Experimental analysis of recoverable performance loss induced by platinum oxide formation at the polymer electrolyte membrane fuel cell cathode
Source abstract
Abstract
Abstract Unrecoverable and recoverable performance degradation is a major issue hindering commercialization of polymer electrolyte membrane fuel cells. The recoverable losses, caused for example by a contaminant adsorption, catalyst flooding, ionomer dehydration, and platinum oxidation, can be reversed, usually following an interruption in the cell operation. In order to elucidate the link between platinum oxidation and recoverable performance loss, three MEAs were characterized in this work. They involved catalysts with different nanoparticle sizes and loadings tested using a combination of the electrochemical impedance spectroscopy, constant-voltage, constant-current and potential controlled techniques, before and after electrocatalyst aging. Experimental results indicate that a decrease in specific activity over time is not affected by nanoparticle size or aging. Nevertheless, linear sweep voltammetry, which is adopted to reduce platinum oxide and as diagnostics for oxide composition, reveals that a change in composition is observed in correlation with catalyst morphology and catalyst aging. The formation of the platinum oxide associated with the peak at 0.61 VRHE in the voltammetry is found to decrease the catalyst's specific activity more than oxides associated with peaks at higher potentials. This indicates that the recoverable performance loss due to the platinum oxide formation depends on the oxide composition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. A polymer electrolyte fuel cell life test: 3 years of continuous operation10.1016/j.jpowsour.2005.09.062 ↗
2. Evaluation of reversible and irreversible degradation rates of polymer electrolyte membrane fuel cells tested in automotive conditions10.1016/j.jpowsour.2016.07.049 ↗
3. Recoverable performance loss due to membrane chemical degradation in PEM fuel cells10.1149/2.063207jes ↗
4. A review of water flooding issues in the proton exchange membrane fuel cell10.1016/j.jpowsour.2007.12.068 ↗
5. A study of polymer electrolyte fuel cell performance at high voltages. Dependence on cathode catalyst layer composition and on voltage conditioning10.1016/S0013-4686(02)00350-X ↗
6. Accelerate the development and introduction of advanced Technologies through model based system engineering 201510.1016/j.ijhydene.2007.05.036 ↗
7. Following ORR intermediates adsorbed on a Pt cathode catalyst during break-in of a PEM fuel cell by in operando X-ray absorption spectroscopy10.1039/C4CP00192C ↗
8. Dynamics of particle growth and electrochemical surface area loss due to platinum dissolution10.1149/2.051403jes ↗
9. Baroody · 2016
10. Surface-oxide growth at platinum electrodes in aqueous H2SO 4 Reexamination of its mechanism through combined cyclic-voltammetry, electrochemical quartz-crystal nanobalance, and Auger electron spectroscopy measurements
11. Initial stages of Pt(111) electrooxidation: dynamic and structural studies by surface X-ray diffraction10.1016/j.electacta.2016.12.028 ↗
12. Elucidating the oxide growth mechanism on platinum at the cathode in PEM fuel cells10.1039/c3cp54740j ↗
13. Analysis of the relation between oxidation state and ORR activity of Pt by linear sweep voltammetry10.1149/1.3484509 ↗
14. In situ and real-time monitoring of oxide growth in a few monolayers at surfaces of platinum nanoparticles in aqueous media10.1021/ja810036h ↗
15. A surface-electrochemical basis for the direct logarithmic growth law for initial stages of extension of anodic oxide films formed at noble metals10.1063/1.459319 ↗
16. Electrochemical oxide film formation at noble metals as a surface-chemical process10.1016/0079-6816(95)00040-6 ↗
17. Surface oxide growth on platinum electrode in aqueous trifluoromethanesulfonic acid10.1063/1.4898707 ↗
18. Re-examination of the Pt particle size effect on the oxygen reduction reaction for ultrathin uniform Pt/C catalyst layers without influence from nafion10.1016/j.electacta.2016.08.001 ↗
19. Strategies to mitigate Pt dissolution in low Pt loading proton exchange membrane fuel cell: I. A gradient Pt particle size design10.1016/j.electacta.2017.07.093 ↗
20. Modelling analysis of heterogeneity of ageing in high temperature polymer electrolyte fuel cells: insight into the evolution of electrochemical impedance spectra10.1016/j.electacta.2016.11.014 ↗
21. Strategies to mitigate Pt dissolution in low Pt loading proton exchange membrane fuel cell: II. A gradient Pt loading design10.1016/j.electacta.2017.06.145 ↗
22. Investigation of platinum oxidation in PEM fuel cells at various relative humidities
23. US Department of Energy (DOE) · 2016 · vol. 2015 · 1
24. Modelling analysis of low platinum polymer fuel cell degradation under voltage cycling: gradient catalyst layers with improved durability10.1016/j.jpowsour.2018.09.092 ↗
25. How theory and simulation can drive fuel cell electrocatalysis10.1016/j.nanoen.2016.06.004 ↗
26. Functional links between Pt single crystal morphology and nanoparticles with different size and shape: the oxygen reduction reaction case10.1039/C4EE01564A ↗
27. Oxygen reduction reaction measurements on platinum electrocatalysts utilizing rotating disk electrode technique10.1149/2.1071509jes ↗
28. Catalyst poisoning property of sulfonimide acid ionomer on Pt (111) surface10.1149/2.051405jes ↗
29. Voltammetric and spectroscopic analyses of the effect of ionomer on oxygen reduction reaction on Pt surface and strategy for developing desirable ionomers10.1149/MA2017-02/34/1483 ↗
30. Subbaraman · 2010 · 8414