Abstract
This work presents a non-destructive in-situ method for probing degradation mechanisms in large format, operating, commercial lithium-ion batteries by neutron diffraction. A fresh battery (15 Ah capacity) was shown to have a uniform (homogeneous) local state of charge (SOC) at 4.0 V (9 Ah SOC) and 4.2 V (15 Ah SOC), with 1.33 C and 2.67 C charging rates, respectively. This battery was then aggressively cycled until it retained only a 9 Ah capacity, 60% of its original value. Inhomogeneous deterioration in the battery was observed: near the edges, both the graphite anode and the spinel-based cathode showed a significant loss of capacity, while near the central area, both electrodes functioned properly. An SOC mapping measurement of the degraded battery in the fully charged state (4.2 V) indicated that the loss of local capacity of the anode and cathode is coupled.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Goodenough · Chem. Mater. · 2010 · 22 · 58710.1021/cm901452z ↗
2. Arora · J. Electrochem. Soc. · 1998 · 145 · 364710.1149/1.1838857 ↗
3. Kanevskii · Russ. J. Electrochem. · 2005 · 41 · 110.1007/s11175-005-0042-y ↗
4. Kerlau · Electrochim. Acta · 2007 · 53 · 138510.1016/j.electacta.2007.10.009 ↗
5. Nanda · Adv. Funct. Mater. · 2011 · 21 · 328210.1002/adfm.201100157 ↗
6. Lei · J. Phys. Chem. B · 2005 · 109 · 95210.1021/jp046027c ↗
7. Kojima · J. Power Sources · 2011 · 196 · 772110.1016/j.jpowsour.2011.05.017 ↗
8. Christensen · J. Electrochem. Soc. · 2005 · 152 · A81810.1149/1.1870752 ↗
9. Premanand · J. Electrochem. Soc. · 2002 · 149 · A5410.1149/1.1426399 ↗
10. Vetter · J. Power Sources · 2005 · 147 · 26910.1016/j.jpowsour.2005.01.006 ↗
11. Xia · J. Electrochem. Soc. · 1997 · 144 · 259310.1149/1.1837870 ↗
12. Hunter · J. Solid State Chem. · 1981 · 39 · 14210.1016/0022-4596(81)90323-6 ↗
13. Lee · J. Power Sources · 2000 · 89 · 710.1016/S0378-7753(00)00375-X ↗
14. Wang · Sci. Rep. · 2012 · 2 · 74710.1038/srep00747 ↗
15. Senyshyn · J. Power Sources · 2012 · 203 · 12610.1016/j.jpowsour.2011.12.007 ↗
16. Kehrwald · J. Electrochem. Soc. · 2011 · 158 · A139310.1149/2.079112jes ↗
17. An · Metall. Mater. Trans. A · 2011 · 42A · 9510.1007/s11661-010-0495-9 ↗
18. Wang · Mater. Sci. Forum · 2010 · 652 · 10510.4028/www.scientific.net/MSF.652.105 ↗
19. K. An, VDRIVE – Data Reduction and Interactive Visualization Software for Event Mode Neutron Diffraction, ORNL Report, Oak Ridge National Laboratory, ORNL-TM-2012-621, 2012.
20. Berg · Solid State Ion. · 2001 · 144 · 6510.1016/S0167-2738(01)00894-3 ↗
21. Toby · J. Appl. Crystallogr. · 2001 · 34 · 21010.1107/S0021889801002242 ↗
22. R.B. Von Dreele, A.C. Larson, Los Alamos National Laboratory Report, LAUR 86-748, 1994.
23. Boulineau · Chem. Mater. · 2009 · 21 · 421610.1021/cm900998n ↗
24. Strobel · J. Solid State Chem. · 1988 · 75 · 9010.1016/0022-4596(88)90305-2 ↗
25. Kim · J. Power Sources · 2008 · 180 · 90910.1016/j.jpowsour.2007.09.054 ↗
26. Xia · J. Electrochem. Soc. · 1996 · 143 · 82510.1149/1.1836544 ↗