journal article·2004-03

Long-term operation of AFC electrodes with CO2 containing gases

E. Gülzow, M. Schulze

Journal of Power Sources· Volume 127· Issue 1-2
Publisher page

Abstract

Low temperature fuel cells represent an important component in pollution-free energy conversion for mobile application. Alkaline fuel cells are an interesting alternative for polymer electrolyte membrane fuel cells (PEFC), because they do not need expensive membranes and catalysts. It is commonly accepted, that carbon dioxide intolerance is the most pronounced disadvantage of air breathing alkaline fuel cells. Thus, alkaline technology is commonly not considered for mobile fuel cell application. In this study, the long-term influence of carbon dioxide containing reaction gases on electrodes manufactured by a rolling process were investigated. To investigate the mechanisms of carbon dioxide poisoning, gas diffusion electrodes (GDEs) which were designed for alkaline fuel cells had been operated in a half cell configuration up to several thousand of hours with a constant load of 150 mA/cm2. The reactants were contaminated with 5% CO2. The experiments were performed with both electrodes, anode and cathode. Control measurements were performed by operating electrodes with pure reactants. During these long-term experiments, the V–I curves were recorded daily. Recently also the chemical surface compositions of the gas diffusion electrodes were investigated by X-ray-induced photoelectron spectroscopy (XPS) after long-term operation. In addition to the characterization of the electrode, the carbonate concentration in the electrolyte was determined after different operation times. The electrochemical performance of the electrodes, anodes and cathodes, decreases during the operation time in both operation modes, operated with pure gases as well as with CO2 containing gases. The decreases in both modes are comparable; this means the CO2 neither enhances the degradation process nor induces a new, detrimental degradation process. The XPS characterization of used cathodes operated with pure and with CO2 containing oxygen yielded no significant difference. A slightly higher carbon concentration was observed on the surface of the anodes which was operated with CO2 containing hydrogen than on surfaces of anodes which were operated with pure hydrogen. The carbonate concentration in the electrolyte increases during fuel cell operation with CO2 containing gases. The long-term behavior of the investigated alkaline fuel cell (AFC) electrodes supplied with CO2 containing gases gives no evidence that CO2 affects significantly the degradation process.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Internet, e.g. http://www.eyeforfuelcells.com: Astris Energi in Discussion with Nine Foreign Fuel Cell Prospects in Six Countries.
2. V. Plzak, H. Wendt, Brennstoffzellen, VDI-Verlag, Düsseldorf, 1990.
3. J. Nitsch, C.-J. Winter, Wasserstoff als Energieträger, Springer-Verlag, Berlin, 1986.
4. Gülzow · J. Power Sources · 1996 · 61 · 9910.1016/S0378-7753(96)02344-0 ↗
5. K. Kordesch, G. Simader, Fuel Cells and Their Applications, VCH-Verlag, Weinheim, 1996.10.1002/352760653X ↗
6. E. Gülzow, M. Schulze, G. Steinhilber, K. Bolwin, in: Proceedings of the Fuel Cell Seminar on Carbon Dioxide Tolerance of Gas Diffusion Electrodes for Alkaline Fuel Cells, San Diego, 1994, p. 319.
7. Davies · J. Appl. Electrochem. · 2000 · 30 · 10110.1023/A:1003831406406 ↗
8. Davies · J. Power Sources · 2000 · 86 · 23710.1016/S0378-7753(99)00524-8 ↗
9. Mattsson · Electrochim. Acta · 2000 · 45 · 140510.1016/S0013-4686(99)00351-5 ↗
10. Hübner · J. Mater. Chem. · 1999 · 9 · 40910.1039/a807129b ↗
11. Schulze · Fresenius J. Anal. Chem. · 1999 · 365 · 10610.1007/s002160051454 ↗
12. Büchi · Electrochim. Acta · 1995 · 40 · 34510.1016/0013-4686(94)00274-5 ↗
13. Gülzow · J. Power Sources · 2000 · 86 · 35210.1016/S0378-7753(99)00451-6 ↗
14. Gupta · J. Appl. Electrochem. · 1998 · 28 · 67310.1023/A:1003288609411 ↗
15. E. Gülzow, M. Fischer, A. Helmbold, R. Reißner, M. Schulze, N. Wagner, M. Lorenz, B. Müller, T. Kaz, in: Proceedings of the Fuel Cell Seminar on Innovative Production Technique for PEFC and DMFC Electrodes and Degradation of MEA-Components, Palm Springs, 16–19 November 1998, p. 469.
16. E. Gülzow, T. Kaz, M. Lorenz, A. Schneider, M. Schulze, in: Proceedings of the Fuel Cell Seminar on Degradation of PEFC Components, Portland, 30 October–02 November 2000, p. 156.
17. Wilson · Electrochim. Acta · 1995 · 40 · 35510.1016/0013-4686(94)00272-3 ↗
18. Dirven · J. Appl. Electrochem. · 1995 · 25 · 12210.1007/BF00248168 ↗
19. Gülzow · J. Power Sources · 2002 · 106 · 12610.1016/S0378-7753(01)01033-3 ↗
20. Gultekin · Int. J. Hydrogen Energy · 1996 · 21 · 48510.1016/0360-3199(95)00086-0 ↗
21. Kiros · J. Power Sources · 2000 · 87 · 10110.1016/S0378-7753(99)00436-X ↗
22. Rahman · J. Appl. Electrochem. · 1997 · 27 · 21510.1023/A:1018412226014 ↗
23. Schulze · Fresenius J. Anal. Chem. · 1995 · 353 · 77810.1007/BF00321370 ↗
24. E. Gülzow, et al., in: Proceedings of the Ninth World Hydrogen Energy Conference on PTFE bonded Gas Diffusion Electrodes for Alkaline Fuel Cells, Paris, 1992, p. 1507.
25. Khalidi · Int. J. Hydrogen Energy · 1996 · 21 · 2510.1016/0360-3199(95)00040-K ↗
26. Schulze · Appl. Surf. Sci. · 2001 · 179 · 25210.1016/S0169-4332(01)00291-4 ↗
27. N. Wagner, E. Gülzow, M. Schulze, W. Schnurnberger, in: H. Steeb, H. Aba Oud (Eds.), Gas Diffusion Electrodes for Alkaline Fuel Cells in Solar Hydrogen Energy, German-Saudi Joint Program on Solar Hydrogen Production and Utilization Phase II 1992–1995 (ISBN 3-89100-028-6), Stuttgart, 1996.
28. M. Schulze, E. Gülzow, Degradation of nickel anodes in alkaline fuel cells, in: Proceedings of the Eighth UECT, Ulm, 20–21 June 2002, J. Power Sources, this issue.
29. H. Sauer, German patent DE 2 941 774 (CI H01M4/88).
30. A. Winsel, German patent DE 3 342 969 (CI C25B11/06).
31. Gülzow · Dechema-Monographien Bd · 1989 · 117 · 365
32. Gülzow · Dechema-Monographien Bd · 1991 · 124 · 675
33. Gülzow · Dechema-Monographien Bd · 1990 · 121 · 483
34. E. Gülzow, K. Bolwin, W. Schnurnberger, Brennstoffzellen, Hrsg. H. Wendt, V. Plzak, VDI-Verlag, Düsseldorf, 1990.
35. Gülzow · Dechema Monographien Bd · 1992 · 125 · 561
36. N. Wagner, Verfahren und Vorrichtung zur Herstellung einer Elektrode, Deutsche Patentanmeldung, Patent Norbert DE19940015A1, 2001.
37. E. Gülzow, et al., Fuel Cell Bull. 15 (1999) 8–12.10.1016/S1464-2859(99)80002-9 ↗
38. D. Bevers, E. Gülzow, A. Helmbold, B. Müller, in: Proceedings of the Fuel Cell Seminar on Innovative Production Technique for PEFC Electrodes, Orlando, 1996, p. 668.10.2172/460319 ↗
39. A. Helmbold, German patent DE 197 57 492 A 1, 1999.
40. D. Bevers, N. Wagner, German patent DE 195 09 749 C2.
41. Gülzow · J. Power Sources · 2002 · 106 · 12210.1016/S0378-7753(01)01030-8 ↗
42. N. Wagner, E. Gülzow, M. Schulze, Long-term investigations of silver cathodes for alkaline fuel cells, in: Proceedings of the Eighth UECT, Ulm, 20–21 June 2002, J. Power Sources, this issue.
43. G. Ertl, J. Küppers, Low Energy Electron and Surface Spectroscopy, VCH-Verlagsgesellschaft, Weinheim, 1985.
44. S.J. Gregg, K.S.W. Sing, Adsorption, Surface Area and Porosity, Academic Press, London, 1982.
45. J.F. Moulder, W.F. Strickle, P.E. Sobol, K.D. Bomben, in: J. Chastain, R.C. King (Eds.), Handbook of X-Ray Photoelectron Spectroscopy, Physical Electronic Inc., MN, 1995.
46. G. Beamson, D. Briggs, High resolution XPS of Organic Polymers, Wiley, Chichester, 1992.
47. Drummond · Fresenius J. Anal. Chem. · 1993 · 346 · 20010.1007/BF00321413 ↗
48. Clark · J. Elec. Spectrosc. Relat. Phenom · 1988 · 47 · 9310.1016/0368-2048(88)85006-0 ↗
49. D.R. Lide (Ed.), Handbook of Chemistry and Physics, 77th ed., CRC Press, Boca Raton, FL, 1996.