journal article·2015-10

Characterization of PEM fuel cell degradation by polarization change curves

Dario Bezmalinovic, Boris Simic, Frano Barbir

Publisher page

Abstract

Polarization change curves, defined as a difference between the polarization curve at the beginning of life and the actual polarization curve after the cell has been operational for some time, were used to analyze degradation of a PEM fuel cell exposed to voltage cycling as an accelerated stress test for electrocatalyst degradation. Degradation, i.e., loss of voltage was due to increase of activation losses and increase of resistance in the catalyst layer, both most likely due to the loss of catalyst electrochemically active area. The results of the polarization change curves analysis correspond to the findings of the periodic individual tests performed during the accelerated stress test, such as electrochemical impedance spectroscopy, cyclic voltammetry and linear sweep voltammetry. Therefore, this method has potential to be used as a relatively quick and simple, yet effective, degradation diagnostic tool.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. 2011
2. Durability of polymer electrolyte fuel cells
3. Degradation of a polymer exchange membrane fuel cell stack with Nafion® membranes of different thicknesses: part I. In situ diagnosis10.1016/j.jpowsour.2010.06.023 ↗
4. Degradation of a PEM fuel cell stack with Nafion® membranes of different thicknesses. Part II: Ex situ diagnosis10.1016/j.jpowsour.2012.01.074 ↗
5. Diagnostic tools for PEMFCs: from conception to implementation10.1016/j.ijhydene.2014.04.163 ↗
6. Local catalyst support degradation during polymer electrolyte fuel cell start-up and shutdown fuel cells, electrolyzers, and energy conversion10.1149/2.019212jes ↗
7. Carbon corrosion fingerprint development and de-convolution of performance loss according to degradation mechanism in PEM fuel cells10.1016/j.jpowsour.2013.03.033 ↗
8. Investigation of electrode composition of polymer fuel cells by electrochemical impedance spectroscopy10.1016/j.electacta.2008.01.084 ↗
9. Diagnosing degradation within PEM fuel cell catalyst layers using electrochemical impedance spectroscopy fuel cells and energy conversion10.1149/2.098205jes ↗
10. DOE fuel cell program: durability technical targets and testing protocols10.1149/1.2781004 ↗
11. The impact of cycle profile on PEMFC durability10.1149/1.2781035 ↗
12. Electrocatalyst durability under simulated automotive drive cycles10.1149/1.2981858 ↗
13. Electrochemical degradation: electrocatalyst and support durability
14. Simultaneous electrochemical measurements of ORR kinetics and Pt oxide formation/reduction
15. Electrochemical impedance of the cathode catalyst layer in, polymer electrolyte fuel cells10.1016/S0022-0728(99)00335-6 ↗
16. Measurement of catalyst layer electrolyte resistance in PEFCs using electrochemical impedance spectroscopy10.1149/1.1888367 ↗
17. Barbir · 2013
18. Characterization of membrane electrode assemblies in polymer electrolyte fuel cells using a.c. impedance spectroscopy10.1023/A:1020551609230 ↗