In this article, we develop a 3D, continuum-level damage model implemented on statistically generated LixNi0.5Mn0.3Co0.2O2 (NMC 532) secondary cathode particles. The primary motivation of the particle-level model is to inform cathode-particle design through detailed exploration of the influence of secondary and primary particle sizes on the damage predicted during operation, and determine charging profiles that reduce cathode fracture. The model considers NMC 532 secondary particles containing an agglomeration of anisotropic, randomly oriented grains. These brittle, Ni-based cathodes are prone to mechanical degradation, which reduces overall battery cycle life. The model predicts that secondary-particle fracture is primarily due to non-ideal grain interactions and high-rate charge demands. The model predicts that small secondary-particles with large grains develop significantly less damage than larger secondary particles with small grains. The model predicts most of the chemo-mechanical damage accumulates in the first few cycles. The chemo-mechanical model predicts monotonically increasing capacity fade with cycling and rate. Comparing to experimental results, the model is well suited for capturing initial capacity fade mechanisms, but additional physics is required to capture long-term capacity fade effects.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Fiber-reinforced polymer composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Batteries for electric and hybrid-electric vehicles10.1146/annurev-chembioeng-073009-100942 ↗
2. Aircraft batteries: current trend towards more electric aircraft10.1049/iet-est.2016.0019 ↗
3. Electrode materials, electrolytes, and challenges in nonaqueous lithium-ion capacitors
4. Mechanical and structural degradation of LiNixMnyCozO2 cathode in Li-ion batteries: An experimental study10.1149/2.1751713jes ↗
5. Electron backscatter diffraction for investigating lithium-ion electrode particle architectures
6. Mapping the architecture of single lithium ion electrode particles in 3D, using electron backscatter diffraction and machine learning segmentation10.1016/j.jpowsour.2020.229148 ↗
7. Electron backscatter diffraction for investigating lithium-ion electrode particle architectures
8. Oxygen release induced chemomechanical breakdown of layered cathode materials10.1021/acs.nanolett.8b01036 ↗
9. Corrosive fracture of electrodes in li-ion batteries10.1016/j.jmps.2018.07.021 ↗
10. Prospect and reality of Ni-rich cathode for commercialization
11. Capacity fading of Ni-rich Li[NixCoyMn1−x−y]O2 (0.6≤x≤0.95) cathodes for high-energy-density lithium-ion batteries: Bulk or surface degradation?10.1021/acs.chemmater.7b05269 ↗
12. Intergranular cracking as a major cause of long-term capacity fading of layered cathodes10.1021/acs.nanolett.7b00379 ↗
13. Single-crystal nickel-rich layered-oxide battery cathode materials: synthesis, electrochemistry, and intra-granular fracture10.1016/j.ensm.2020.01.027 ↗
14. High-voltage charging-induced strain, heterogeneity, and micro-cracks in secondary particles of a nickel-rich layered cathode material
15. Degradation mechanisms and mitigation strategies of nickel-rich NMC-based lithium-ion batteries
16. Intrinsic origins of crack generation in Ni-rich LiNi0.8Co0.1Mn0.1O2 layered oxide cathode material10.1038/srep39669 ↗
17. Grid indentation of mechanical properties of composite electrodes in Li-ion batteries10.1016/j.eml.2016.03.002 ↗
18. Recent advance in understanding the electro-chemo-mechanical behavior of lithium-ion batteries by electron microscopy10.1016/j.mtnano.2019.100040 ↗
19. Effect of electrolyte composition on rock salt surface degredation in NMC cathodes during high-voltage potential holds10.1016/j.nanoen.2018.10.065 ↗
20. Structural and chemical evolution of Li- and Mn-rich layered cathode material10.1021/cm5045978 ↗
21. Degradation mechanisms and mitigation strategies of nickel-rich NMC-based lithium-ion batteries
22. Thermally driven mesoscale chemomechanical interplay in Li0.5Ni0.6Mn0.2Co0.2O2 cathode materials10.1039/C8TA08973F ↗
23. Disintegration of meatball electrodes for LiNixMnyCozO2 cathode materials10.1007/s11340-017-0292-0 ↗
24. A shrinking-core model for the degredation of high-nickel cathodes (NMC811) in Li-ion batteries: Passivation layer growth and oxygen evolution10.1149/1945-7111/abdc71 ↗
25. A chemo-mechanical grain boundary model and its application to understand the damage of Li-ion battery materials10.1016/j.scriptamat.2020.03.027 ↗
26. Artificial generation of representative single Li-ion electrode particle architectures from microscopy data10.1038/s41524-021-00567-9 ↗
27. Lemaitre · 2012
28. Soille · 2013
29. Improving model-based fNIRS analysis using mesh-based anatomical and light-transport models
30. Fundamental mechanisms of fracture and its suppression in Ni-rich layered cathodes: Mechanics-based multiscale approaches10.1016/j.eml.2018.05.010 ↗
31. Slawinski · 2015
32. The FEniCS project version 1.5
33. 2012
34. Extreme fast charge challenges for lithium-ion battery: Variability and positive electrode issues10.1149/2.0731910jes ↗
35. Extended cycle life implications of fast charging for lithium-ion battery cathode10.1016/j.ensm.2021.07.001 ↗
36. Fictitious phase separation in Li layered oxides driven by electro-autocatalysis10.1038/s41563-021-00936-1 ↗
37. The interactions of composition and stress in crystalline solids10.6028/jres.089.026 ↗
38. Chemo-mechanical behavior of highly anisotropic and isotropic polycrystalline graphite particles during lithium intercalation10.1149/1945-7111/aba5d2 ↗
39. Computational analysis of chemo-mechanical behaviors of composite electrodes in Li-ion batteries10.1557/jmr.2016.302 ↗
40. A finite strain model of stress, diffusion, plastic flow, and electrochemical reactions in a lithium-ion half-cell10.1016/j.jmps.2011.01.003 ↗
41. Jelvehpour · 2016
42. On the fragmentation of active material secondary particles in lithium ion battery cathodes induced by charge cycling10.1016/j.eml.2016.03.018 ↗
43. Requirements for enabling extreme fast charging of high energy density Li-ion cells while avoiding lithium plating10.1149/2.0451908jes ↗
44. Single-particle model for a lithium-ion cell: Thermal behavior10.1149/1.3521314 ↗
45. Review and performance comparison of mechanical-chemical degredation models for lithium-ion batteries10.1149/2.0281914jes ↗
46. Characterization of electronic and ionic transport of Li1−xNi0.33Mn0.33Co0.33O2 (NMC333) and Li1−xNi0.50Mn0.20Co0.30O2 (NMC523) as a function of Li content10.1149/2.0131608jes ↗
47. Chemo-thermo-mechanical coupling in protonic ceramic fuel cells from fabrication to operation10.1149/2.1071912jes ↗
48. Vyshenska · 2018
49. Power and thermal characterization of a lithium-ion battery pack for hybrid-electric vehicles10.1016/j.jpowsour.2006.01.038 ↗
50. Galvanostatic intermittent titration and performance based analysis of LiNi0.5Co0.2Mn0.3O2 cathode10.1149/2.1701713jes ↗
51. Understanding structural changes in NMC Li-cells by in situ neutron diffraction10.1016/j.jpowsour.2014.01.010 ↗
52. The diffusion induced stress and cracking behavior of primary particle for Li-ion battery electrode10.1016/j.ijmecsci.2020.105608 ↗
53. Thermodynamically consistent modeling of elementary electrochemistry in lithium-ion batteries10.1016/j.electacta.2010.08.018 ↗
54. Electrode scale and electrolyte transport effects on extreme fast charging of lithium-ion cells10.1016/j.electacta.2020.135854 ↗
55. Quantification of inactive lithium and solid-electrolyte interface species on graphite electrodes after fast charging10.1021/acsenergylett.0c00859 ↗
56. A nonlocal model with strain-based damage10.1016/j.ijsolstr.2009.08.009 ↗
57. Fracture in quasi-brittle materials: a review of continuum damage-based approaches10.1016/S0013-7944(01)00082-0 ↗
58. Cracking in quasi-brittle materials using isotropic damage mechanics
59. A nonlocal continuum damage model for brittle fracture10.1016/j.engfracmech.2017.10.019 ↗
60. Localisation issues in local and nonlocal continuum approaches to fracture10.1016/S0997-7538(02)01211-1 ↗
61. Nonlocal continuum damage, localization instability and convergence10.1115/1.3173674 ↗
62. Gradient enhanced damage for quasi-brittle materials10.1002/(SICI)1097-0207(19961015)39:19<3391::AID-NME7>3.0.CO;2-D ↗
63. An anisotropic gradient damage model for quasi-brittle materials10.1016/S0045-7825(99)00213-3 ↗
64. A macroscopic gradient-enhanced damage model for deformation behavior of concrete under cyclic loadings10.1007/s00419-020-01669-4 ↗