journal article·2021-11

Mechanical degradation of catalyst layer under accelerated relative humidity cycling in a polymer electrolyte membrane fuel cell

Jing Liu, Yan Yin, Junfeng Zhang, Tong Zhang, Xiaojie Zhang, Huicui Chen

Publisher page

Abstract

Abstract Microstructure changes in the catalyst layer (CL) of polymer electrolyte membrane fuel cell (PEMFC) cause the performance degradation, especially under dynamic operating conditions. In this study, the effect of relative humidity (RH) cycling on the CL microstructure changes, the associated mechanisms, and fuel cell performance degradation are investigated. It is found that the Pt/C agglomerates size grows significantly due to RH cycling, especially at locations under the rib of bipolar plate. At 1000 mA cm−2, the output voltage of the degraded CL drops about 6.56% in comparison with the fresh one. The electrochemical impedance spectrum and cyclic voltammetry are also measured correspondingly. Furthermore, a mathematical model is proposed to simulate the microstructure changes in the CL based on finite element method. Residual plastic strain may exist in the ionomer due to the swelling and shrinking behavior, resulting in the interfacial delamination between the ionomer and the Pt/C agglomerates. With the accumulation of plastic strain, the ionomer may be damaged during long term operation. The squeezed agglomerates may be combined each other during the swelling/shrinking process which can be seen as the agglomerates size growth mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Water transport in polymer electrolyte membrane fuel cells10.1016/j.pecs.2010.06.002 ↗
2. Development of the fuel cell system in the mirai FCV
3. No free ride to zero-emissions: simulating a region's need to implement its own zero-emissions vehicle (ZEV) mandate to achieve 2050 GHG targets10.1016/j.enpol.2017.08.031 ↗
4. A review of PEM fuel cell durability: degradation mechanisms and mitigation strategies10.1016/j.jpowsour.2008.06.006 ↗
5. A review on polymer electrolyte membrane fuel cell catalyst degradation and starvation issues: causes, consequences and diagnostic for mitigation10.1016/j.jpowsour.2009.03.060 ↗
6. Durability studies on performance degradation of Pt/C catalysts of proton exchange membrane fuel cell10.1016/j.ijhydene.2009.03.045 ↗
7. Advanced platinum-based oxygen reduction electrocatalysts for fuel cells10.1021/acs.accounts.0c00488 ↗
8. Oxygen reduction electrocatalysts toward practical fuel cells: progress and perspectives10.1002/anie.202016977 ↗
9. A review of automotive proton exchange membrane fuel cell degradation under start-stop operating condition10.1016/j.apenergy.2018.04.049 ↗
10. A review of polymer electrolyte membrane fuel cell durability for vehicular applications: degradation modes and experimental techniques10.1016/j.enconman.2019.112022 ↗
11. Degradation mechanisms of proton exchange membrane fuel cell under typical automotive operating conditions10.1016/j.pecs.2020.100859 ↗
12. Dynamic fuel cell gas humidification system10.1016/j.ijhydene.2012.01.143 ↗
13. Modeling and experimental validation of H2 gas bubble humidifier for a 50 kW stationary PEMFC system10.1016/j.ijhydene.2014.04.058 ↗
14. Experimental observations of microstructure changes in the catalyst layers of proton exchange membrane fuel cells under wet-dry Cycles10.1149/2.0391806jes ↗
15. Local resolved investigation of PEMFC performance degradation mechanism during dynamic driving cycle10.1016/j.ijhydene.2016.01.048 ↗
16. Investigation of dynamic driving cycle effect on performance degradation and micro-structure change of PEM fuel cell10.1016/j.ijhydene.2008.10.054 ↗
17. Diagnosis of MEA degradation under accelerated relative humidity cycling10.1016/j.jpowsour.2011.01.088 ↗
18. Microstructure changes in the catalyst layers of PEM fuel cells induced by load cycling. Part I. Mechanical model10.1016/j.jpowsour.2007.10.006 ↗
19. Modelling of mechanical microstructure chenges in the catalyst layer of a polymer electrolyte membrane fuel cell10.1016/j.ijhydene.2018.10.157 ↗
20. Accelerated stress test procedures for PEM fuel cells under actual load constraints: state-of-art and proposals10.1016/j.ijhydene.2015.07.026 ↗
21. A review of accelerated stress tests of MEA durability in PEM fuel cells10.1016/j.ijhydene.2008.10.012 ↗
22. Degradation on a PTFE/Nafion membrane electrode assembly with accelerating degradation technique10.1016/j.ijhydene.2010.03.118 ↗
23. Effect of humidity and thermal cycling on the catalyst layer structural changes in polymer electrolyte membrane fuel cells10.1016/j.enconman.2019.03.066 ↗
24. Mechanical response of fuel cell membranes subjected to a hygro-thermal cycle10.1016/j.jpowsour.2006.05.020 ↗
25. Mechanical behavior of fuel cell membranes under humidity cycles and effect of swelling anisotropy on the fatigue stresses10.1016/j.jpowsour.2007.03.063 ↗
26. Microstructural changes of membrane electrode assemblies during PEFC durability testing at high humidity conditions10.1149/1.1873492 ↗
27. Stresses in proton exchange membranes due to hygro-thermal loading10.1115/1.2173666 ↗
28. Constitutive modeling of the rate, temperature, and hydration dependent deformation response of Nafion to monotonic and cyclic loading10.1016/j.jpowsour.2010.03.047 ↗
29. A tangent modulus method for rate dependent solids10.1016/0045-7949(84)90033-6 ↗
30. Cohesive Zone Models: a critical review of traction-separation relationships across fracture surfaces
31. Finite element formulation of large deformation impact contact problems with friction10.1016/0045-7949(90)90324-U ↗
32. Numerical simulations of fast crack growth in brittle solids10.1016/0022-5096(94)90003-5 ↗
33. Microstructure changes in the catalyst layers of PEM fuel cells induced by load cycling: Part II. Simulation and understanding10.1016/j.jpowsour.2007.10.007 ↗
34. In-situ simulation of membrane fatigue in polymer electrolyte fuel cells10.1016/j.ijhydene.2017.01.173 ↗
35. Ionomer migragation within PEMFC catalyst layers induces by humidity changes10.1016/j.elecom.2019.106590 ↗
36. Degradation mechanisms of Pt/C fuel cell catalysts under simulated start–stop conditions10.1021/cs300024h ↗
37. Sulfonated hydrocarbon membranes for medium-temperature and low-humidity proton exchange membrane fuel cells (PEMFCs)10.1016/j.progpolymsci.2011.06.001 ↗
38. Preparation and characterization of proton exchange poly (ether sulfone)s membranes grafted propane sulfonic acid on pendant phenyl groups10.1016/j.electacta.2013.11.173 ↗
39. An experimental investigation of humidity and temperature effects on the mechanical properties of perfluorosulfonic acid membrane10.1016/j.msea.2006.03.055 ↗
40. Effects of isolated chemical and mechanical degradation stressors on the ionomer morphology in fuel cell membranes10.1016/j.polymdegradstab.2017.10.006 ↗