journal article·2011-12

Enhanced sinterability of BaZr0.1Ce0.7Y0.1Yb0.1O3−δ by addition of nickel oxide

Yong Liu, Lei Yang, Mingfei Liu, Zhiyuan Tang, Meilin Liu

Journal of Power Sources· Volume 196· Issue 23
Publisher page

Abstract

Abstract The effect of nickel oxide addition on the sintering behavior and electrical properties of BaZr0.1Ce0.7Y0.1Yb0.1O3−δ (BZCYYb) as an electrolyte for solid oxide fuel cells was systematically studied. Results suggest that the addition of a small amount (∼1 wt%) of NiO to BZCYYb greatly promoted densification, achieving ∼96% of the theoretical density after sintering at 1350 °C in air for 3 h (reducing the sintering temperature by ∼200 °C). Further, a sample sintered at 1450 °C for 3 h showed high open circuit voltages (OCVs) when used as the electrolyte membrane to separate the two electrodes under typical SOFC operating conditions, indicating that the electrical conductivity of the electrical conductivity of the BZCYYb was not adversely affected by the addition of ∼1 wt% NiO.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalysis and Oxidation Reactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Yang · Science · 2009 · 326 · 12610.1126/science.1174811 ↗
2. Yang · Nat. Commun. · 2011 · 2 · 23710.1038/ncomms1359 ↗
3. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
4. Haile · Acta Mater. · 2003 · 51 · 598110.1016/j.actamat.2003.08.004 ↗
5. Kreuer · Ann. Rev. Mater. Res. · 2003 · 33 · 33310.1146/annurev.matsci.33.022802.091825 ↗
6. Kreuer · Solid State Ionics · 1999 · 125 · 28510.1016/S0167-2738(99)00188-5 ↗
7. Kreuer · Solid State Ionics · 1997 · 97 · 110.1016/S0167-2738(97)00082-9 ↗
8. Zuo · Adv. Mater. · 2006 · 18 · 331810.1002/adma.200601366 ↗
9. Zuo · J. Power Sources · 2006 · 159 · 129110.1016/j.jpowsour.2005.12.042 ↗
10. Zuo · Electrochem. Solid State Lett. · 2005 · 8 · J3510.1149/1.2081807 ↗
11. Zuo · Chem. Mater. · 2006 · 18 · 464710.1021/cm0518224 ↗
12. Bonanos · Solid State Ionics · 1995 · 79 · 16110.1016/0167-2738(95)00056-C ↗
13. Gopalan · J. Electrochem. Soc. · 1993 · 140 · 106010.1149/1.2056197 ↗
14. Babilo · J. Am. Ceram. Soc. · 2005 · 88 · 236210.1111/j.1551-2916.2005.00449.x ↗
15. Costa · Solid State Ionics · 2009 · 180 · 89110.1016/j.ssi.2009.02.018 ↗
16. Azad · J. Alloys Compd. · 2002 · 334 · 11810.1016/S0925-8388(01)01785-6 ↗
17. Tsai · Solid State Ionics · 2010 · 181 · 108310.1016/j.ssi.2010.06.028 ↗
18. Marder · J. Eur. Ceram. Soc. · 2011 · 31 · 105710.1016/j.jeurceramsoc.2010.12.032 ↗
19. Mendelson · J. Am. Ceram. Soc. · 1969 · 52 · 44310.1111/j.1151-2916.1969.tb11975.x ↗
20. Tong · Solid State Ionics · 2010 · 181 · 49610.1016/j.ssi.2010.02.008 ↗
21. Tong · J. Mater. Chem. · 2010 · 20 · 633310.1039/c0jm00381f ↗
22. Haile · J. Mater. Sci. · 2001 · 36 · 114910.1023/A:1004877708871 ↗
23. Takahash · Electrochim. Acta · 1967 · 12 · 2110.1016/0013-4686(67)85002-3 ↗