journal article·2011-03

Impact of pore microstructure evolution on polarization resistance of Ni-Yttria-stabilized zirconia fuel cell anodes

J. Scott Cronin, James R. Wilson, Scott A. Barnett

Journal of Power Sources· Volume 196· Issue 5
Publisher page

Abstract

Abstract Temperature induced degradation in Solid Oxide Fuel Cell (SOFC) Ni-YSZ anodes was studied using both impedance spectroscopy and three-dimensional tomography via Focused Ion Beam–Scanning Electron Microscopy. A 100 h anneal at 1100 °C caused a 90% increase in cell polarization resistance, which correlated with the observed factor of ∼2 reduction in the electrochemically active three-phase boundary (TPB) density. The TPB decrease was caused by a significant decrease in pore percolation, and a reduction in pore interfacial area due to pores becoming larger and more equiaxed. The anneal caused no measurable change in average Ni particle size; Ni coarsening was apparently highly constrained in these anodes due to the relatively large YSZ volume fraction and low pore volume.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Cayan · J. Power Sources · 2008 · 185 · 59510.1016/j.jpowsour.2008.06.058 ↗
2. Matsuzaki · Solid State Ionics · 2000 · 132 · 26110.1016/S0167-2738(00)00653-6 ↗
3. Fergus · Int. J. Hydrogen Energy · 2007 · 32 · 366410.1016/j.ijhydene.2006.08.005 ↗
4. Matsuzaki · Solid State Ionics · 2000 · 132 · 27110.1016/S0167-2738(00)00654-8 ↗
5. Liu · Solid State Ionics · 2005 · 176 · 43510.1016/j.ssi.2004.08.018 ↗
6. Liu · Solid State Ionics · 2003 · 161 · 110.1016/S0167-2738(03)00271-6 ↗
7. Simner · Electrochem. Solid-State Lett. · 2006 · 9 · A47810.1149/1.2266160 ↗
8. Osinkin · Russ. J. Electrochem. · 2010 · 46 · 4110.1134/S1023193510010052 ↗
9. Matsui · J. Electrochem. Soc. · 2010 · 157 · B77610.1149/1.3336830 ↗
10. Jiang · J. Mater. Sci. · 2003 · 38 · 377510.1023/A:1025936317472 ↗
11. Jiang · Solid State Ionics · 2005 · 176 · 118510.1016/j.ssi.2005.02.013 ↗
12. Simwonis · Solid State Ionics · 2000 · 132 · 24110.1016/S0167-2738(00)00650-0 ↗
13. Faes · Fuel Cells · 2009 · 9 · 84110.1002/fuce.200800147 ↗
14. Tanasini · Fuel Cells · 2009 · 9 · 74010.1002/fuce.200800192 ↗
15. Wilson · J. Power Sources · 2009 · 195 · 182910.1016/j.jpowsour.2009.09.074 ↗
16. Iwata · J. Electrochem. Soc. · 1996 · 143 · 152110.1149/1.1836673 ↗
17. Hagen · J. Electrochem. Soc. · 2006 · 153 · A116510.1149/1.2193400 ↗
18. Wilson · Nat. Mater. · 2006 · 5 · 54110.1038/nmat1668 ↗
19. Wilson · Scripta Mater. · 2010
20. Shearing · J. Power Sources · 2010 · 195 · 480410.1016/j.jpowsour.2010.02.047 ↗
21. Iwai · J. Power Sources · 2009 · 195 · 95510.1016/j.jpowsour.2009.09.005 ↗
22. Jørgensen · Ultramicroscopy · 2010 · 110 · 21610.1016/j.ultramic.2009.11.013 ↗
23. Gostovic · Electrochem. Solid-State Lett. · 2007 · 10 · B21410.1149/1.2794672 ↗
24. Chen · J. Power Sources · 2011 · 196 · 133310.1016/j.jpowsour.2010.08.010 ↗
25. Wilson · Electrochem. Solid-State Lett. · 2008 · 11 · B18110.1149/1.2960528 ↗
26. Nicholas · J. Electrochem. Soc. · 2010 · 157 · B53610.1149/1.3284519 ↗
27. Wilson · Electrochem. Commun. · 2009 · 11 · 105210.1016/j.elecom.2009.03.010 ↗
28. Wilson · Microsc. Microanal. · 2009 · 15 · 7110.1017/S1431927609090096 ↗
29. Holzer · J. Microsc. · 2004 · 216 · 8410.1111/j.0022-2720.2004.01397.x ↗
30. J.R. Wilson, Ph.D. Thesis, Department of Materials Science and Engineering, Northwestern University, Evanston, IL, 2008, pp. 1–298.
31. Wilson · ECS Trans. · 2009 · 25 · 228310.1149/1.3205779 ↗
32. Leonide · J. Electrochem. Soc. · 2008 · 155 · B3610.1149/1.2801372 ↗
33. Barfod · J. Electrochem. Soc. · 2007 · 154 · B37110.1149/1.2433311 ↗