Abstract

A simple and broadly applicable preparation procedure to obtain silica-supported transition metal (namely Cr, Co and Mn)-based radical scavengers, containing sulfonic acid functionalities, is reported. These systems are widely characterised in terms of structure, bulk and surface composition and morphology by X-Ray Diffraction (XRD), X-Ray Fluorescence (XRF), X-Ray Photoelectron Spectroscopy (XPS) and Transmission Electron Microscopy (TEM). The scavenger material is loaded in ePTFE reinforced membranes prepared from Aquivion® perfluorosulfonic acid (PFSA) dispersions. All these composite membranes show longer lifetime in Accelerated Stress Tests (AST) and reduced fluoride release in Fenton's tests than the scavenger-free membranes without any loss in electrochemical performance. The Cr-scavenger-based polymer electrolyte shows a three-time larger stability than the pristine membrane.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Advanced battery technologies research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Fuel cells: principles, types, fuels, and applications10.1002/1439-7641(20001215)1:4<162::AID-CPHC162>3.0.CO;2-Z ↗
2. The current status of fuel cell technology for mobile and stationary applications10.1039/b415317k ↗
3. Development of ionomer membranes for fuel cells10.1016/S0376-7388(00)00631-1 ↗
4. Polymer membranes for fuel cells
5. Solid polymer electrolyte membranes for fuel cell applications – a review10.1016/j.memsci.2005.01.035 ↗
6. Performance analysis of polymer electrolyte membranes for direct methanol fuel cells10.1016/j.jpowsour.2013.05.180 ↗
7. Recent development of polymer electrolyte membranes for fuel cells10.1021/cr200035s ↗
8. A. Perfluorinated ionic polymers for PEFCs (including supported PFSA)
9. http://www.solvayplastics.com.
10. Understanding short-side-chain perfluorinated sulfonic acid and its application for high temperature polymer electrolyte membrane fuel cells10.1039/C3RA43735C ↗
11. Performance comparison of long and short-side chain perfluorosulfonic membranes for high temperature polymer electrolyte membrane fuel cell operation10.1016/j.jpowsour.2010.12.084 ↗
12. High temperature operation of a solid polymer electrolyte fuel cell stack based on a new ionomer membrane10.1002/fuce.201000031 ↗
13. Ranking the stability of perfluorinated membranes used in fuel cells to attack by hydroxyl radicals and the effect of Ce(III): a competitive kinetics approach based on spin trapping ESR10.1021/ma1001386 ↗
14. Membrane degradation during combined chemical and mechanical accelerated stress testing of polymer electrolyte fuel cells10.1016/j.jpowsour.2014.01.106 ↗
15. Sulfonated poly(arylene ether sulfone ketone) multiblock copolymers with highly sulfonated blocks. long-term fuel cell operation and post-test analyses10.1021/am200579z ↗
16. Visualizing chemical reactions and crossover processes in a fuel cell inserted in the ESR resonator: detection by spin trapping of oxygen radicals, nafion-derived fragments, and hydrogen and deuterium atoms10.1021/jp901597f ↗
17. Aspects of PEMFC degradation10.1149/1.2214557 ↗
18. Modeling and simulation of the degradation of perfluorinated ion-exchange membranes in PEM fuel cells fuel cells and energy conversion10.1149/1.3077573 ↗
19. Selective formation of hydrogen and hydroxyl radicals by electron beam irradiation and their reactivity with perfluorosulfonated acid ionomer10.1021/ja408032p ↗
20. Mechanism for degradation of nafion in PEM fuel cells from quantum mechanics calculations10.1021/ja2074642 ↗
21. Fuel cell perfluorinated sulfonic acid membrane degradation correlating accelerated stress testing and lifetime10.1021/cr200424d ↗
22. The chemical behavior and degradation mitigation effect of cerium oxide nanoparticles in perfluorosulfonic acid polymer electrolyte membranes10.1016/j.polymdegradstab.2013.05.025 ↗
23. Synthesis of Nafion/CeO2 hybrid for chemically durable proton exchange membrane of fuel cell10.1016/j.memsci.2012.07.014 ↗
24. Degradation mitigation in PEM fuel cells using metal nanoparticle and metal oxide additives
25. CeO2 surface oxygen vacancy concentration governs in situ free radical scavenging efficacy in polymer electrolytes10.1021/am3016069 ↗
26. Mitigation of perfluorosulfonic acid membrane chemical degradation using cerium and manganese ions10.1149/1.2982015 ↗
27. Degradation study of MEA for PEMFCs under low humidity conditions10.1149/1.1739314 ↗
28. Towards fuel cell membranes with improved lifetime: Aquivion® perfluorosulfonic acid membranes containing immobilized radical scavengers10.1016/j.jpowsour.2014.09.045 ↗
29. Self-humidifying polymer electrolyte membranes for fuel cells10.1149/1.1837307 ↗
30. Comparison of ethanol and methanol oxidation in a liquid-feed solid polymer electrolyte fuel cell at high temperature10.1149/1.1390638 ↗
31. Composite polymer electrolyte for direct ethanol fuel cell application10.1149/1.2356251 ↗
32. High surface area Nafion resin/silica nanocomposites; a new class of solid acid catalyst10.1021/ja9541950 ↗
33. Silica-immobilized Aquivion PFSA Superacid: application to heterogeneous direct etherification of glycerol with n-butanol10.1039/C5CY00534E ↗
34. Electron paramagnetic study on radical scavenging properties of ceria nanoparticles10.1016/j.cplett.2007.06.026 ↗
35. Degradation mitigation in polymer electrolyte membranes using cerium oxide as a regenerative free-radical scavenger10.1149/1.2916443 ↗
36. Reversible and irreversible degradation in fuel cells during open circuit voltage durability testing10.1016/j.jpowsour.2008.04.009 ↗
37. Degradation mechanism of PEMFC under open circuit operation10.1149/1.2266163 ↗
38. A performance and degradation study of Nafion 212 membrane for proton exchange membrane fuel cells10.1016/j.jpowsour.2009.04.038 ↗
39. In-situ diagnostics and degradation mapping of a mixed-mode accelerated stress test for proton exchange membranes10.1016/j.jpowsour.2014.10.116 ↗
40. Effect of catalyst properties on membrane degradation rate and the underlying degradation mechanism in PEMFCs10.1149/1.2219708 ↗
41. Performance and degradation of high temperature polymer electrolyte fuel cell catalysts10.1016/j.jpowsour.2007.10.005 ↗