Re-heating effect of Ni-rich cathode material on structure and electrochemical properties

Jae Hyeon Jo, Chang-Heum Jo, Hitoshi Yashiro, Sun-Jae Kim, Seung-Taek Myung

Publisher page

Abstract

Abstract The re-heating effect for Ni-rich Li[Ni 0.7 Mn 0.3 ]O 2 is investigated because the process is required in surface modification and removal of adhered water molecules. A representative binary Ni-rich Li[Ni 0.7 Mn 0.3 ]O 2 (in which cationic distribution in Li layers is not affected by heteroelements) is selected and synthesized via co-precipitation. The as-synthesized Ni-rich Li[Ni 0.7 Mn 0.3 ]O 2 is re-heated at 200 °C, 400 °C, and 600 °C, so that the resulting structural and electrochemical properties are compared by means of X-ray diffraction, transmission electron microscopy, time of flight-secondary ion spectroscopy, thermogravimetric analysis, high temperature X-ray diffraction, and electrochemical tests. Raising the re-heating temperature increases the occupancy of Ni 2+ in Li layers and accelerates the aggregation of lithium-related compounds such as Li 2 CO 3 and LiOH towards the particle surface. Among the several conditions tested, re-heating at 200 °C results in a negligible change in the crystal structure; specifically, Ni 2+ occupation in Li layers, higher capacity with good reversibility upon cycling tests, better rate capability, and thermal properties. Therefore, re-heating of cathode active materials, in particular Ni-rich compositions, should be considered to stabilize both electrode performances and thermal properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Supercapacitor Materials and Fabrication

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Sun · Nat. Mater. · 2009 · 8 · 32010.1038/nmat2418 ↗
2. Scrosati · J. Power Sources · 2010 · 195 · 241910.1016/j.jpowsour.2009.11.048 ↗
4. Etacheri · Energy Environ. Sci. · 2011 · 4 · 324310.1039/c1ee01598b ↗
5. Mizushima · Mater. Res. Bull. · 1980 · 15 · 78310.1016/0025-5408(80)90012-4 ↗
6. Amatucci · J. Electrochem. Soc. · 1996 · 143 · 111410.1149/1.1836594 ↗
7. Lu · Electrochem. Solid State Lett. · 2001 · 4
8. Makimara · J. Power Sources · 2003 · 119–121 · 15610.1016/S0378-7753(03)00170-8 ↗
9. Sun · Nat. Mater. · 2012 · 11 · 94210.1038/nmat3435 ↗
10. Yoon · Chem. Mater. · 2003 · 15 · 316110.1021/cm030220m ↗
11. Lee · Electrochim. Acta · 2008 · 53 · 603310.1016/j.electacta.2008.02.106 ↗
12. Myung · Chem. Mater. · 2006 · 18 · 165810.1021/cm052704j ↗
13. Sun · J. Electrochem. Soc. · 2007 · 154
14. Lee · J. Electrochem. Soc. · 2007 · 154
15. Myung · J. Power Sources · 2005 · 146 · 22210.1016/j.jpowsour.2005.03.031 ↗
16. Belharouak · J. Power Sources · 2003 · 132 · 24710.1016/S0378-7753(03)00529-9 ↗
17. Lee · Electrochim. Acta · 2004 · 50 · 93910.1016/j.electacta.2004.07.038 ↗
18. Myung · Chem. Mater. · 2005 · 17 · 369510.1021/cm050566s ↗
19. Zhecheva · Solid State Ion. · 1993 · 66 · 14310.1016/0167-2738(93)90037-4 ↗
20. Yoon · Chem. Mater. · 2003 · 15 · 316110.1021/cm030220m ↗
21. Noh · J. Power Sources · 2013 · 223 · 12110.1016/j.jpowsour.2013.01.063 ↗
22. Sun · ACS Appl Interfaces · 2013 · 5 · 1143410.1021/am403684z ↗
23. Roisnel · 2002
24. Shanon · Acta Cryst. · 1976 · A32 · 75110.1107/S0567739476001551 ↗
25. Cho · J. Electrochem. Soc. · 2014 · 161
26. Jo · Nano Res. · 2015 · 8 · 146410.1007/s12274-014-0631-8 ↗
27. Myung · J. Phys. Chem. C · 2010 · 114 · 471010.1021/jp9082322 ↗
28. Jo · J. Power Sources · 2015 · 282 · 51110.1016/j.jpowsour.2015.02.068 ↗
29. Guilmard · Chem. Mater. · 2003 · 15 · 448410.1021/cm030340u ↗