An electrochemically roughened Cu current collector for Si-based electrode in Li-ion batteries
Source abstract
Abstract
An electrochemically roughened copper foil was evaluated as a current collector for micrometric Si powder (ball-milled) based electrodes prepared by the conventional slurry-coating method. The formation of a bunch of copper nanowires on the current collector provides a rough surface, which enhances the adhesion of the Si composite electrode as confirmed from scratch tests. This produces a major decrease of the irreversible capacity associated with the electrical disconnection of the Si particles with cycling, which results in a great improvement of the electrode cycle life. With such a roughened Cu current collector, the micrometric Si-based electrode is able to maintain a discharge capacity of 1200 mAh g−1 for at least 1000 cycles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Semiconductor materials and devices · Supercapacitor Materials and Fabrication
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Beaulieu · Electrochem. Solid-State Lett. · 2001 · 4 · A13710.1149/1.1388178 ↗
2. Ryu · Electrochem. Solid-State Lett. · 2004 · 7 · A30610.1149/1.1792242 ↗
3. Winter · Zeit. Phys. Chem. · 2009 · 223 · 139510.1524/zpch.2009.6086 ↗
4. Oumellal · J. Mater. Chem. · 2011 · 21 · 620110.1039/c1jm10213c ↗
5. Mazouzi · J. Power Sources · 2012 · 220 · 18010.1016/j.jpowsour.2012.08.007 ↗
6. Kasavajjula · J. Power Sources · 2007 · 163 · 100310.1016/j.jpowsour.2006.09.084 ↗
7. Zhang · J. Power Sources · 2011 · 19 · 1310.1016/j.jpowsour.2010.07.020 ↗
8. Szczech · Energy Environ. Sci. · 2011 · 4 · 5610.1039/C0EE00281J ↗
9. Roginskaya · Russ. J. Electrochem. · 2008 · 44 · 99210.1134/S1023193508090024 ↗
10. Lee · J. Power Sources · 2004 · 129 · 27010.1016/j.jpowsour.2003.10.013 ↗
11. Guo · Mater. Sci. Eng. B · 2006 · 131 · 17310.1016/j.mseb.2006.04.008 ↗
12. Kim · J. Electrochem. Soc. · 2006 · 153 · A45510.1149/1.2158567 ↗
13. Takamura · J. Power Sources · 2004 · 129 · 9610.1016/j.jpowsour.2003.11.014 ↗
14. Takamura · J. Power Sources · 2006 · 158 · 140110.1016/j.jpowsour.2005.10.081 ↗
15. Nguyen · Electrochim. Acta · 2010 · 55 · 302610.1016/j.electacta.2009.12.067 ↗
16. Uehara · J. Power Sources · 2005 · 146 · 44110.1016/j.jpowsour.2005.03.097 ↗
17. Zhang · Electrochim. Acta · 2008 · 53 · 566010.1016/j.electacta.2008.03.017 ↗
18. Hwang · J. Power Sources · 2009 · 194 · 106110.1016/j.jpowsour.2009.05.047 ↗
19. Hwang · Electrochim. Acta · 2011 · 56 · 673710.1016/j.electacta.2011.05.070 ↗
20. Li · J. Alloys Compd. · 2011 · 509 · 291910.1016/j.jallcom.2010.11.156 ↗
21. Xu · J. Electrochem. Soc. · 2010 · 157 · A76510.1149/1.3417076 ↗
22. Wolf · J. Power Sources · 2009 · 190 · 15710.1016/j.jpowsour.2008.07.035 ↗
23. Chen · Adv. Funct. Mater. · 2011 · 21 · 38010.1002/adfm.201001475 ↗
24. Yu · Adv. Energy Mater. · 2012 · 2 · 6810.1002/aenm.201100634 ↗
25. Kim · Electrochim. Acta · 2008 · 53 · 450010.1016/j.electacta.2008.01.050 ↗
26. Jiang · Electrochem. Commun. · 2007 · 9 · 93010.1016/j.elecom.2006.11.031 ↗
27. Sa · J. Power Sources · 2012 · 208 · 4610.1016/j.jpowsour.2012.02.020 ↗
28. Rousselot · J. Power Sources · 2012 · 202 · 26210.1016/j.jpowsour.2011.11.045 ↗
29. M. Gauthier, D. Mazouzi, D. Reyter, B. Lestriez, P. Moreau, B. Lestriez, D. Guyomard, L. Roué, Energy Environ. Sci. 2013, in press.
30. Mazouzi · Electrochem. Solid State Lett. · 2009 · 12 · A21510.1149/1.3212894 ↗
31. Reyter · J. Electrochem. Soc. · 2007 · 154 · K3610.1149/1.2746805 ↗
32. Gauthier · J. Power Sources · 2013 · 227 · 23710.1016/j.jpowsour.2012.11.047 ↗
33. Etiemble · EWGAE Proc. · 2012 · E30 · 1