Aging mechanisms of NMC811/Si-Graphite Li-ion batteries
Source abstract
Abstract
Electrode degradation processes at various Li-ion batteries’ state-of-health (SoH 100 %, 80 %, 50 %, and 30 %) and cycling temperatures (5 °C, 23 °C, and 45 °C) were investigated. For this purpose, the standard format of Li-ion cylindrical 18,650 batteries with Si-Graphite negative and LiNi 0 · 8 Co 0 · 1 Mn 0 · 1 O 2 (NMC811) positive electrodes were cycled with registering battery parameters and the electrochemical impedance spectrum were recorded after every 200 cycles. Once reaching their end-of-life, electrodes from cycled batteries were subjected to post-mortem analysis. NMC811 positive electrode was observed to crack during the charge and discharge processes, suffered by irreversible phase transition, transition metal dissolution, cathode electrolyte interphase growth, and cation mixing. The Si-Graphite negative electrode material was also affected by crack formation, layer exfoliation, solid electrolyte interphase (SEI) recompositing, Li dendrite growth, transition metal contamination, and Si dissolution. Degradation of components leads to an increase of the contact resistance, Li + diffusion limitations, reduction of active materials participating in Li-ion storage and, as a result, capacity fade that finally rendered the battery utilization unfeasible. Degradation processes can be detected by capacity fade and impedance growth of the full battery. High temperature accelerates electrode degradation processes when low temperature leads to SEI and Li dendrite growth. • Cycling and post-mortem analysis of Li batteries • Comprehensive analysis of electrodes from fresh and cycle aged cells • Temperature and state-of-health degradation dependence of Li batteries • Key aging mechanisms have been discussed
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (81)
Show source-provided references
1. The birth of the lithium-ion battery10.1002/anie.201105006 ↗
2. Nakajima · 1887 · US4668595A
3. Li-ion batteries: Basics, progress, and challenges10.1002/ese3.95 ↗
4. Memory effect in a lithium-ion battery10.1038/nmat3623 ↗
5. Li-ion battery fire hazards and safety strategies10.3390/en11092191 ↗
6. Lithium batteries: status, prospects and future10.1016/j.jpowsour.2009.11.048 ↗
7. Cui · 2015
8. Cycle life testing and modeling of graphite/LiCoO2 cells under different state of charge ranges10.1016/j.jpowsour.2016.07.057 ↗
9. Calendar aging model for lithium-ion batteries considering the influence of cell characterization10.1016/j.est.2021.103506 ↗
10. Impact of temperature on calendar ageing of Lithium-ion battery using incremental capacity analysis
11. Investigation of the temperature and DOD effect on the performance-degradation behavior of lithium–sulfur pouch cells during calendar aging10.1016/j.apenergy.2022.120543 ↗
12. Effect of ambient storage on the degradation of Ni-rich positive electrode materials (NMC811) for Li-ion batteries10.1149/2.0401802jes ↗
13. Temperature dependent ageing mechanisms in Lithium-ion batteries – a Post-Mortem study10.1016/j.jpowsour.2014.03.112 ↗
14. Heat generation and thermal transport in lithium-ion batteries: a scale-bridging perspective10.1080/15567265.2019.1572679 ↗
15. Lithium ion batteries (NMC/graphite) cycling at 80 °C: different electrolytes and related degradation mechanism10.1016/j.jpowsour.2017.11.014 ↗
16. Unravelling and quantifying the aging processes of commercial Li(Ni0.5Co0.2Mn0.3)O2/graphite lithium-ion batteries under constant current cycling10.1039/D2TA05960F ↗
17. Lithium ion battery electrolyte degradation of field-tested electric vehicle battery cells – a comprehensive analytical study10.1016/j.jpowsour.2019.227370 ↗
18. Review—“Knees” in lithium-ion battery aging trajectories10.1149/1945-7111/ac6d13 ↗
19. The formation and stability of the solid electrolyte interface on the graphite anode10.1016/j.jpowsour.2014.06.024 ↗
20. Generation and evolution of the solid electrolyte interphase of lithium-ion batteries10.1016/j.joule.2019.08.018 ↗
21. A failure modes, mechanisms, and effects analysis (FMMEA) of lithium-ion batteries10.1016/j.jpowsour.2015.07.100 ↗
22. Modeling of lithium-ion battery degradation for cell life assessment10.1109/TSG.2016.2578950 ↗
23. Degradation mechanism of monocrystalline Ni-rich Li[Ni x Mn y Co z ]O 2 (NMC) active material in lithium ion batteries10.1149/1945-7111/ac239f ↗
24. Liquid cell transmission electron microscopy observation of lithium metal growth and dissolution: root growth, dead lithium and lithium flotsams10.1016/j.nanoen.2016.12.001 ↗
25. Suppression of lithium dendrite growth using cross-linked polyethylene/poly(ethylene oxide) electrolytes: a new approach for practical lithium-metal polymer batteries10.1021/ja502133j ↗
26. Lithium plating mechanism, detection, and mitigation in lithium-ion batteries10.1016/j.pecs.2021.100953 ↗
27. Extensive comparison of doping and coating strategies for Ni-rich positive electrode materials10.1016/j.jpowsour.2022.231633 ↗
28. Investigating the reversibility of structural modifications of LixNiyMnzCo1-y-zO2 cathode materials during initial charge/discharge, at multiple length scales10.1021/acs.chemmater.5b02457 ↗
29. New insights in Al-doping effects on the LiNiO2 positive electrode material by a sol-gel method10.1002/er.6536 ↗
30. Degradation mechanisms and mitigation strategies of nickel-rich NMC-based lithium-ion batteries10.1007/s41918-019-00053-3 ↗
31. Two electrolyte decomposition pathways at nickel-rich cathode surfaces in lithium-ion batteries10.1039/D1EE04053G ↗
32. Capacity-fading mechanisms of LiNiO[sub 2]-based lithium-ion batteries10.1149/1.3076137 ↗
33. Surface changes on LiNi0.8Co0.2O2 particles during testing of high-power lithium-ion cells10.1016/S1388-2481(02)00388-0 ↗
34. Intercalation/de-intercalation reactions of lithium ion at graphite in electrolyte solutions containing 3D-transition-metal ions and cyclic ethers10.1149/2.0111614jes ↗
35. Review—SEI: past, present and future10.1149/2.1441707jes ↗
36. Face to face at the cathode electrolyte interphase: from interface features to interphase formation and dynamics10.1002/admi.202102078 ↗
37. Cathode-electrolyte interphase in lithium batteries revealed by cryogenic electron microscopy10.1016/j.matt.2020.10.021 ↗
38. Influence of the electrolyte salt concentration on the rate capability of ultra‐thick NCM 622 electrodes10.1002/batt.202000098 ↗
39. Comparison of methodologies to estimate state-of-health of commercial Li-ion cells from electrochemical frequency response data10.1016/j.jpowsour.2022.231814 ↗
40. HISTORICAL commentary NIH Image to ImageJ : 25 years of image analysis10.1038/nmeth.2089 ↗
41. The BALDER beamline at the MAX IV laboratory
42. ATHENA, artemis, hephaestus: data analysis for X-ray absorption spectroscopy using IFEFFIT10.1107/S0909049505012719 ↗
43. Experimental investigation of the lithium-ion battery impedance characteristic at various conditions and aging states and its influence on the application10.1016/j.apenergy.2012.09.030 ↗
44. Cycle aging of commercial NMC/graphite pouch cells at different temperatures10.1016/j.apenergy.2015.04.110 ↗
45. Low-temperature aging mechanisms of commercial graphite/LiFePO 4 cells cycled with a simulated electric vehicle load profile — a post-mortem study10.1016/j.est.2018.10.007 ↗
46. Nickel, manganese, and cobalt dissolution from Ni-rich NMC and their effects on nmc622-graphite cells10.1149/2.1151902jes ↗
47. Kabir · 2017 · 1963
48. Ageing mechanisms in lithium-ion batteries10.1016/j.jpowsour.2005.01.006 ↗
49. Postmortem analysis of calendar-aged graphite/LiFePO 4 cells10.1016/j.jpowsour.2013.01.147 ↗
50. Understanding the role of SEI layer in low-temperature performance of lithium-ion batteries10.1021/acsami.1c23934 ↗
51. Synthesis of Li-rich NMC: a comprehensive study10.1021/acs.chemmater.7b03230 ↗
52. Electrolyte additives for lithium ion battery electrodes: progress and perspectives10.1039/C6EE00123H ↗
53. Tuning the li/ni disorder of the nmc811 cathode by thermally driven competition between lattice ordering and structure decomposition10.1021/acs.jpcc.0c00720 ↗
54. Understanding the degradation mechanisms of LiNi0.5Co 0.2Mn0.3O2 cathode material in lithium ion batteries10.1002/aenm.201300787 ↗
55. A new insight into the capacity decay mechanism of Ni-rich layered oxide cathode for lithium-ion batteries10.1002/smll.202204613 ↗
56. Effect of synthesis conditions and composition modification on the structural and electrochemical properties of layered transition metal oxide cathode materials
57. Structural degradation of layered cathode materials in lithium-ion batteries induced by ball milling10.1149/2.0091910jes ↗
58. Continuous activation of Li2MnO3 component upon cycling in Li1.167Ni0.233Co0.100Mn 0.467Mo0.033O2 cathode material for lithium ion batteries10.1039/c2ta00309k ↗
59. Boosting the cycling stability of Ni-rich layered oxide cathode by dry coating of ultrastable Li3V2(PO4)3 nanoparticles10.1039/D0NR08305D ↗
60. Addressing cation mixing in layered structured cathodes for lithium-ion batteries: a critical review
61. Crossover effects of transition metal ions in high-voltage lithium metal batteries10.1007/s12274-022-5334-y ↗
62. Insights into the crossover effects in cells with high-nickel layered oxide cathodes and silicon/graphite composite anodes
63. Quantitative estimation methods for concentrations and layer thicknesses of elements using edge-jump ratios of X-ray absorption spectra10.2116/analsci.26.281 ↗
64. Diffusion-limited C-rate: a fundamental principle quantifying the intrinsic limits of Li-ion batteries10.1002/aenm.201902523 ↗
65. Impact of bracing on large format prismatic lithium‐ion battery cells during aging
66. In situ inorganic conductive network formation in high-voltage single-crystal Ni-rich cathodes10.1038/s41467-021-25611-6 ↗
67. Electrolyte regulating toward stabilization of cobalt-free ultrahigh-nickel layered oxide cathode in lithium-ion batteries10.1021/acsenergylett.1c00374 ↗
68. Phase behavior during electrochemical cycling of Ni-rich cathode materials for Li-ion batteries10.1002/aenm.202003404 ↗
69. Applications of voltammetry in lithium ion battery research10.33961/jecst.2019.00619 ↗
70. Irreversible capacity loss of Li-ion batteries cycled at low temperature due to an untypical layer hindering Li diffusion into graphite electrode10.1149/2.0491712jes ↗
71. Diverting exploration of silicon anode into practical way: a review focused on silicon-graphite composite for lithium ion batteries10.1016/j.ensm.2020.11.028 ↗
72. Relationships between polypyrrole synthesis conditions, its morphology and electronic structure with supercapacitor properties measured in electrolytes with different ions and pH values10.1016/j.electacta.2021.138892 ↗
73. Preparation of a high-purity ultrafine α-Al2O3 powder and characterization of an Al2O3-coated PE separator for lithium-ion batteries10.1016/j.powtec.2017.07.027 ↗
74. Electrochemical characterization and post-mortem analysis of aged LiMn 2O4-Li(Ni0.5Mn0.3Co 0.2)O2/graphite lithium ion batteries. Part I: cycle aging10.1016/j.jpowsour.2013.11.080 ↗
75. Modeling of degradation effects considering side reactions for a pouch type Li-ion polymer battery with carbon anode10.1016/j.jpowsour.2014.03.045 ↗
76. In situ XRD study of the structural changes of graphite anodes mixed with SiOx during lithium insertion and extraction in lithium ion batteries10.1016/j.electacta.2013.06.059 ↗
77. X-ray diffraction patterns of graphite and turbostratic carbon10.1016/j.carbon.2007.03.038 ↗
78. Understanding the mechanism of capacity increase during early cycling of commercial NMC/graphite lithium-ion batteries10.1016/j.jechem.2022.07.005 ↗
79. Kinetically determined phase transition from stage II (LiC12) to stage i (LiC6) in a graphite anode for Li-ion batteries10.1021/acs.jpclett.8b02750 ↗
80. Analysis of the deterioration mechanism of Si electrode as a Li-ion battery anode using Raman microspectroscopy10.1021/jp5121965 ↗
81. Si-based anode materials for li-ion batteries: a mini review10.1007/s40820-014-0008-2 ↗