journal article·2006-07

Oxidation kinetics and phase evolution of a Fe–16Cr alloy in simulated SOFC cathode atmosphere

Pu Jian, Li Jian, Hua Bing, Guangyuan Xie

Journal of Power Sources· Volume 158· Issue 1
Publisher page

Abstract

Abstract The oxidation behavior of a Fe–16Cr alloy containing a small amount of Mn oxidized in air for up to 500 h within the temperature range of 650–850 °C was examined. Two consecutive oxidation stages were found and these obeyed the parabolic rate law with various rate constants. Formation and growth of Cr 2 O 3 , MnCr 2 O 4 , surface nodules and oxide spallation were found to be responsible in the oxidation stages accordingly to various situations. The thin film X-ray diffraction, SEM and EDX confirmed the duplex oxide microstructure with MnCr 2 O 4 on top of Cr 2 O 3 , Cr and Mn diffusion in Cr 2 O 3 is considered to be responsible for the formation of each layer, respectively. The estimated area specific resistance (ASR) suggests the possibility of using this alloy as the interconnect material in reduced temperature SOFCs, however, surface modification to enhance its oxidation and spallation resistances is desired.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Singh · Int. J. Appl. Ceram. Technol. · 2004 · 1 · 510.1111/j.1744-7402.2004.tb00149.x ↗
2. Singhal · Solid State Ionics · 2003 · 152–153 · 405
3. Fuel Cell Handbook, 5th ed., EG&G Services, National Technical Information Service, U.S. Department of Commerce, 2000.
4. Zhu · Mater. Sci. Eng. · 2003 · A348 · 22710.1016/S0921-5093(02)00736-0 ↗
5. Yasuda · J. Electrochem. Soc. · 1996 · 143 · 158310.1149/1.1836683 ↗
6. de Souza · J. Electrochem. Soc. · 1997 · 144 · L3510.1149/1.1837484 ↗
7. Hung · J. Am. Ceram. Soc. · 1998 · 81 · 256510.1111/j.1151-2916.1998.tb02662.x ↗
8. Leng · Int. J. Hydrogen Energy · 2004 · 29 · 102510.1016/j.ijhydene.2004.01.009 ↗
9. Brylewski · J. Therm. Anal. Calorim. · 2004 · 77 · 20710.1023/B:JTAN.0000033205.69427.8e ↗
10. Meulenberg · J. Mater. Sci. · 2003 · 38 · 50710.1023/A:1021879800937 ↗
11. Zhu · Mater. Res. Bull. · 2003 · 38 · 95710.1016/S0025-5408(03)00076-X ↗
12. Huang · Solid State Ionics · 2000 · 129 · 23710.1016/S0167-2738(99)00329-X ↗
13. Fuel cell Handbook, The U.S. Department of energy, 2002.
14. Horita · J. Power Sources · 2003 · 118 · 3510.1016/S0378-7753(03)00058-2 ↗
15. Brylewski · Solid State Ionics · 2001 · 143 · 13110.1016/S0167-2738(01)00863-3 ↗
16. Kurokawa · Solid State Ionics · 2004 · 168 · 1310.1016/j.ssi.2004.02.008 ↗
17. Yen · J. Electrochem. Soc. · 1996 · 143 · 249310.1149/1.1837036 ↗
18. Marasco · Oxid. Met. · 1991 · 36 · 15710.1007/BF00938460 ↗
19. Fava · J. Phys: Condens. Matter · 1997 · 9 · 1071510.1088/0953-8984/9/48/014 ↗
20. Qu Wei, Master Thesis, University of Calgary, Canada, 2004.
21. Horita · J. Electrochem. Soc. · 2003 · 150 · A24310.1149/1.1539498 ↗
22. Yearian · Corrosion · 1956 · 12 · 5510.5006/0010-9312-12.10.55 ↗
23. Hagel · Trans. Am. Soc. Met. · 1963 · 56 · 583
24. Caplan · Trans. AIME · 1965 · 233 · 766
25. Lobnig · Oxid. Met. · 1992 · 27 · 8110.1007/BF00665632 ↗
26. Wild · Corrsion Sci. · 1977 · 17 · 8710.1016/0010-938X(77)90011-7 ↗
27. Cox · Phila. Mag. · 1972 · 26 · 83910.1080/14786437208226960 ↗
28. Caplan · Trans. AIME · 1965 · 233 · 766
29. G.V. Samsonov, The Oxide Handbook, translated from Russian by C. Nigel Turton and T. Turton, IFI/Plenum, 1973.10.1007/978-1-4615-9597-7 ↗
30. A.V. Virkar, U.S. Patent 6,054,231 (April 25, 2000).10.1088/1126-6708/2000/07/054 ↗