journal article·2010-10

Double-perovskites A2FeMoO6− (A= Ca, Sr, Ba) as anodes for solid oxide fuel cells

Leilei Zhang, Qingjun Zhou, Qiang He, Tianmin He

Journal of Power Sources· Volume 195· Issue 19
Publisher page

Abstract

Abstract Double-perovskites A 2 FeMoO 6− δ ( A = Ca, Sr, Ba) have been investigated as potential anode materials for solid oxide fuel cells (SOFCs). At room temperature, A 2 FeMoO 6− δ compounds crystallize in monoclinic, tetragonal, and cubic structures for A = Ca, Sr, and Ba, respectively. A weak peak observed at around 880 cm −1 in the Raman spectra can be attributed to traces of A MoO 4 . XPS has confirmed the coexistence of Fe 2+ –Mo 6+ and Fe 3+ –Mo 5+ electronic configurations. Moreover, a systematic shift from Fe 2+/3+ –Mo 6+/5+ to Fe 2+ –Mo 6+ configuration is seen with increasing A -site cation size. A 2 FeMoO 6− δ samples display distinct electrical properties in H 2 , which can be attributed to different degrees of degeneracy of the Fe 2+ –Mo 6+ and Fe 3+ –Mo 5+ configurations. Ca 2 FeMoO 6− δ is unstable in a nitrogen atmosphere, while Sr 2 FeMoO 6− δ and Ba 2 FeMoO 6− δ are stable up to 1200 °C. The thermal expansion coefficients of Sr 2 FeMoO 6− δ and Ba 2 FeMoO 6− δ are very close to that of La 0.9 Sr 0.1 Ga 0.8 Mg 0.2 O 3− δ (LSGM). The performances of cells with 300 μm thick LSGM electrolyte, double-perovskite SmBaCo 2 O 5+ x cathodes, and A 2 FeMoO 6− δ anodes follow the sequence Ca 2 FeMoO 6− δ 2 FeMoO 6− δ 2 FeMoO 6− δ . The maximum power densities of a cell with an Sr 2 FeMoO 6− δ anode reach 831 mW cm −2 in dry H 2 and 735 mW cm −2 in commercial city gas at 850 °C, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Magnetic and transport properties of perovskites and related materials · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Murray · Nature · 1999 · 400 · 64910.1038/23220 ↗
2. Atkinson · Nat. Mater. · 2004 · 3 · 1710.1038/nmat1040 ↗
3. Goodenough · J. Power Sources · 2007 · 173 · 110.1016/j.jpowsour.2007.08.011 ↗
4. Tao · Nat. Mater. · 2003 · 2 · 32010.1038/nmat871 ↗
5. Zhu · Mater. Sci. Eng. A · 2003 · 362 · 22810.1016/S0921-5093(03)00620-8 ↗
6. Jiang · J. Mater. Sci. · 2004 · 39 · 440510.1023/B:JMSC.0000034135.52164.6b ↗
7. McIntosh · Chem. Rev. · 2004 · 104 · 484510.1021/cr020725g ↗
8. Tao · Chem. Rec. · 2004 · 4 · 8310.1002/tcr.20003 ↗
9. Lashtabeg · J. Mater. Chem. · 2006 · 16 · 316110.1039/B603620A ↗
10. Sun · J. Power Sources · 2007 · 171 · 24710.1016/j.jpowsour.2007.06.086 ↗
11. Tsipis · J. Solid State Electrochem. · 2008 · 12 · 136710.1007/s10008-008-0611-6 ↗
12. Zha · J. Solid State Chem. · 2005 · 178 · 184410.1016/j.jssc.2005.03.027 ↗
13. Huang · Science · 2006 · 312 · 25410.1126/science.1125877 ↗
14. Huang · J. Electrochem. Soc. · 2006 · 153 · A126610.1149/1.2195882 ↗
15. Marrero-Lopez · Mater. Res. Bull. · 2008 · 43 · 244110.1016/j.materresbull.2007.07.032 ↗
16. Bernuy-Lopez · Chem. Mater. · 2007 · 19 · 103510.1021/cm0624116 ↗
17. Huang · Chem. Mater. · 2009 · 21 · 231910.1021/cm8033643 ↗
18. Ji · Electrochem. Commun. · 2007 · 9 · 188110.1016/j.elecom.2007.04.006 ↗
19. Wei · Electrochem. Commun. · 2008 · 10 · 136910.1016/j.elecom.2008.07.005 ↗
20. Nakamura · Mater. Res. Bull. · 1981 · 16 · 32110.1016/0025-5408(81)90048-9 ↗
21. Falcón · Appl. Catal. B-Environ. · 2004 · 53 · 3710.1016/j.apcatb.2004.05.004 ↗
22. Yamazoe · Catal. Today · 1990 · 8 · 17510.1016/0920-5861(90)87017-W ↗
23. Zhou · J. Power Sources · 2008 · 185 · 75410.1016/j.jpowsour.2008.07.064 ↗
24. Cong · J. Alloys Compd. · 2003 · 348 · 32510.1016/S0925-8388(02)00859-9 ↗
25. Shen · J. Am. Ceram. Soc. · 2009 · 92 · 225910.1111/j.1551-2916.2009.03196.x ↗
26. Philipp · Phys. Rev. B · 2003 · 68 · 14443110.1103/PhysRevB.68.144431 ↗
27. Son · J. Raman Spectrosc. · 2001 · 32 · 81710.1002/jrs.764 ↗
28. Zhang · J. Raman Spectrosc. · 2004 · 35 · 108110.1002/jrs.1258 ↗
29. Porto · Phys. Rev. · 1967 · 157 · 71610.1103/PhysRev.157.716 ↗
30. Merino · Catal. Lett. · 2007 · 113 · 13010.1007/s10562-007-9017-9 ↗
31. Fierro · Catal. Today · 1990 · 8 · 15310.1016/0920-5861(90)87016-V ↗
32. Tabata · J. Mater. Sci. Lett. · 1987 · 6 · 103010.1007/BF01729122 ↗
33. Bartkowski · Phys. Rev. B · 1997 · 56 · 1065610.1103/PhysRevB.56.10656 ↗
34. Cantalini · IEEE Sens. J. · 2003 · 3 · 17110.1109/JSEN.2002.807489 ↗
35. Kuepper · Phys. Status Solidi A · 2004 · 201 · 325210.1002/pssa.200405432 ↗
36. Besse · Europhys. Lett. · 2002 · 60 · 60810.1209/epl/i2002-00262-4 ↗
37. Yasukawa · J. Solid State Chem. · 2004 · 177 · 265510.1016/j.jssc.2004.04.031 ↗
38. Woodward · J. Mater. Res. · 1994 · 9 · 211810.1557/JMR.1994.2118 ↗
39. Niebieskikwiat · Phys. Rev. B · 2000 · 62 · 334010.1103/PhysRevB.62.3340 ↗
40. Sleight · J. Phys. Chem. Solids · 1972 · 33 · 67910.1016/0022-3697(72)90076-5 ↗
41. Kobayashi · Nature · 1998 · 395 · 67710.1038/27167 ↗
42. Zener · Phys. Rev. · 1951 · 82 · 40310.1103/PhysRev.82.403 ↗
43. Itoh · Mater. Sci. Eng. B · 1996 · 41 · 5510.1016/S0921-5107(96)01623-6 ↗
44. Allub · Phys. Rev. B · 1997 · 55 · 1411310.1103/PhysRevB.55.14113 ↗
45. Matsuda · J. Solid State Chem. · 2009 · 182 · 171310.1016/j.jssc.2009.04.016 ↗
46. Marrero-López · Solid State Ionics · 2010 · 180 · 167210.1016/j.ssi.2009.11.005 ↗
47. Peña · Chem. Rev. · 2001 · 101 · 198110.1021/cr980129f ↗
48. Pacchioni · Chem. Phys. Chem. · 2003 · 4 · 104110.1002/cphc.200300835 ↗
49. Mori · Solid State Ionics · 2002 · 146 · 30110.1016/S0167-2738(01)01020-7 ↗
50. Onuma · Solid State Ionics · 2004 · 174 · 28710.1016/j.ssi.2004.07.037 ↗
51. Murray · Solid State Ionics · 2001 · 143 · 26510.1016/S0167-2738(01)00871-2 ↗
52. Bao · J. Power Sources · 2009 · 193 · 60710.1016/j.jpowsour.2009.04.034 ↗
53. Coyle · J. Power Sources · 2009 · 193 · 73010.1016/j.jpowsour.2009.04.042 ↗