Mechanistic investigation of silicon-graphite/LiNi0.8Mn0.1Co0.1O2 commercial cells for non-intrusive diagnosis and prognosis
Source abstract
Abstract
Due to their high energy density, lithium-ion batteries with blended silicon-graphite (Si-Gr) anodes and nickel-rich (NMC) cathodes have been regarded as one of the most promising technologies for next-generation consumer electronics and electric vehicles. However, there are still several technical challenges to overcome for successful wide-spread adoption; in particular, deciphering the degradation phenomena remains complex and challenging, as the blended nature of the electrode creates a new paradigm, with the Si/Gr ratio likely changing with aging. Although ex-situ techniques have been used, a set of in-operando tools that enable diagnosis and prognosis on this technology has yet to be developed. Herein, we present a mechanistic investigation that generates a complete degradation mapping coupled with proposed aging features of interest, to attain accurate diagnosis and prognosis. The mechanistic model allows analyzing aging modes that display incubation periods as a potential prelude to thermodynamic plating, and the identification via incremental capacity of unique silicon features that change predictably as it degrades. A comprehensive look-up table summarizing key features is provided to provide support both to scientists and engineers on designing next-generation battery management systems for this technology.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Extraction and Separation Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Li-ion battery materials: present and future10.1016/j.mattod.2014.10.040 ↗
2. Review on recent progress of nanostructured anode materials for Li-ion batteries10.1016/j.jpowsour.2013.11.103 ↗
3. The lithium-ion battery: State of the art and future perspectives10.1016/j.rser.2018.03.002 ↗
4. Silicon based lithium-ion battery anodes: a chronicle perspective review10.1016/j.nanoen.2016.11.013 ↗
5. Nickel-rich layered lithium transition-metal oxide for high-energy lithium-ion batteries10.1002/anie.201409262 ↗
6. An epoxy-silane approach to prepare anode materials for rechargeable lithium ion batteries10.1149/1.2048667 ↗
7. Pyrolyzed polysiloxanes for use as anode materials in lithium-ion batteries10.1149/1.1837828 ↗
8. 25th anniversary article: understanding the lithiation of silicon and other alloying anodes for lithium-ion batteries10.1002/adma.201301795 ↗
9. High-performance lithium battery anodes using silicon nanowires10.1038/nnano.2007.411 ↗
10. Nanoscale silicon as anode for Li-ion batteries: the fundamentals, promises, and challenges10.1016/j.nanoen.2015.08.025 ↗
11. Novel strategy to improve the Li-storage performance of micro silicon anodes10.1016/j.jpowsour.2017.03.020 ↗
12. Pure silicon thin-film anodes for lithium-ion batteries: a review10.1016/j.jpowsour.2018.12.068 ↗
13. Recent progress on silicon-based anode materials for practical lithium-ion battery applications10.1016/j.ensm.2018.07.014 ↗
14. Silicon-based materials as high capacity anodes for next generation lithium ion batteries10.1016/j.jpowsour.2014.05.096 ↗
15. Integration of graphite and silicon anodes for the commercialization of high-energy lithium-ion batteries
16. Comparison of the structural and electrochemical properties of layered Li[NixCoyMnz]O2 (x = 1/3, 0.5, 0.6, 0.7, 0.8 and 0.85) cathode material for lithium-ion batteries10.1016/j.jpowsour.2013.01.063 ↗
17. Designing principle for Ni-rich cathode materials with high energy density for practical applications10.1016/j.nanoen.2018.04.062 ↗
18. A perspective on nickel-rich layered oxide cathodes for lithium-ion batteries10.1016/j.ensm.2016.10.007 ↗
19. Modeling and simulation of inhomogeneities in a 18650 nickel-rich, silicon-graphite lithium-ion cell during fast charging10.1016/j.jpowsour.2018.11.043 ↗
20. Degradation mechanisms of high capacity 18650 cells containing Si-graphite anode and nickel-rich NMC cathode10.1016/j.electacta.2018.11.194 ↗
21. Reversible self-discharge and calendar aging of 18650 nickel-rich, silicon-graphite lithium-ion cells10.1016/j.jpowsour.2019.03.109 ↗
22. Operando quantification of (De)Lithiation behavior of silicon-graphite blended electrodes for lithium-ion batteries
23. Differentiating the degradation phenomena in silicon-graphite electrodes for lithium-ion batteries10.1149/2.1921712jes ↗
24. Performance and failure analysis of full cell lithium ion battery with LiNi0.8Co0.15Al0.05O2 and silicon electrodes10.1016/j.jpowsour.2019.226884 ↗
25. Synthesize battery degradation modes via a diagnostic and prognostic model10.1016/j.jpowsour.2012.07.016 ↗
26. Performance and cost of materials for lithium-based rechargeable automotive batteries10.1038/s41560-018-0107-2 ↗
27. Driving change in the battery industry10.1038/nnano.2014.92 ↗
28. Identify capacity fading mechanism in a commercial LiFePO4 cell10.1016/j.jpowsour.2009.05.036 ↗
29. Durability and reliability of EV batteries under electric utility grid operations: path dependence of battery degradation10.1149/2.0421805jes ↗
30. State of health battery estimator enabling degradation diagnosis: model and algorithm description10.1016/j.jpowsour.2017.05.121 ↗
31. Intrinsic variability in the degradation of a batch of commercial 18650 lithium-ion cells10.3390/en11051031 ↗
32. Electrode behavior RE-visited: monitoring potential windows, capacity loss, and impedance changes in Li 1.03 (Ni 0.5 Co 0.2 Mn 0.3) 0.97 O 2/Silicon-Graphite full cells10.1149/2.0271606jes ↗
33. Evaluation of commercial lithium-ion cells based on composite positive electrode for plug-in hybrid electric vehicle (PHEV) applications: IV. Over-discharge phenomena10.1149/2.0481509jes ↗
34. Degradation diagnosis of lithium-ion batteries with a LiNi0.5Co0.2Mn0.3O2 and LiMn2O4 blended cathode using dV/dQ curve analysis10.1016/j.jpowsour.2018.04.043 ↗
35. Battery durability and reliability under electric utility grid operations: path dependence of battery degradation10.1149/2.0971910jes ↗
36. Battery energy storage system modeling: investigation of intrinsic cell-to-cell variations10.1016/j.est.2019.02.016 ↗
37. Fast charging technique for high power LiFePO4 batteries: a mechanistic analysis of aging10.1016/j.jpowsour.2016.04.140 ↗
38. Performance degradation of high-power lithium-ion cells—electrochemistry of harvested electrodes10.1016/j.jpowsour.2007.03.071 ↗
39. Postmortem analysis of calendar-aged graphite/LiFePO4 cells10.1016/j.jpowsour.2013.01.147 ↗
40. Durability and reliability of electric vehicle batteries under electric utility grid operations. Part 1: cell-to-cell variations and preliminary testing10.3390/batteries2030028 ↗
41. Reproducibility of Li-ion cell reassembling processes and their influence on coin cell aging10.1016/j.est.2019.04.006 ↗
42. A guide to full coin cell making for academic researchers10.1149/2.1171902jes ↗
43. Alawa Central
44. CMC-citric acid Cu(II) cross-linked binder approach to improve the electrochemical performance of Si-based electrodes10.1016/j.electacta.2019.03.026 ↗
45. Phase diagram of LixC610.1103/PhysRevB.44.9170 ↗
46. Li 15 Si 4 formation in silicon thin film negative electrodes10.1149/2.0551602jes ↗
47. Crumpled graphene-encapsulated Si nanoparticles for lithium ion battery anodes10.1021/jz3006892 ↗
48. Kinetics accommodation in Li-ion mechanistic modeling10.1016/j.jpowsour.2019.227117 ↗