Load cycle durability of a graphitized carbon black-supported platinum catalyst in polymer electrolyte fuel cell cathodes
Source abstract
Abstract
We focus on Pt degradation occurring during fuel cell vehicle (FCV) combined drive cycles involving load and open circuit voltage (OCV) just after startup and during idling. Load cycle durability is evaluated as a function of OCV/load holding time, load rate and relative humidity (RH) with a graphitized carbon black-supported platinum catalyst (Pt/GCB) in the cathode. The degradation of Pt/GCB is suppressed for shorter OCV holding times, lower load rates and lower RH. Scanning ion microscopy (SIM) images of membrane cross-sections indicate that the amount of Pt deposited in the membrane decreases during drive cycles involving load with short OCV holding times. Investigations of the Pt distribution in the cathode catalyst layer (CL) by using scanning TEM-EDX show that the dissolution of Pt is suppressed on the membrane side in the CL. The Pt dissolution is accelerated by the high Pt oxidation due to the long OCV holding time. A load cycle with both long OCV holding time and low load inhibits the Pt2+ migration into the membrane but accelerates the Pt particle growth due to electrochemical Ostwald ripening; meanwhile, a load cycle with long OCV holding time at lower RH prevents both the Pt dissolution and particle growth.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. A reverse-current decay mechanism for fuel cells10.1149/1.1896466 ↗
2. The impact of carbon stability on PEM fuel cell startup and shutdown voltage degradation10.1149/1.2356199 ↗
3. Investigation of the corrosion of carbon supports in polymer electrolyte fuel cells using simulated start-up/shutdown cycling10.1016/j.electacta.2012.12.082 ↗
4. Deleterious effects of interim cyclic voltammetry on Pt/carbon black catalyst degradation during start-up/shutdown cycling evaluation10.1016/j.electacta.2013.12.120 ↗
5. PEM fuel cell electrocatalyst durability measurements10.1016/j.jpowsour.2006.03.009 ↗
6. Investigation of dynamic driving cycle effect on performance degradation and micro-structure change of PEM fuel cell10.1016/j.ijhydene.2008.10.054 ↗
7. Degradation mechanism of PEMFC under open circuit operation10.1149/1.2266163 ↗
8. Reversible and irreversible degradation in fuel cells during open circuit voltage durability testing10.1016/j.jpowsour.2008.04.009 ↗
9. A ring-disk electrode study of the current/potential behaviour of platinum in 1.0 M sulphuric and 0.1 M perchloric acids10.1016/0013-4686(70)80070-6 ↗
10. A study of the dissolution of platinum, palladium, rhodium and gold electrodes in 1 m sulphuric acid by cyclic voltammetry10.1016/S0022-0728(72)80308-5 ↗
11. Effect of voltage on platinum dissolution10.1149/1.2180536 ↗
12. Crystallite growth of platinum dispersed on graphitized carbon black10.1016/0021-9517(74)90209-7 ↗
13. Crystallite growth of platinum dispersed on graphitized carbon black: II. Effect of liquid environment10.1016/0021-9517(76)90207-4 ↗
14. Deterioration of Pt catalyst under potential cycling10.1149/1.2356183 ↗
15. Consumption rate of Pt under potential cycling10.1149/1.2400596 ↗
16. Dissolution of platinum in acidic media10.1016/j.electacta.2008.07.052 ↗
17. Degradation of Pt/C under various potential cycling patterns10.1007/s12678-012-0105-2 ↗
18. The Impact of cycle profile on PEMFC durability10.1149/1.2781035 ↗
19. Electrocatalyst durability under simulated automotive drive cycles10.1149/1.2981858 ↗
20. Platinum dissolution and deposition in the polymer electrolyte membrane of a PEM fuel cell as studied by potential cycling10.1039/B514342J ↗
21. Surface platinum electrooxidation in the presence of oxygen10.1021/jp211490a ↗
22. Platinum-alloy cathode catalyst degradation in proton exchange membrane fuel cells: nanometer-scale compositional and morphological changes10.1149/1.3258275 ↗
23. Electrochemical oxide film formation at noble metals as a surface-chemical process10.1016/0079-6816(95)00040-6 ↗
24. In situ and real-time monitoring of oxide growth in a few monolayers at surfaces of platinum nanoparticles in aqueous media10.1021/ja810036h ↗
25. Surface-oxide growth at platinum electrodes in aqueous H2SO4 reexamination of its mechanism through combined cyclic-voltammetry, electrochemical quartz-crystal nanobalance, and auger electron spectroscopy measurements
26. In situ STM observation of morphological changes of the Pt(111) electrode surface during potential cycling in 10 mM HF solution10.1039/b923956a ↗
27. New preparation method of a high performance gas diffusion electrode working at 100% utilization of catalyst clusters and analysis of the reaction layer10.1016/0022-0728(86)80149-8 ↗
28. Spatially resolved electrode diagnostic technique for fuel cell applications10.1149/1.2780956 ↗
29. Comprehensive study of the growth of thin oxide layers on Pt electrodes under well-defined temperature, potential, and time conditions10.1016/j.jelechem.2006.01.022 ↗
30. Dissolution mechanism of platinum in sulfuric acid solution10.1149/2.017212jes ↗
31. The effect of humidity and oxygen partial pressure on degradation of Pt/C catalyst in PEM fuel cell10.1016/j.electacta.2008.10.008 ↗
32. Investigation of water transport through membrane in a PEM fuel cell by water balance experiments10.1016/j.jpowsour.2005.09.013 ↗
33. Distribution profile of hydrogen and oxygen permeating in polymer electrolyte membrane measured by mixed potential10.1016/j.elecom.2007.05.011 ↗