CuMn1.8O4 protective coatings on metallic interconnects for prevention of Cr-poisoning in solid oxide fuel cells
Source abstract
Abstract
Abstract Cr-poisoning of the cathodes due to the presence of metallic interconnects is detrimental to the performance of intermediate temperature solid oxide fuel cell stacks. Applying a protective coating on the interconnect is an effective solution to preventing Cr-poisoning. In this study, the application of a protective CuMn1.8O4 spinel coating is explored. Dense coatings are deposited on both metallic flat plates and meshes by electrophoretic deposition followed by thermal densification steps. The coating is found to be a mixture of Mn3O4 and cubic spinel phases at room temperature but is a pure cubic spinel phase between 750 °C and 850 °C. A reaction layer between the Cr2O3 scale at the coating/interconnect interface and CuMn1.8O4 coating is found to be a mixture of (Cu,Mn,Cr)3-xO4 cubic spinel phases with Cr-rich precipitates believed to be Cr2O3, indicating that the coating layer acts as a Cr getter. Solubility experiments show that 1 mol of the CuMn1.8O4 phase can getter at least 1.83 mol of Cr2O3 at 800 °C. Electrochemical testing of cells in the presence of coated interconnects show that the CuMn1.8O4 coating getters Cr effectively for 12 days at 800 °C, leading to no performance loss of the cell due to Cr-poisoning.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. EG&G Technical Services, Inc · 2004
2. O'Hayre · 2016
3. A review of recent progress in coatings, surface modifications and alloy developments for solid oxide fuel cell ferritic stainless steel interconnects10.1016/j.jpowsour.2009.09.069 ↗
4. Development of interconnect materials for solid oxide fuel cells10.1016/S0921-5093(02)00736-0 ↗
5. Chromium deposition and poisoning of cathodes of solid oxide fuel cells–a review10.1016/j.ijhydene.2013.10.042 ↗
6. Reduced area specific resistance for iron-based metallic interconnects by surface oxide coatings10.1016/S0025-5408(01)00506-2 ↗
7. Yttrium, cobalt and yttrium/cobalt oxide coatings on ferritic stainless steels for SOFC interconnects10.1016/j.jpowsour.2005.07.052 ↗
8. LaCrO3-based coatings on ferritic stainless steel for solid oxide fuel cell interconnect applications10.1016/j.surfcoat.2003.05.003 ↗
9. Evaluation of perovskite overlay coatings on ferritic stainless steels for SOFC interconnect applications10.1149/1.2239371 ↗
10. Electrical conductivity and thermal expansion of spinels at elevated temperatures10.1111/j.1551-2916.2007.01522.x ↗
11. Recent development of SOFC metallic interconnect10.1016/S1005-0302(10)60049-7 ↗
12. Thermal growth and performance of manganese cobaltite spinel protection layers on ferritic stainless steel SOFC interconnects10.1149/1.1990462 ↗
13. Conductive protection layers on oxidation resistant alloys for SOFC interconnect applications10.1016/j.surfcoat.2006.08.082 ↗
14. Oxidation kinetics of Mn1.5Co1.5O4-coated Haynes 230 and Crofer 22 APU for solid oxide fuel cell interconnects10.1149/1.3391820 ↗
15. Interactions between SOFC interconnect coating materials and chromia10.1111/j.1551-2916.2011.04749.x ↗
16. Formation of spinel reaction layers in manganese cobaltite–coated Crofer22 APU for solid oxide fuel cell interconnects10.1016/j.jpowsour.2012.07.091 ↗
17. Highly dense Mn-Co spinel coating for protection of metallic interconnect of solid oxide fuel cells10.1149/2.0541414jes ↗
18. Evaluating electrophoretically deposited Cu-Mn-O spinel coatings on stainless steel substrates used in solid oxide fuel cell interconnects
19. Spinel coatings for UNS 430 stainless steel interconnects, surf10.1016/j.surfcoat.2006.10.011 ↗
20. Oxidation and electrical conductivity behavior of spinel coatings for metallic interconnects of solid oxide fuel cells10.5006/1.3278404 ↗
21. Evaluation of electrophoretically deposited CuMn1.8O4 spinel coatings on Crofer 22 APU for solid oxide fuel cell interconnects10.1149/1.2975367 ↗
22. (Mn,Cu)3O4 based conductive coatings as effective barriers to high-temperature oxidation of metallic interconnects for solid oxide fuel cells10.1007/s10008-013-2245-6 ↗
23. Development of Cu1.3Mn1.7O4 spinel coating on ferritic stainless steel for solid oxide fuel cell interconnects10.1016/j.jpowsour.2014.10.017 ↗
24. Deposition of La0.8Sr0.2Cr0.97V0.03O3 and MnCr2O4 thin films on ferritic alloy for solid oxide fuel cell application10.1016/j.surfcoat.2007.07.046 ↗
25. Electrophoretic deposition of (Mn,Co)3O4 spinel coating for solid oxide fuel cell interconnects10.1016/j.jpowsour.2011.05.053 ↗
26. Fabrication of Mn–Co spinel coatings on Crofer 22 APU stainless steel by electrophoretic deposition for interconnect applications in solid oxide fuel cells10.1111/ijac.12013 ↗
27. Cu1.3Mn1.7O4 spinel coatings deposited by electrophoretic deposition on Crofer 22 APU substrates for solid oxide fuel cell applications10.1016/j.surfcoat.2016.09.028 ↗
28. Effect of Laves phase strengthening on the mechanical properties of high Cr ferritic steels for solid oxide fuel cell interconnect application10.1016/j.msea.2011.03.112 ↗
29. Roles of humidity and cathodic current in chromium poisoning of Sr-doped LaMnO3-based cathodes in solid oxide fuel cells10.1016/j.jpowsour.2017.06.005 ↗
30. Chromium poisoning effects on performance of (La,Sr)MnO3-based cathode in anode-supported solid oxide fuel cells10.1149/2.0441707jes ↗
31. Evaluation of the oxidation and Cr evaporation properties of selected FeCr alloys used as SOFC interconnects10.1016/j.ijhydene.2013.09.044 ↗
32. Mitigation of chromium poisoning of cathodes in solid oxide fuel cells employing CuMn1.8O4 spinel coating on metallic interconnect10.1016/j.jpowsour.2017.11.069 ↗