journal article·2004-01

Electrochemical performance of lithium ion battery, nano-silicon-based, disordered carbon composite anodes with different microstructures

Xiang-Wu Zhang, Prashanth K Patil, Chunsheng Wang, A.John Appleby, Frank.E Little, David L Cocke

Journal of Power Sources· Volume 125· Issue 2
Publisher page

Abstract

Abstract Nano-silicon-based disordered carbon composites prepared by mechanical milling and pyrolysis have been examined as anodes of a lithium ion cell. Electrochemical measurements show that the charge–discharge capacity of disordered carbon composites incorporating both silicon-polyparaphenylene (Si-PPP) and silicon-polyvinyl chloride (Si-PVC) with differing silicon contents, decreases with increasing pyrolysis temperature. Si-PVC-based materials have a better cycle life than those based on Si-PPP at the same silicon content.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Supercapacitor Materials and Fabrication · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Megahed · J. Power Sources · 1994 · 51 · 7910.1016/0378-7753(94)01956-8 ↗
2. Zhou · J. Power Sources · 1997 · 68 · 29610.1016/S0378-7753(96)02563-3 ↗
3. Kinoshita · J. Power Sources · 2002 · 110 · 41610.1016/S0378-7753(02)00206-9 ↗
4. R.A. Huggins, in: J.O. Besenhard (Ed.), Handbook of Battery Materials, Wiely/VCH, Weinheim, 1999, p. 359.10.1002/9783527611676.ch16 ↗
5. Besenhard · J. Power Sources · 1997 · 68 · 8710.1016/S0378-7753(96)02547-5 ↗
6. Beaulieu · J. Electrochem. Soc. · 2000 · 147 · 320610.1149/1.1393884 ↗
7. Li · Electrochem. Solid State Lett. · 1999 · 2 · 54710.1149/1.1390899 ↗
8. Wang · J. Electrochem. Soc. · 1998 · 145 · 275110.1149/1.1838709 ↗
9. Yoshio · J. Electrochem. Soc. · 2002 · 149 · A159810.1149/1.1518988 ↗
10. Kurita · Carbon · 2002 · 40 · 25310.1016/S0008-6223(01)00089-6 ↗
11. Xiang · Solid State Ionics · 1997 · 74 · 2410
12. Dahn · Electrochim. Acta · 1993 · 38 · 117910.1016/0013-4686(93)80048-5 ↗
13. Kambe · Mater. Sci. Eng. · 1979 · 40 · 110.1016/0025-5416(79)90002-8 ↗
14. Tatsumi · J. Electrochem. Soc. · 1995 · 142 · 71610.1149/1.2048523 ↗
15. Dollimore · Carbon · 1967 · 5 · 6510.1016/0008-6223(67)90108-X ↗
16. Inagaki · J. Eur. Ceram. Soc. · 1998 · 18 · 101110.1016/S0955-2219(97)00176-3 ↗