Corrosion inhibition of aromatic acids on Al-7075 anode for Al-air batteries with alkaline electrolyte
Source abstract
Abstract
The severe hydrogen evolution corrosion is the major obstacle for the extensive application of the aluminium-air batteries. In this research, three aromatic acids, i.e. benzoic acid (BEA), iso-phthalic acid (IPA), and trimesic acid (TRA), are performed as corrosion inhibitors for Al-7075 alloy in 2 M KOH water-ethanol (volume ratio 8:2) solution. The results reveal that all of the three aromatic acids are excellent inhibitors for Al-7075 alloy in alkaline medium with the following inhibition efficiency order: BEA > IPA > TRA, and the peak value of inhibition efficiency is 43.7% when 5 mM BEA is added. The addition of aromatic acids significantly improves the discharge characteristics of the Al-air battery, which increases the capacity density (1357.47 mA cm −2 ) and anode utilization (45.6%) remarkably. The results of Fourier transform infrared spectroscopy (FT-IR) and X-ray photoelectron spectroscopy (XPS) demonstrate that the protective film, which is composed of Al salts of organic acid (RCOO-Al), is adsorbed on the Al-7075 alloy surface through chemical bonds between Al substrate and the O atoms on C O groups, which enhances the corrosion and electrochemical characteristics of the Al-7075 anode for Al-air battery with alkaline electrolyte.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advanced battery technologies research · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Electrical energy storage for the grid: a battery of choices10.1126/science.1212741 ↗
2. Toward a new generation of low cost, efficient, and durable metal-air flow batteries10.1039/C9TA10658H ↗
3. A comprehensive review on recent progress in aluminum–air batteries10.1016/j.gee.2017.06.006 ↗
4. Advances and challenges in lithium-air batteries10.1016/j.apenergy.2017.07.054 ↗
5. MOF-based separator in an Li-O-2 battery: an effective strategy to restrain the shuttling of dual redox mediators10.1021/acsenergylett.8b00014 ↗
6. Advanced hybrid electrolyte Li-O-2 battery realized by dual superlyophobic membrane10.1016/j.joule.2019.09.002 ↗
7. A rechargeable zinc-air battery based on zinc peroxide chemistry10.1126/science.abb9554 ↗
8. Developments in electrode materials and electrolytes for aluminium-air batteries10.1016/j.jpowsour.2013.01.141 ↗
9. Corrosion rates and negative difference effects for Al and some Al alloys10.1023/A:1003447018115 ↗
10. Evaluation OF alloy anodes for aluminum-air batteries - corrosion studies10.5006/1.3584979 ↗
11. Performance of Al−1Mg−1Zn−0.1Ga−0.1Sn as anode for Al-air battery10.1016/j.electacta.2014.02.080 ↗
12. Performance of Al–0.5 Mg–0.02 Ga–0.1 Sn–0.5 Mn as anode for Al–air battery in NaCl solutions10.1016/j.jpowsour.2013.12.053 ↗
13. Electrochemical performances of Al–0.5Mg–0.1Sn–0.02In alloy in different solutions for Al–air battery10.1016/j.jpowsour.2015.05.113 ↗
14. Performance of Al-0.6 Mg-0.05 Ga-0.1 Sn- 0.1 in as anode for Al-air battery in KOH electrolytes10.1149/2.0871512jes ↗
15. Influence of alloying additives on the performance of commercial grade aluminium as galvanic anode in alkaline zincate solution for use in primary alkaline batteries10.1023/A:1024141918663 ↗
16. Corrosion and anodic behaviors of pure aluminum in a novel alkaline electrolyte10.1016/S1872-1508(08)60067-4 ↗
17. The effects of surface treatment and stannate as an electrolyte additive on the corrosion and electrochemical performances of pure aluminum in an alkaline methanol–water solution10.1016/j.matchemphys.2010.02.006 ↗
18. Performance of Al-0.5In as anode for Al–air battery in inhibited alkaline solutions10.1149/2.0881508jes ↗
19. Gum Arabic as a potential corrosion inhibitor for aluminium in alkaline medium and its adsorption characteristics10.1108/00035590610692554 ↗
20. Corrosion inhibition of aluminium in acidic and alkaline media by Sansevieria trifasciata extract10.1016/j.corsci.2006.08.009 ↗
21. Potential of aqueous extract of Hibiscus sabdariffa leaves for inhibiting the corrosion of aluminum in alkaline solutions10.1007/s10800-009-9826-1 ↗
22. Gossipium hirsutum L. extracts as green corrosion inhibitor for aluminum in NaOH solution10.1016/j.corsci.2009.04.016 ↗
23. Aluminum as the anode IN primary alkaline batteries10.1016/0376-4583(85)90112-8 ↗
24. Complex behaviour of aluminium dissolution in alkaline aqueous 2-propanol solution10.1016/S0378-7753(96)02388-9 ↗
25. Novel package for inhibition of aluminium corrosion in alkaline solutions10.1016/j.matchemphys.2010.07.059 ↗
26. Influence of 8-hydroxyquinoline addition on the corrosion behavior of commercial Al and Al-HO411 alloys in NaOH aqueous media10.1016/j.corsci.2011.05.045 ↗
27. Organic inhibitors of the anode self-corrosion in aluminum-air batteries10.1115/1.4025534 ↗
28. Excellent performance of aluminium anode based on dithiothreitol additives for alkaline aluminium/air batteries
29. Influences of zinc oxide and an organic additive on the electrochemical behavior of pure aluminum in an alkaline solution10.1007/s10800-004-6204-x ↗
30. Aluminum corrosion mitigation in alkaline electrolytes containing hybrid inorganic/organic inhibitor system for power sources applications10.1016/j.jpowsour.2015.03.048 ↗
31. Evaluation of AA5052 alloy anode in alkaline electrolyte with organic rare-earth complex additives for aluminium-air batteries10.1016/j.jpowsour.2015.05.104 ↗
32. An effective hybrid organic/inorganic inhibitor for alkaline aluminum-air fuel cells10.1016/j.electacta.2017.07.108 ↗
33. Modified alkaline electrolyte with 8-hydroxyquinoline and ZnO complex additives to improve Al-air battery10.1016/j.jpowsour.2019.05.077 ↗
34. Materials, Carboxylic acids as corrosion inhibitors for aluminium in acidic and alkaline solutions
35. Aromatic acid derivatives as corrosion inhibitors for aluminium in acidic and alkaline solutions
36. Experimental and theoretical investigation on corrosion inhibition of AA5052 aluminium alloy by L-cysteine in alkaline solution10.1016/j.matchemphys.2015.11.041 ↗
37. Performance of AA5052 alloy anode in alkaline ethylene glycol electrolyte with dicarboxylic acids additives for aluminium-air batteries10.1016/j.jpowsour.2015.08.033 ↗
38. Inhibition effect and mechanism of inorganic-organic hybrid additives on three-dimension porous aluminum foam in alkaline Al-air battery10.1016/j.jpowsour.2019.227460 ↗
39. Al-6013-T6 and Al-7075-T7351 alloy anodes for aluminium-air battery10.1016/j.ijhydene.2017.02.136 ↗
40. The effect of grain size on aluminum anodes for Al-air batteries in alkaline electrolytes10.1016/j.jpowsour.2015.03.063 ↗
41. Effect of halides ions on H-2 production during aluminum corrosion in formic acid and using some inorganic inhibitors to control hydrogen evolution10.1016/j.jpowsour.2013.05.066 ↗
42. Evaluation OF alloy anodes for aluminum-air batteries .4. Electrochemical impedance analysis OF pure aluminum IN 4M-KOH at 25-DEGREES-C10.1149/1.2095348 ↗
43. Electrochemical behaviour of aluminium in concentrated NaOH solutions10.1016/S0010-938X(98)00107-3 ↗
44. The effect of anions on the electrochemical behaviour of aluminium10.1016/0013-4686(83)85076-2 ↗
45. The behavior of aluminum in alkaline media10.1016/S0010-938X(00)00055-X ↗
46. Anodic dissolution of aluminum in KOH ethanol solutions10.1016/j.elecom.2003.10.007 ↗
47. Inhibition of aluminium corrosion in alkaline solutions using natural compound10.1016/j.matchemphys.2007.11.038 ↗
48. Computational simulation of the molecular structure and properties of heterocyclic organic compounds with possible corrosion inhibition properties10.1016/j.theochem.2004.10.036 ↗
49. Three novel di-quaternary ammonium salts as corrosion inhibitors for API X65 steel pipeline in acidic solution. Part I: experimental results10.1016/j.corsci.2013.12.010 ↗
50. Effect of ethylenediarnine tetraacetic acid disodium on the corrosion of cold rolled steel in the presence of benzotriazole in hydrochloric acid10.1016/j.electacta.2007.04.114 ↗
51. Surface protection of copper in acid medium by azoles and surfactants10.1016/j.electacta.2005.04.003 ↗
52. Zn-Al layered double oxides as high-performance anode materials for zinc-based secondary battery10.1039/C5TA00279F ↗
53. ESCA, xrd, and ir characterization OF aluminum-oxide, HYDROXYFLUORIDE, and fluoride surfaces IN correlation with their catalytic activity IN heterogeneous halogen exchange-reactions10.1006/jcat.1994.1208 ↗
54. Corrosion protection of aluminium alloy 2024-T3 in 0.05M NaCl by cerium cinnamate10.1016/j.corsci.2011.03.012 ↗
55. Cerium tartrate as a corrosion inhibitor for AA 2024-T310.1016/j.corsci.2015.03.010 ↗