An all-solid-state lithium ion battery electrolyte membrane fabricated by hot-pressing method
Source abstract
Abstract
Abstract A cross-linked polymer electrolyte membrane (SPE) was fabricated by a solvent-free hot-pressing method for all-solid-state lithium ion battery. The ionic conductivity of the electrolyte is 1.34 × 10 −3 S cm −1 and the decomposition potential is 4.87 V at the ethylene oxide (EO):LiN(SO 2 CF 3 ) 2 (LiTFSI) molar ratio of 20:1 and 120 °C. TG-DSC results show that the SPE is thermally stable up to 230 °C in argon atmosphere. The assembled LiFePO 4 /SPE/Li all-solid-state battery can stably work in the temperature range of 80–140 °C. At 120 °C, the initial discharge capacity of the battery is 156.7 mAh g −1 at 1C which is close to the theoretical capacity of the cathode material, showing that the solvent-free filming method is low-cost and environment-friendly for solid polymer electrolyte and all-solid-state lithium ion battery.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Scrosati · Electrochim. Acta · 2000 · 45 · 246110.1016/S0013-4686(00)00333-9 ↗
2. Shi · J. Mater. Chem. A · 2013 · 1 · 1501610.1039/c3ta13364h ↗
3. Lian · J. Membr. Sci. · 2014 · 469 · 6710.1016/j.memsci.2014.05.065 ↗
4. Wakihara · J. Solid State Electrochem. · 2012 · 16 · 84710.1007/s10008-012-1643-5 ↗
5. Li · ChemSusChem. · 2014 · 7 · 190110.1002/cssc.201400113 ↗
6. Etacheri · Energy Environ. Sci. · 2011 · 4 · 324310.1039/c1ee01598b ↗
7. Fenton · Polymer · 1973 · 14 · 58910.1016/0032-3861(73)90146-8 ↗
8. P. Vashishta, J.N. Mundy, G. Shenoy, North Holland, New York, 1979, pp. 131–136.
9. Edman · J. Mater. Res. · 2000 · 15 · 195010.1557/JMR.2000.0281 ↗
10. Goodenough · Chem. Mater. · 2009 · 22 · 58710.1021/cm901452z ↗
11. Krawiec · J. Power Sources · 1995 · 54 · 31010.1016/0378-7753(94)02090-P ↗
12. Croce · Electrochim. Acta · 2001 · 46 · 245710.1016/S0013-4686(01)00458-3 ↗
13. Yuan · J. Power Sources · 2013 · 240 · 65310.1016/j.jpowsour.2013.05.030 ↗
14. Schaetzl · J. Phys. Chem. C · 2014 · 118 · 1883610.1021/jp501786r ↗
15. Reddy · J. Power Sources · 2006 · 161 · 53510.1016/j.jpowsour.2006.02.104 ↗
16. Angulakshmi · J. Phys. Chem. C · 2014 · 118 · 2424010.1021/jp506464v ↗
17. Chiu · Macromolecules · 2004 · 37 · 842410.1021/ma0488156 ↗
18. Xiao · J. Membr. Sci. · 2009 · 334 · 11710.1016/j.memsci.2009.02.018 ↗
19. Lee · Solid State Ionics · 2014 · 255 · 610.1016/j.ssi.2013.11.010 ↗
20. Digar · Polymer · 2002 · 43 · 68110.1016/S0032-3861(01)00655-3 ↗
21. Santhosh · J. Power Sources · 2006 · 160 · 60910.1016/j.jpowsour.2006.01.091 ↗
22. Zhang · Macromolecules · 2003 · 36 · 917610.1021/ma0349276 ↗
23. Ünügür Çelik · Curr. Appl. Phys. · 2013 · 13 · 166810.1016/j.cap.2013.06.009 ↗
24. Oh · J. Power Sources · 2003 · 119 · 44210.1016/S0378-7753(03)00187-3 ↗
25. Soo · J. Electrochem. Soc. · 1999 · 146 · 3210.1149/1.1391560 ↗
26. Larkin · 2011
27. Papke · J. Phys. Chem. Solids · 1981 · 42 · 49310.1016/0022-3697(81)90030-5 ↗
28. Aihara · Electrochim. Acta · 2000 · 45 · 132110.1016/S0013-4686(99)00339-4 ↗
29. Stoeva · J. Am. Chem. Soc. · 2003 · 125 · 461910.1021/ja029326t ↗
30. Gadjourova · Nature · 2001 · 412 · 52010.1038/35087538 ↗
31. Ratner · MRS Bull. · 2000 · 25 · 3110.1557/mrs2000.16 ↗
32. Tominaga · Electrochim. Acta · 2000 · 45 · 128510.1016/S0013-4686(99)00333-3 ↗
33. Abraham · 1993
34. Wen · J. Electroanal. Chem. · 1996 · 408 · 11310.1016/0022-0728(96)04536-6 ↗
35. Rey · Electrochim. Acta · 1998 · 43 · 150510.1016/S0013-4686(97)10092-5 ↗
36. Echeverri · Macromolecules · 2012 · 45 · 606810.1021/ma3008509 ↗