journal article·2017-03

Temperature effects on cycling stability of Li plating/stripping on Ta-doped Li7La3Zr2O12

Fumihiro Yonemoto, Atsuki Nishimura, Munekazu Motoyama, Nobuo Tsuchimine, Susumu Kobayashi, Yasutoshi Iriyama

Publisher page

Abstract

Abstract This paper reports on the cycling stability of Li plating/stripping on Li6.6La3Zr1.6Ta0.4O12 [LLZ(Ta0.4)] with high sintering density at 25, 60, and 100 °C. Plated/stripped Li thicknesses are sequentially increased to 200 nm, 1.0 μm, and 2.0 μm after every ten cycles. The overpotential gradually increases with cycling Li plating/stripping processes, and the cells eventually short-circuit at 25 and 60 °C. However, the cycling stability of Li plating/stripping significantly improves at 100 °C, and the short-circuiting is prevented perfectly. Moreover, the cycling stability of Li plating/stripping at 25 °C is dramatically improved by pre-cycling the cell at 100 °C. Only heating a cell with Li metal at 100 °C for the same duration does not improve the cycling stability of the cell. It is hence considered that forced migrations of Li atoms and ions across entire Li/LLZ(Ta0.4) interfaces at 100 °C change the properties of the interfacial regions even for the following plating/stripping cycles at 25 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Zheng · Nat. Nanotech. · 2014 · 9 · 61810.1038/nnano.2014.152 ↗
2. Yan · Nat. Mater. · 2016 · 1 · 110.24909/NOSM2016111.1 ↗
3. Hovington · Nano Lett. · 2015 · 15 · 267110.1021/acs.nanolett.5b00326 ↗
4. Lee · Sci. Rep. · 2016 · 6
5. Xu · Energy Environ. Sci. · 2014 · 7 · 51310.1039/C3EE40795K ↗
6. Nazar · MRS Bull. · 2014 · 39 · 43610.1557/mrs.2014.86 ↗
7. Ma · Chem. Commun. · 2014 · 50 · 1420910.1039/C4CC05535G ↗
8. Kozen · ACS Nano · 2015 · 9 · 588410.1021/acsnano.5b02166 ↗
9. Sun · J. Am. Chem. Soc. · 2014 · 136 · 894110.1021/ja501877e ↗
10. McCloskey · J. Phys. Chem. Lett. · 2015 · 6 · 458110.1021/acs.jpclett.5b01814 ↗
11. Ishiguro · J. Electrochem. Soc. · 2014 · 161 · A66810.1149/2.013405jes ↗
12. Islam · J. Electrochem. Soc. · 2014 · 161 · E300910.1149/2.005408jes ↗
13. Hayashi · J. Power Sources · 2003 · 5 · 701
14. Lin · Angew. Chem. Int. Ed. · 2013 · 52 · 746010.1002/anie.201300680 ↗
15. Nagao · Electrochem. Comm. · 2012 · 22 · 17710.1016/j.elecom.2012.06.015 ↗
16. Agostini · Solid State Ionics · 2013 · 244 · 4810.1016/j.ssi.2013.04.024 ↗
17. Neudecker · J. Electrochem. Soc. · 2000 · 147 · 51710.1149/1.1393226 ↗
18. Kato · Nat. Energy · 2016 · 1 · 1603010.1038/nenergy.2016.30 ↗
19. Janek · Nat. Energy · 2016 · 1 · 1614110.1038/nenergy.2016.141 ↗
20. Dudney · 2015
21. Murugan · Angew. Chem. Int. Ed. · 2007 · 46 · 777810.1002/anie.200701144 ↗
22. Ohta · J. Power Sources · 2011 · 196 · 334210.1016/j.jpowsour.2010.11.089 ↗
23. Sudo · Solid State Ionics · 2014 · 262 · 15110.1016/j.ssi.2013.09.024 ↗
24. Nagao · Phys. Chem. Chem. Phys. · 2013 · 1510.1039/c3cp51059j ↗
25. Sakuda · J. Ceram. Soc. Jp. · 2013 · 121 · 94610.2109/jcersj2.121.946 ↗
26. Yu · Chem. Mater. · 2016 · 28 · 19710.1021/acs.chemmater.5b03854 ↗
27. Moroe · J. Electrochem. Soc. · 2005 · 152 · A39610.1149/1.1850854 ↗
28. Jow · J. Electrochem. Soc. · 1983 · 130 · 73710.1149/1.2119795 ↗
29. Meyer · Solid State Ionics · 1983 · 9–10 · 68910.1016/0167-2738(83)90315-6 ↗
30. Janek · Solid State Ionics · 1997 · 101–103 · 72110.1016/S0167-2738(97)00180-X ↗
31. Janek · Solid State Ionics · 2000 · 131 · 12910.1016/S0167-2738(00)00628-7 ↗
32. Rohnke · Solid State Ionics · 2006 · 17710.1016/j.ssi.2005.12.002 ↗
33. Solid electrode-inorganic solid electrolyte interface for advanced all-solid-state rechargeable lithium batteries
34. Hiratani · Solid State Ionics · 1988 · 28–30 · 140610.1016/0167-2738(88)90394-3 ↗
35. Akolkar · J. Power Sources · 2014 · 246 · 8410.1016/j.jpowsour.2013.07.056 ↗
36. Wachtman · J. Am. Ceram. Soc. · 1959 · 42 · 25410.1111/j.1151-2916.1959.tb15462.x ↗
37. Hess · J. Electrochem. Soc. · 2015 · 162 · A308410.1149/2.0121502jes ↗
38. Awaka · J. Solid State Chem. · 2009 · 182 · 204610.1016/j.jssc.2009.05.020 ↗
39. Logéat · Solid State Ionics · 2012 · 206 · 3310.1016/j.ssi.2011.10.023 ↗
40. Ren · Electrochem. Commun. · 2015 · 57 · 2710.1016/j.elecom.2015.05.001 ↗
41. Kato · J. Power Sources · 2014 · 260 · 29210.1016/j.jpowsour.2014.02.102 ↗
42. Pichl · Mater. Sci. Engin. A · 1999 · 273−275 · 20810.1016/S0921-5093(99)00372-X ↗