Stability of La0.6Sr0.4Co0.2Fe0.8O3/Ce0.9Gd0.1O2 cathodes during sintering and solid oxide fuel cell operation

Ragnar Kiebach, Wei-Wei Zhang, Wei Zhang, Ming Chen, Kion Norrman, Hsiang-Jen Wang, Jacob R. Bowen, Rasmus Barfod, Peter Vang Hendriksen

Publisher page

Abstract

Abstract Degradation phenomena of La0.58Sr0.4Co0.2Fe0.8O3/Ce0.9Gd0.1O2 (LSCF/CGO) cathodes were investigated via post-mortem analyses of an experimental solid oxide fuel cell (SOFC) stack tested at 700 °C for 2000 h using advanced electron microscopy (SEM-EDS, HR-TEM-EDS) and time-of-flight secondary ion mass spectrometry (TOF-SIMS). Similar studies were carried out on non-tested reference cells for comparison. The analysis focused on the LSCF/CGO cathode and the CGO barrier layer, as the cathode degradation can be a major contributor to the overall degradation in this type of SOFC. SEM-EDS and TOF-SIMS were used to investigate inter-diffusion across the barrier layer—electrolyte interface and the barrier layer—cathode interface. In addition, TOF-SIMS data were employed to investigate impurity distribution before and after testing. HR-TEM-EDS was used to investigate possible phase segregation in the LSCF and to look for reaction between the phases. The results show that phase separation and inter-diffusion across the cathode–barrier layer interface and the barrier layer–electrolyte interface happened mainly during sintering and cathode firing, and to a very little degree during the test period.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Menzler · J. Mater. Sci. · 2010 · 45 · 310910.1007/s10853-010-4279-9 ↗
2. Blum · J. Power Sources · 2013 · 241 · 47710.1016/j.jpowsour.2013.04.110 ↗
3. Liu · Int. J. Hydrogen Energy · 2012 · 37 · 861310.1016/j.ijhydene.2012.02.139 ↗
4. Wang · Solid Sate Ionics · 2005 · 176 · 45710.1016/j.ssi.2004.09.007 ↗
5. Mai · Solid State Ionics · 2006 · 177 · 210310.1016/j.ssi.2005.12.010 ↗
6. Jordan · Solid State Ionics · 2008 · 179 · 91910.1016/j.ssi.2007.12.008 ↗
7. Mai · Solid Sate Ionics · 2006 · 177 · 196510.1016/j.ssi.2006.06.021 ↗
8. Mai · Solid Sate Ionics · 2005 · 176 · 134110.1016/j.ssi.2005.03.009 ↗
9. Steele · Solid State Ionics · 2000 · 134 · 310.1016/S0167-2738(00)00709-8 ↗
10. Simner · Electrochem. Solid-State Lett. · 2006 · 9 · A47810.1149/1.2266160 ↗
11. Tu · J. Power Sources · 2004 · 127 · 28410.1016/j.jpowsour.2003.09.025 ↗
12. Tietz · J. Power Sources · 2006 · 156 · 2010.1016/j.jpowsour.2005.08.015 ↗
13. Yokokawa · J. Alloys Compd. · 2008 · 452 · 4110.1016/j.jallcom.2006.12.150 ↗
14. Martínez-Amesti · J. Power Sources · 2008 · 185 · 40110.1016/j.jpowsour.2008.06.049 ↗
15. Uhlenbruck · Solid State Ionics · 2009 · 180 · 41810.1016/j.ssi.2009.01.014 ↗
16. Knibbe · J. Am. Ceram. Soc. · 2010 · 93 · 287710.1111/j.1551-2916.2010.03763.x ↗
17. Komatsu · J. Power Sources · 2008 · 176 · 13210.1016/j.jpowsour.2007.10.068 ↗
18. Komatsu · J. Power Sources · 2009 · 193 · 58510.1016/j.jpowsour.2009.04.014 ↗
19. Nielsen · Solid State Ionics · 2010 · 181 · 51710.1016/j.ssi.2010.02.018 ↗
20. Zhang · Micros. Microanal. · 2013 · 19 · 50110.1017/S1431927613000019 ↗
21. Kindermann · Solid State Ionics · 1996 · 89 · 21510.1016/0167-2738(96)00366-9 ↗
22. Li · J. Eur. Ceram. Soc. · 2001 · 21 · 290310.1016/S0955-2219(01)00218-7 ↗
23. Kilo · J. Eur. Ceram. Soc. · 2000 · 20 · 206910.1016/S0955-2219(00)00072-8 ↗
24. Bekale · Philos. Mag. · 2008 · 88 · 110.1080/14786430701708331 ↗
25. Borgenstam · J. Phase Equilib. · 2000 · 21 · 26910.1361/105497100770340057 ↗
26. Hauch · J. Electrochem. Soc. · 2007 · 154 · A61910.1149/1.2733861 ↗
27. Kiebach · Dalton Trans. · 2014 · 40 · 1494910.1039/C4DT01053A ↗
28. Izuki · J. Power Sources · 2011 · 196 · 723210.1016/j.jpowsour.2010.11.013 ↗
29. Bekale · Philos. Mag. · 2007 · 88 · 110.1080/14786430701708331 ↗
30. Jun · Electrochim. Acta · 2013 · 89 · 37210.1016/j.electacta.2012.11.002 ↗
31. Kromp · Fuel Cells · 2013 · 13 · 59810.1002/fuce.201200165 ↗
32. Badwal · Solid State Ionics · 1997 · 99 · 29710.1016/S0167-2738(97)00247-6 ↗
33. Matsuzaki · J. Electrochem. Soc. · 2001 · 148 · A12610.1149/1.1339869 ↗
34. Yasuda · Proc. Electrochem. Soc. · 2001 · 131
35. Kim · Ceram. Eng. Sci. Proc. · 2005 · 26 · 12910.1002/9780470291238.ch16 ↗
36. Fergus · Int. J. Hydrogen Energy · 2007 · 32 · 366410.1016/j.ijhydene.2006.08.005 ↗
37. Bentzen · Fuel Cells · 2009 · 9 · 82310.1002/fuce.200800143 ↗
38. Kim · J. Electrochem. Soc. · 2006 · 153 · A88010.1149/1.2181435 ↗
39. Zhen · Electrochem. Solid-State Lett. · 2008 · 11 · B4210.1149/1.2828212 ↗
40. Chu · 2008