Experimental investigation of cascading failure in 18650 lithium ion cell arrays: Impact of cathode chemistry
Source abstract
Abstract
To investigate thermal runaway propagation in lithium ion cell arrays (referred to as cascading failure), a set of experiments was conducted under well-controlled conditions in a wind tunnel where 18650 form factor cells were arranged into a densely packed array. The cell arrays were constructed from 12 lithium ion cells arranged in a rectangular configuration (3 columns by 4 rows) with no inter-cell spacing (each cell was in a contact with the adjacent cells). Commercial cells of different cathode chemistry, lithium cobalt oxide (LCO), lithium nickel manganese cobalt oxide (NMC), and lithium iron phosphate (LFP), were employed as test samples in this study. All studied cells were fully charged. The experiments were conducted in both anaerobic (N2) and air environments to demonstrate the impact of flaming combustion. In each experiment, thermal runaway was triggered into the middle cell of row 1 using an electric heater and was observed to propagate through the array via thermocouples attached to the cell bottom surfaces. The dynamics of cascading failure were quantified together with thermal energy release for each cathode chemistry. Furthermore, the yields of the ejected O2, total hydrocarbons (THC), CO, CO2, and H2 were determined; corresponding fire hazards were assessed. For LCO and NMC cell arrays tested in an N2 or air environment, it was found that thermal runaway of the intentionally failed cell was sufficient to initiate cascading failure that fully propagated through the array. LFP cell arrays, however, underwent incomplete/partial cascading failure (maximum of six and eight cells out of twelve failed in N2 and air, respectively). When LCO, NMC, LFP cell arrays were tested in air rather than N2, the row-to-row thermal runaway propagation speed increased by factors of 9, 2, and 7, respectively, which was attributed to the influence flaming combustion of ejected materials. On average, individual LCO, NMC, and LFP cells lost 38.4%, 54.7%, and 11.7% of their initial mass, respectively, when tested in N2, and this percentage increased by 0.3-3.2% when tested in air. Measurements showed that failed LCO and NMC cells produced minor mass yields of O2 and H2 in addition to relatively large amounts of THC, CO, and CO2. The yields of gases ejected from LFP cells were significantly less than the yields obtained for LCO and NMC cells. The lower flammability limit of the flammable portion (THC, CO, and H2) of the ejected gases was found to be 5.79 ± 0.12, 5.92 ± 0.15, and 4.28 ± 0.15 vol.% in air for LCO, NMC, and LFP cells, respectively. The maximum volume of an enclosure where the gas ejection from a single cell creates a flammable mixture in an air environment was estimated to be 0.087 ± 0.017, 0.076 ± 0.0146, and 0.029 ± 0.019 m3 for LCO, NMC, and LFP cells, respectively. The sum of the chemical heat (associated with chemical reactions between battery materials inside and outside the cell casing during failure) and flaming combustion energy (associated with burning of ejected cell materials) was found to be 3.2, 1.9, or 2.5 times greater than the electrical energy stored for LCO, NMC, or LFP cell, respectively. Overall, the obtained results showed that LFP-based cell arrays are the least hazardous arrays. Therefore, they are recommended as a safe option, even though the nominal capacity of the LFP cells is relatively low.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Maloney · 2016
2. Maloney · 2016
3. Maloney · 2016
4. Energetics of lithium ion battery failure10.1016/j.jhazmat.2016.06.047 ↗
5. A review of lithium ion battery failure mechanisms and fire prevention strategies10.1016/j.pecs.2019.03.002 ↗
6. Thermal runaway caused fire and explosion of lithium ion battery10.1016/j.jpowsour.2012.02.038 ↗
7. Safety mechanisms in lithium-ion batteries10.1016/j.jpowsour.2005.12.002 ↗
8. Comprehensive calorimetry of the thermally-induced failure of a lithium ion battery10.1016/j.jpowsour.2015.01.125 ↗
9. Heat release during thermally-induced failure of a lithium ion battery: impact of cathode composition10.1016/j.firesaf.2016.08.001 ↗
10. Simultaneous measurement of multiple thermal hazards associated with a failure of prismatic lithium ion battery10.1016/j.proci.2018.05.066 ↗
11. Comprehensive analysis of dynamics and hazards associated with cascading failure in 18650 lithium ion cell arrays10.1016/j.apenergy.2019.04.141 ↗
12. A Thermo-kinetic model of thermally-induced failure of a lithium ion battery: development, validation and application10.1149/2.0111813jes ↗
13. Investigation on the fire-induced hazards of Li-ion battery cells by fire calorimetry, Energ
14. Evaluating the thermal failure risk of large-format lithium-ion batteries using a cone calorimeter10.1177/0734904118816616 ↗
15. Study of the temperature and flame characteristics of two capacity LiFePO4 batteries in thermal runaway10.1149/2.0531816jes ↗
16. New-type gel dry-water extinguishants and its effectiveness10.1016/j.jclepro.2017.08.005 ↗
17. Thermal-runaway experiments on consumer Li-ion batteries with metal-oxide and olivin-type cathodes10.1039/C3RA45748F ↗
18. Thermal runaway of commercial 18650 Li-ion batteries with LFP and NCA cathodes – impact of state of charge and overcharge10.1039/C5RA05897J ↗
19. Characteristics of lithium-ion batteries during fire tests10.1016/j.jpowsour.2014.08.027 ↗
20. Toxic fluoride gas emissions from lithium-ion battery fires10.1038/s41598-017-09784-z ↗
21. Impact of state of charge and cell arrangement on thermal runaway propagation in lithium ion battery cell arrays, Transportation Research Record10.1177/0361198119845654 ↗
22. Failure propagation in multi-cell lithium ion batteries10.1016/j.jpowsour.2014.10.081 ↗
23. Thermal failure propagation in lithium-ion battery modules with various shapes10.3390/app8081263 ↗
24. Experimental analysis of thermal runaway propagation risk within 18650 lithium-ion battery modules10.1149/2.0461809jes ↗
25. Experimental analysis of thermal runaway and propagation in lithium-ion battery modules10.1149/2.0921509jes ↗
26. Tenergy
27. Co
28. K2energy
29. Tenergy
30. Tenergy
31. LG
32. LG
33. K2energy
34. Linden · 2001
35. Hurley · 201610.1007/978-1-4939-2565-0 ↗
36. McAllister · 201110.1007/978-1-4419-7943-8 ↗
37. A comparison of the electrode/electrolyte reaction at elevated temperatures for various Li-ion battery cathodes10.1016/S0378-7753(01)01013-8 ↗
38. Quintiere · 2016