Differential voltage analyses of high-power lithium-ion cells. 4. Cells containing NMC
Source abstract
Abstract
Abstract Cells with and without a LiC2O4BF2 electrolyte additive and that contained Li1.05(Mn1/3Co1/3Ni1/3)0.95O2 (NMC) positive electrodes were tested for calendar and cycle life at 60% state of charge. The temperatures used in these tests were 25 and 45 °C (cycle life) and 45 and 55 °C (calendar life). An analysis of the C/25 capacity data shows that the C/25 capacity decreases with the square root of time. The additive slowed down the rate of capacity decline. The C/25 data were subjected to differential voltage analysis to determine the possible cause of the capacity decrease and at which electrode the capacity decrease was occurring. Data from full cells and half-cells were compared to elucidate individual electrode contributions. This analysis indicated that lithium-capacity-consuming side reactions were occurring primarily at the negative electrode.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. FY2008 Progress Report for Energy Storage Research and Development, U.S. Department of Energy, January 2009. http://www1.eere.energy.gov/vehiclesandfuels/pdfs/program/2008_energy_storage.pdf.
2. Bloom · J. Power Sources · 2003 · 124 · 53810.1016/S0378-7753(03)00806-1 ↗
3. Bloom · J. Power Sources · 2005 · 139 · 29510.1016/j.jpowsour.2004.07.021 ↗
4. Bloom · J. Power Sources · 2005 · 139 · 30410.1016/j.jpowsour.2004.07.022 ↗
5. Bloom · J. Power Sources · 2006 · 155 · 41510.1016/j.jpowsour.2005.05.008 ↗
6. Bloom · J. Power Sources · 2006 · 157 · 53710.1016/j.jpowsour.2005.07.054 ↗
7. Abraham · J. Power Sources · 2007 · 170 · 46510.1016/j.jpowsour.2007.03.071 ↗
8. Yabuuchi · J. Power Sources · 2003 · 119–121 · 17110.1016/S0378-7753(03)00173-3 ↗
9. Yoshizawa · J. Power Sources · 2007 · 174 · 81310.1016/j.jpowsour.2007.06.153 ↗
10. Yabuuchi · J. Power Sources · 2007 · 154 · A314
11. Cordova · 2008 · 307
12. Ferguson · 2008 · 461
13. PNGV Battery Test Manual, DOE/ID-10597, Rev. 3, U.S. Department of Energy, February 2001.
14. Andersson · J. Electrochem. Soc. · 2002 · 149 · A135810.1149/1.1505636 ↗
15. Ensling · J. Mater. Chem. · 2009 · 19 · 8210.1039/B813099J ↗
16. Arora · J. Electrochem. Soc. · 1998 · 145 · 364710.1149/1.1838857 ↗
17. Aurbach · J. Power Sources · 1999 · 81/82 · 9510.1016/S0378-7753(99)00187-1 ↗
18. Abraham · Electrochim. Acta · 2004 · 49 · 476310.1016/j.electacta.2004.05.040 ↗
19. Xiao · J. Electrochem. Soc. · 2009 · 156 · A31810.1149/1.3078020 ↗