073 ↗
35. 10.1006/jcat.1998.205110.1006/jcat.1998.2051 ↗
36. 10.1016/s0926-3373(99)00133-210.1016/s0926-3373(99)00133-2 ↗
37. 10.1016/s0166-9834(00)80427-310.1016/s0166-9834(00)80427-3 ↗
38. Driscoll, D. R. Stabilization of Metallic Catalyst Microstructures against High Temperature Thermal Coarsening. Ph.D. Dissertation, Montana State University, Bozeman, MT, 2016.
39. 10.1016/0021-9517(91)90333-y10.1016/0021-9517(91)90333-y ↗
40. 10.1016/j.fuproc.2003.12.01310.1016/j.fuproc.2003.12.013 ↗
41. 10.1016/j.apcata.2008.06.00710.1016/j.apcata.2008.06.007 ↗
42. 10.1016/s0926-860x(00)00424-510.1016/s0926-860x(00)00424-5 ↗
43. 10.1016/j.elecom.2008.11.01410.1016/j.elecom.2008.11.014 ↗
44. 10.1016/j.jpowsour.2009.11.12610.1016/j.jpowsour.2009.11.126 ↗
45. 10.1016/j.jpowsour.2014.06.08710.1016/j.jpowsour.2014.06.087 ↗
46. 10.1016/j.jpowsour.2014.01.01410.1016/j.jpowsour.2014.01.014 ↗
47. 10.1007/s40843-015-0033-610.1007/s40843-015-0033-6 ↗
48. 10.1007/s10853-018-2205-810.1007/s10853-018-2205-8 ↗
49. 10.1103/physrevb.86.04541110.1103/physrevb.86.045411 ↗
50. 10.1021/jp910492b10.1021/jp910492b ↗
51. 10.1021/ac048600u10.1021/ac048600u ↗
52. 10.1146/annurev.anchem.111808.07364110.1146/annurev.anchem.111808.073641 ↗
53. 10.1016/0021-9517(94)90002-710.1016/0021-9517(94)90002-7 ↗
54. 10.1016/j.molcata.2004.09.01610.1016/j.molcata.2004.09.016 ↗
55. 10.1016/j.jeurceramsoc.2009.10.01210.1016/j.jeurceramsoc.2009.10.012 ↗
56. McIntyre, M. D. In Operando Studies of High Temperature Electrocatalysts Used for Energy Conversion. Ph.D. Dissertation, Montana State University, Bozeman, MT, 2016.
57. 10.1021/ac301504g10.1021/ac301504g ↗
58. 10.1016/j.jpowsour.2017.11.02410.1016/j.jpowsour.2017.11.024 ↗
59. 10.1149/1.155906410.1149/1.1559064 ↗
60. 10.1021/acs.jpcc.5b1186110.1021/acs.jpcc.5b11861 ↗