journal article·2024-07Open access

Review of factors affecting the performance degradation of Ni-YSZ fuel electrodes in solid oxide electrolyzer cells

Xiaolin Shao, Riyan Achmad Budiman, Takashi Sato, Mina Yamaguchi, Tatsuya Kawada, Keiji Yashiro

Abstract

Solid oxide electrolysis cells (SOECs) are an attractive technology for addressing the global environmental and energy problems caused by the heavy use of fossil fuels. The commercialization of SOECs is important for achieving decentralized hydrogen energy systems. SOECs have the advantages of high efficiency and a high conversion rate for the produced hydrogen compared to competing technologies. However, SOEC systems suffer from performance degradation after long-term operation, which mainly originates from the fuel electrode side, e.g., the Ni/yttria-stabilized zirconia (YSZ) electrode. The most common degradation phenomena are Ni agglomeration, Ni separation from the YSZ electrolyte, Ni re-oxidation, carbon deposition, and poisoning by gas impurities. These phenomena are mainly related to Ni migration occurring in the Ni/YSZ cathode owing to factors such as high water vapor concentration, high applied voltage or current density, high temperature, and the presence of gas impurities. In this review, the most important factors affecting Ni migration and other related degradation phenomena are summarized to provide insights into the degradation mechanisms of Ni/YSZ fuel electrodes. Based on these insights, strategies for improving the lifetime of Ni/YSZ fuel electrodes are discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Chemical Looping and Thermochemical Processes · Advanced Power Generation Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Technological development of hydrogen production by solid oxide electrolyzer cell (SOEC)10.1016/j.ijhydene.2008.02.048 ↗
2. Solid oxide electrolysis of H2O and CO2 to produce hydrogen and low-carbon fuels10.1007/s41918-021-00097-4 ↗
3. Degradation of solid oxide electrolysis cells: phenomena, mechanisms, and emerging mitigation strategies—a review10.1016/j.jmst.2019.07.026 ↗
4. Advancing the multiscale understanding on solid oxide electrolysis cells via modelling approaches: a review10.1016/j.rser.2021.110863 ↗
5. Stempien · 2013 · 216
6. Integration of solid oxide electrolyzer and Fischer-Tropsch: a sustainable pathway for synthetic fuel10.1016/j.apenergy.2015.10.053 ↗
7. Power-to-liquid via synthesis of methanol, DME or Fischer–Tropsch-fuels: a review10.1039/D0EE01187H ↗
8. Energy performance of Power-to-Liquid applications integrating biogas upgrading, reverse water gas shift, solid oxide electrolysis and Fischer-Tropsch technologies
9. Low carbon fuel production from combined solid oxide CO2 co-electrolysis and Fischer-Tropsch synthesis system: a modelling study10.1016/j.apenergy.2019.03.145 ↗
10. Modelling of SOEC-FT reactor: pressure effects on methanation process10.1016/j.apenergy.2016.10.095 ↗
11. A review on synthesis of methane as a pathway for renewable energy storage with a Focus on solid oxide electrolytic cell-based processes10.3389/fenrg.2020.570112 ↗
12. Synthetic natural gas via integrated high-temperature electrolysis and methanation: Part I—energy performance10.1016/j.est.2015.04.002 ↗
13. Exergy analysis of an integrated solid oxide electrolysis cell-methanation reactor for renewable energy storage10.1016/j.apenergy.2018.02.022 ↗
14. Highly efficient high temperature electrolysis10.1039/b718822f ↗
15. Singhal · 2003
16. Review—materials degradation of solid oxide electrolysis cells10.1149/2.0101611jes ↗
17. Transport properties of solid oxide electrolyte ceramics: a brief review10.1016/j.ssi.2004.06.015 ↗
18. Solid oxide electrolysis cell analysis by means of electrochemical impedance spectroscopy: a review10.1016/j.jpowsour.2014.01.110 ↗
19. Long term testing of solid oxide fuel cell stacks with yttria Stabilised zirconia electrolyte in the H2O electrolysis mode
20. Electrochemical performance and durability of flat-tube solid oxide electrolysis cells for H2O/CO2 co-electrolysis10.1016/j.ijhydene.2022.01.105 ↗
21. Study of solid oxide electrolysis cells operated in potentiostatic mode: effect of operating temperature on durability10.1016/j.cej.2021.129260 ↗
22. Ni migration in solid oxide cell electrodes: review and revised hypothesis10.1002/fuce.202100072 ↗
23. High temperature water electrolysis using metal supported solid oxide electrolyser cells (SOEC)10.1007/s10800-008-9672-6 ↗
24. Interfacial stability and cation diffusion across the LSCF/GDC interface10.1016/j.jpowsour.2010.11.013 ↗
25. Influence of the oxygen electrode and inter-diffusion barrier on the degradation of solid oxide electrolysis cells10.1016/j.jpowsour.2012.08.063 ↗
26. Durability of high performance Ni–yttria stabilized zirconia supported solid oxide electrolysis cells at high current density10.1016/j.jpowsour.2014.03.133 ↗
27. Interlayer modification for high-performance and stable solid oxide electrolysis cell10.1016/j.matlet.2021.131419 ↗
28. Influence of La0.6Sr0.4Co0.2Fe0.8O3-δ microstructure on GDC interlayer stability and cation diffusion across the LSCF/GDC/YSZ interfaces10.1149/2.0021614jes ↗
29. Air electrodes and related degradation mechanisms in solid oxide electrolysis and reversible solid oxide cells10.1016/j.rser.2021.110918 ↗
30. Stability of LSCF electrode with GDC interlayer in YSZ-based solid oxide electrolysis cell10.1016/j.ssi.2014.01.001 ↗
31. Solid oxide electrolysis cells: microstructure and degradation of the Ni/Yttria-Stabilized zirconia electrode10.1149/1.2967331 ↗
32. (Invited) on degradation mechanisms of Ni-YSZ fuel electrodes in solid oxide cells10.1149/11205.0071ecst ↗
33. Integrated 3D modeling unravels the measures to mitigate nickel migration in solid oxide fuel/electrolysis cells10.1039/D3TA06563D ↗
34. A parameter study of solid oxide electrolysis cell degradation: microstructural changes of the fuel electrode10.1016/j.electacta.2018.04.170 ↗
35. 3D microstructural characterization of Ni/yttria-stabilized zirconia electrodes during long-term CO2 electrolysis10.1039/D3TA01503C ↗
36. Study on the effects of polarization on local morphological change of nickel at active three-phase-boundary using patterned nickel-film electrode in solid oxide fuel cell anode10.1016/j.actamat.2017.05.051 ↗
37. Comparison of microstructural evolution of fuel electrodes in solid oxide fuel cells and electrolysis cells10.1016/j.jpowsour.2019.227599 ↗
38. Understanding the Ni migration in solid oxide cell: a Coupled experimental and modeling approach10.1149/1945-7111/acc1a3 ↗
39. Study of Ni-YSZ electrode capacitance and its correlation with the microstructure10.1149/1945-7111/acc1a4 ↗
40. Degradation of Ni-YSZ electrodes in solid oxide cells: impact of polarization and initial microstructure on the Ni evolution10.1149/2.1261915jes ↗
41. Microstructural comparison of solid oxide electrolyser cells operated for 6100 h and 9000 h10.1016/j.jpowsour.2014.10.188 ↗
42. Ni migration of Ni-YSZ electrode in solid oxide electrolysis cell: an integrated model study10.1016/j.jpowsour.2021.230660 ↗
43. Degradation of anode supported SOFCs as a function of temperature and current load10.1149/1.2193400 ↗
44. Relation between Ni particle shape change and Ni migration in Ni-YSZ electrodes - a hypothesis10.1002/fuce.201600222 ↗
45. Comprehensive hypotheses for degradation mechanisms in Ni-stabilized zirconia electrodes10.1149/09101.0613ecst ↗
46. Degradation phenomena in a solid oxide electrolysis cell after 9000 h of operation10.1016/j.jpowsour.2012.09.061 ↗
47. Degradation study by 3D reconstruction of a nickel-yttria stabilized zirconia cathode after high temperature steam electrolysis operation10.1016/j.jpowsour.2014.07.066 ↗
48. Impact of Nickel agglomeration on Solid Oxide Cell operated in fuel cell and electrolysis modes10.1016/j.jpowsour.2018.06.097 ↗
49. Microstructural degradation of Ni/YSZ electrodes in solid oxide electrolysis cells under high current10.1149/2.098308jes ↗
50. Oxygen nonstoichiometry, thermo-chemical stability and lattice expansion of La0.6Sr0.4FeO3−δ10.1016/j.ssi.2011.05.013 ↗
51. Fundamental mechanisms limiting solid oxide fuel cell durability10.1016/j.jpowsour.2008.02.016 ↗
52. Oxidation-induced degradation of SOFC Ni anodes at high fuel utilizations10.1149/06801.1345ecst ↗
53. Degradation of solid oxide cells during co-electrolysis of steam and carbon dioxide at high current densities10.1016/j.jpowsour.2016.08.055 ↗
54. Durability of high performance Ni-yttria stabilized zirconia supported solid oxide electrolysis cells at high current density10.1016/j.jpowsour.2014.03.133 ↗
55. Degradation mechanism and Ni migration in anode of solid oxide cells
56. Study of long-term stability of Ni-Zr0.92Y0.08O2-delta|Zr0.92Y0.08O2-delta|Ce0.9Gd0.1O2-delta |Pr0.6Sr0.4CoO3-delta at SOFC and SOEC mode10.3390/en14040824 ↗
57. 3D microstructural characterization of Ni/YSZ electrodes exposed to 1 Year of electrolysis testing10.1149/2.1281902jes ↗
58. A decade of solid oxide electrolysis improvements at DTU energy10.1149/07542.0003ecst ↗
59. Ni/YSZ electrodes structures optimized for increased electrolysis performance and durability10.1016/j.ssi.2016.06.003 ↗
60. Long-term performance prediction of solid oxide electrolysis cell (SOEC) for CO2/H2O co-electrolysis considering structural degradation through modelling and simulation10.1016/j.cej.2021.132158 ↗
61. Systematic parameter study on the influence of humidification and current density on SOEC degradation10.1149/06801.3553ecst ↗
62. Extreme management strategy and thermodynamic analysis of high temperature H2O/CO2 co-electrolysis for energy conversion10.1016/j.renene.2021.10.096 ↗
63. High-efficiency intermediate temperature solid oxide electrolyzer cells for the conversion of carbon dioxide to fuels10.1016/j.jpowsour.2013.11.047 ↗
64. Syngas production performance and degradation analysis of a solid oxide electrolyzer stack10.1016/j.jpowsour.2019.05.072 ↗
65. Carbon deposition in solid oxide cells during Co-electrolysis of H2O and CO210.1149/2.079403jes ↗
66. Role of initial microstructure on nickel-YSZ cathode degradation in solid oxide electrolysis cells10.1016/j.ijhydene.2014.09.057 ↗
67. Three-dimensional microstructural changes in the Ni–YSZ solid oxide fuel cell anode during operation10.1016/j.actamat.2012.02.041 ↗
68. High temperature Co-electrolysis of steam and CO2 in an SOC stack: performance and durability10.1002/fuce.201200169 ↗
69. Experimental characterization and modeling of the electrochemical reduction of CO2 in solid oxide electrolysis cells10.1016/j.electacta.2012.10.107 ↗
70. Carbon deposition and sulfur poisoning during CO2 electrolysis in nickel-based solid oxide cell electrodes10.1016/j.jpowsour.2017.10.097 ↗
71. CO2 electrolysis - gas impurities and electrode overpotential causing detrimental carbon deposition10.1016/j.jpowsour.2021.230108 ↗
72. Electrochemical performance of solid oxide electrolysis cell electrodes under high-temperature coelectrolysis of steam and carbon dioxide10.1016/j.jpowsour.2010.09.018 ↗
73. Carbon deposition on patterned nickel/yttria stabilized zirconia electrodes for solid oxide fuel cell/solid oxide electrolysis cell modes10.1016/j.jpowsour.2014.11.106 ↗
74. High temperature solid oxide H2O/CO2 co-electrolysis for syngas production10.1016/j.fuproc.2016.08.009 ↗
75. Electrolysis of carbon dioxide in solid oxide electrolysis cells10.1016/j.jpowsour.2009.02.093 ↗
76. Electrochemical performance and durability of flat-tube solid oxide electrolysis cells for H2O/CO2 co-electrolysis10.1016/j.ijhydene.2022.01.105 ↗
77. A comparative study of durability of solid oxide electrolysis cells tested for Co-electrolysis under galvanostatic and potentiostatic conditions10.1149/2.0151810jes ↗
78. TOF-SIMS characterization of impurity enrichment and redistribution in solid oxide electrolysis cells during operation10.1039/C4DT01053A ↗
79. Dependence of solid oxide fuel cell electrode microstructure parameters on focused ion beam – scanning electron microscopy resolution10.1016/j.ijhydene.2016.09.006 ↗
80. Poisoning of solid oxide electrolysis cells by impurities10.1149/1.3464804 ↗
81. Operando observations of active three phase boundary of patterned nickel- Yttria stabilized zirconia electrode in solid oxide cell10.1016/j.jpowsour.2022.231228 ↗
82. In-operando observations of Ni-YSZ patterned fuel electrodes under SOFC and SOEC operations10.1149/10301.1219ecst ↗
83. Carbon monoxide/carbon dioxide electrochemical conversion on patterned nickel electrodes operating in fuel cell and electrolysis cell modes10.1016/j.ijhydene.2016.01.019 ↗
84. Mechanism for reversible CO/CO2 electrochemical conversion on a patterned nickel electrode10.1016/j.jpowsour.2017.09.019 ↗
85. Elementary reaction modeling of reversible CO/CO2 electrochemical conversion on patterned nickel electrodes10.1016/j.jpowsour.2018.01.016 ↗
86. Influence of polarization on the morphological changes of nickel in fuel electrodes of solid oxide cells10.1149/1945-7111/ab6f5b ↗
87. Electrochemical performance and preliminary post-mortem analysis of a solid oxide cell stack with 20,000 h of operation10.1149/2.0541802jes ↗
88. Long-term behavior of a solid oxide electrolyzer (SOEC) stack10.1002/fuce.201900245 ↗
89. Degradation of flat-tube solid oxide electrolytic stack for co-electrolysis of H2O and CO2 under pulsed current10.1016/j.jpowsour.2023.233372 ↗
90. Mechanism of rate-limiting step switchover for reversible solid oxide cells in H2/H2O atmosphere10.1016/j.electacta.2019.135003 ↗
91. Post-test characterization of an SOFC short-stack after 17,000 hours of steady operation10.1149/1.3569994 ↗
92. Post-test characterization of a solid oxide fuel cell stack operated for more than 30,000 hours: the cell10.1016/j.jpowsour.2017.11.025 ↗
93. Long-term testing of SOFC stacks at forschungszentrum Julich10.1002/fuce.201200151 ↗
94. Post-test characterization of a solid oxide fuel cell after more than 10 years of stack testing10.1016/j.jpowsour.2020.228770 ↗
95. Local evolution of anode microstructure morphology in a solid oxide fuel cell after long-term stack operation10.1016/j.jpowsour.2015.04.092 ↗
96. Post-operational characterization of solid oxide fuel cell stacks10.1016/j.ijhydene.2016.05.065 ↗
97. Exploring electrochemical impedance spectroscopy to identify and quantify degradation in commercial solid oxide electrolysis stacks10.1002/fuce.202300023 ↗
98. Investigation on the reaction mechanism of solid oxide co-electrolysis with different inlet mixtures based on the comparison of CO2 electrolysis and H2O electrolysis
99. Towards strategies to mitigate degradation and regenerate performance of a solid oxide electrolyzer during co-electrolysis operation10.1016/j.jpowsour.2022.232404 ↗
100. Performance and degradation of solid oxide electrolysis cells in stack10.1149/2.0941508jes ↗