journal article·2010-05

Intermediate temperature fuel cell with a doped ceria–carbonate composite electrolyte

Chun Xia, Yi Li, Ye Tian, Qinghua Liu, Zhiming Wang, Lijun Jia, Yicheng Zhao, Yongdan Li

Journal of Power Sources· Volume 195· Issue 10
Publisher page

Abstract

Abstract The performance of a composite electrolyte composed of a samarium doped ceria (SDC) and a binary eutectic carbonate melt phase has been examined. This material shows higher ionic conductivity than pure SDC in intermediate temperature region. SDC with different morphologies is obtained by co-precipitation, sol–gel and glycine-nitrate combustion preparation techniques. A tri-layer single cell is prepared with a cost-effective co-pressing and co-sintering technique. It is found that the surface properties of SDC and the electrolyte thickness have a great influence on the fuel cell performance. When the co-precipitated SDC is used as the electrolyte component and CO2/O2 gas mixture is adopted as the cathode oxidant gas, a fuel cell with an excellent performance is obtained, which has a peak power output of 1704 mW cm−2 at a current density of 3000 mA cm−2 at 650 °C. The influence of cathode atmosphere is examined with conductivity measurement and fuel cell performance test. The results support the concept of O2−/H+/CO32− ternary conduction.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Haile · Acta Mater. · 2003 · 51 · 598110.1016/j.actamat.2003.08.004 ↗
2. Zhu · Int. J. Energy Res. · 2006 · 30 · 89510.1002/er.1195 ↗
3. Lv · Mater. Sci. Eng. A · 2007 · 458 · 35510.1016/j.msea.2006.12.072 ↗
4. Minervini · Solid State Ionics · 1999 · 116 · 33910.1016/S0167-2738(98)00359-2 ↗
5. Lee · J. Power Sources · 2007 · 166 · 3510.1016/j.jpowsour.2006.12.099 ↗
6. Yokokawa · Solid State Ionics · 2004 · 174 · 20510.1016/j.ssi.2004.05.030 ↗
7. Leng · J. Power Sources · 2003 · 117 · 2610.1016/S0378-7753(03)00350-1 ↗
8. Hui · J. Power Sources · 2007 · 172 · 84010.1016/j.jpowsour.2007.05.036 ↗
9. Peng · Solid State Ionics · 2002 · 152–153 · 56110.1016/S0167-2738(02)00365-X ↗
10. Kim · J. Power Sources · 2005 · 139 · 6710.1016/j.jpowsour.2004.07.013 ↗
11. Zhu · Int. J. Electrochem. Sci. · 2006 · 1 · 38310.1016/S1452-3981(23)17167-7 ↗
12. Xia · J. Power Sources · 2009 · 188 · 15610.1016/j.jpowsour.2008.11.068 ↗
13. Ai · J. Membr. Sci. · 2006 · 286 · 25510.1016/j.memsci.2006.10.003 ↗
14. Torrens · Solid State Ionics · 1998 · 111 · 910.1016/S0167-2738(98)00172-6 ↗
15. Huang · Solid State Ionics · 1997 · 100 · 2310.1016/S0167-2738(97)00309-3 ↗
16. Huang · Electrochem. Commun. · 2006 · 8 · 78510.1016/j.elecom.2006.03.016 ↗
17. Zhu · Electrochem. Commun. · 1999 · 1 · 24210.1016/S1388-2481(99)00047-8 ↗
18. Will · Solid State Ionics · 2000 · 131 · 7910.1016/S0167-2738(00)00624-X ↗
19. Jiang · J. Power Sources · 2007 · 165 · 13410.1016/j.jpowsour.2006.12.026 ↗
20. Xia · J. Am. Ceram. Soc. · 2001 · 84 · 190310.1111/j.1151-2916.2001.tb00934.x ↗
21. Singh · Ionics · 2007 · 13 · 42910.1007/s11581-007-0123-x ↗
22. Huang · Electrochem. Solid State Lett. · 2005 · 8 · A43710.1149/1.1960139 ↗
23. Béléké · Vib. Spectrosc. · 2006 · 40 · 6610.1016/j.vibspec.2005.07.002 ↗
24. Mizuhata · J. Electrochem. Soc. · 2004 · 151 · E17910.1149/1.1688798 ↗
25. Delnick · J. Electrochem. Soc. · 1990 · 137 · 1110.1149/1.2086345 ↗
26. Mizuhata · Electrochim. Acta · 2007 · 53 · 7110.1016/j.electacta.2007.06.020 ↗
27. Huang · Electrochem. Commun. · 2007 · 9 · 260110.1016/j.elecom.2007.07.036 ↗
28. Huang · J. Power Sources · 2008 · 175 · 23810.1016/j.jpowsour.2007.09.018 ↗
29. Li · Electrochem. Commun. · 2007 · 9 · 286310.1016/j.elecom.2007.10.010 ↗
30. Liu · Key Eng. Mater. · 2005 · 280–283 · 42510.4028/www.scientific.net/KEM.280-283.425 ↗
31. Zhu · Electrochem. Commun. · 2008 · 10 · 30210.1016/j.elecom.2007.11.037 ↗
32. Li · Int. J. Hydrogen Energy · 2009
33. Zhu · Mater. Res. Bull. · 2006 · 41 · 205710.1016/j.materresbull.2006.04.001 ↗
34. Liu · J. Power Sources · 2008 · 185 · 102210.1016/j.jpowsour.2008.08.100 ↗
35. Zhu · Int. J. Hydrogen Energy · 2008 · 33 · 338510.1016/j.ijhydene.2008.03.065 ↗
36. Rui · J. Membr. Sci. · 2009 · 345 · 11010.1016/j.memsci.2009.08.034 ↗
37. Li · Catal. Today · 2009 · 148 · 30310.1016/j.cattod.2009.08.009 ↗