Highly conductive epoxy/graphite composites for bipolar plates in proton exchange membrane fuel cells
Source abstract
Abstract
Abstract Carbon-filled epoxy composites are developed for potential application as bipolar plates in proton exchange membrane (PEM) fuel cells. These composites are prepared by solution intercalation mixing, followed by compression molding and curing. Electrical conductivity, thermal and mechanical properties, and hygrothermal characteristics are determined as function of carbon-filler content. Expanded graphite and carbon black are used as synergistic combination to obtain desired in-plane and through-plane conductivities. These composites show high glass transition temperatures (Tg ∼ 180 °C), high thermal degradation temperatures (T2 ∼ 415 °C), in-plane conductivity of 200–500 S cm−1 with 50 wt% carbon fillers, in addition to offering high values of flexural modulus, flexural strength, and impact strength, respectively 2 × 104 MPa, 72 MPa, and 173 J m−1. The presence of carbon fillers helps reduce water uptake from 4 to 5 wt% for unfilled epoxy resins to 1–2 wt%. In addition, morphology, electrical, mechanical, and thermal properties remain unchanged on exposure to boiling water and acid reflux. This data indicate that the composites developed in this work meet many attributes of bipolar plates for use in PEM fuel cells.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Advanced Battery Technologies Research · Membrane-based Ion Separation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Larminie · 2003
2. Huang · J. Power Sources · 2005 · 150 · 11010.1016/j.jpowsour.2005.02.074 ↗
3. Heinzel · J. Power Sources · 2004 · 131 · 3510.1016/j.jpowsour.2004.01.014 ↗
4. Li · Int. J. Hydrogen Energy · 2005 · 30 · 35910.1016/j.ijhydene.2004.09.019 ↗
5. 2003 · 286
6. Clulow · 2002 · 417
7. Lafront · Electrochim. Acta · 2007 · 52 · 507610.1016/j.electacta.2007.01.080 ↗
8. Tawfik · J. Power Sources · 2007 · 163 · 75510.1016/j.jpowsour.2006.09.088 ↗
9. Show · Diam. Relat. Mater. · 2007 · 16 · 115910.1016/j.diamond.2006.11.068 ↗
10. Wang · J. Power Sources · 2006 · 163 · 50010.1016/j.jpowsour.2006.09.048 ↗
11. Wang · J. Power Sources · 2006 · 162 · 48610.1016/j.jpowsour.2006.06.084 ↗
12. Paulauskas · Corros. Sci. · 2006 · 48 · 315710.1016/j.corsci.2005.10.019 ↗
13. Cunningham · J. Mater. Chem. · 2006 · 16 · 435810.1039/b611883f ↗
14. Barbir · J. New Mater. Electrochem. Sys. · 1999 · 2 · 197
15. Kuan · J. Power Sources · 2004 · 134 · 710.1016/j.jpowsour.2004.02.024 ↗
16. Kumar · J. Power Sources · 2004 · 129 · 6210.1016/j.jpowsour.2003.11.011 ↗
17. Cho · J. Power Sources · 2004 · 125 · 17810.1016/j.jpowsour.2003.08.039 ↗
18. Cunningham · J. Power Sources · 2007 · 168 · 41810.1016/j.jpowsour.2007.03.036 ↗
19. Besmann · J. Electrochem. Soc. · 2000 · 147 · 408310.1149/1.1394023 ↗
20. Kuo · J. Power Sources · 2006 · 162 · 20710.1016/j.jpowsour.2006.06.034 ↗
21. Zou · J. Polym. Sci. Part B: Polym. Phys. · 2002 · 40 · 95410.1002/polb.10141 ↗
22. Zheng · Comp. Sci. Tech. · 2003 · 63 · 22510.1016/S0266-3538(02)00201-4 ↗
23. Clingerman · Polym. Compos. · 2002 · 23 · 91110.1002/pc.10488 ↗
24. 1993 · 1
25. Blunk · J. Power Sources · 2006 · 159 · 53310.1016/j.jpowsour.2005.09.068 ↗
26. Meha · J. Power Sources · 2003 · 114 · 3210.1016/S0378-7753(02)00542-6 ↗
27. Gottesfeld · Adv. Electrochim. Sci. Eng. · 1997 · 5 · 19510.1002/9783527616794.ch4 ↗
28. Zhou · Polymer · 1999 · 40 · 550510.1016/S0032-3861(98)00790-3 ↗
29. Zhou · Polymer · 1999 · 40 · 551310.1016/S0032-3861(98)00791-5 ↗
30. Zhou · J. Thermoplast. Compos. Mater. · 1996 · 9 · 31610.1177/089270579600900402 ↗
31. Shin · J. Thermoplast. Compos. Mater. · 2000 · 13 · 4010.1106/WKTW-G6RL-DNJF-EAK7 ↗
32. Sichel · 1982
33. Wessling · Polym. Eng. Sci. · 2004 · 31 · 120010.1002/pen.760311608 ↗
34. Wypych · 2000