journal article·2022-10

Physics-based, reduced order degradation model of lithium-ion batteries

Aniruddha Jana, A. Surya Mitra, Supratim Das, William C. Chueh, Martin Z. Bazant, R. Edwin García

Publisher page

Abstract

A physics-based, reduced order framework is developed to calculate the charge capacity loss contributions from spatially homogeneous and heterogeneous degradation mechanisms, chemomechanical cycling and initial capacity recovery. The formulation goes well beyond prevalent coulomb-counting models and is tuned solely based on experimentally measurable parameters, although it neglects any buildup of internal resistance. The model is compared against the largest data set available to date for commercial LiFePO 4-graphite cells and shows less than 10% error for 92% of the cells. Results suggest that in most cells the charge capacity increases through the first ∼ 50 cycles, beyond which homogeneous SEI growth dominates capacity loss up to ∼ 500 cycles. Above ∼ 500 cycles and at high current densities, the model attributes capacity loss primarily to heterogeneous SEI growth proceeding at microstructurally favored locations, further assisted by chemomechanical failure of the graphite anode particles towards the end of cell life. The developed model sets the stage for on-the-fly capacity loss calculations in hybrid and electric vehicles, especially at low currents and constant voltage holds and could be extended to capture the deleterious effects of high current densities in fast-charging scenarios by including resistive losses.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. The development and future of lithium ion batteries10.1149/2.0251701jes ↗
2. Batteries and fuel cells for emerging electric vehicle markets10.1038/s41560-018-0108-1 ↗
3. Renewable energies and operational and environmental efficiencies of the US oil and gas companies: A true fixed effect model10.1016/j.egyr.2021.04.032 ↗
4. Promise and reality of post-lithium-ion batteries with high energy densities
5. A wide range of testing results on an excellent lithium-ion cell chemistry to be used as benchmarks for new battery technologies10.1149/2.0981913jes ↗
6. Battery lifetime prognostics10.1016/j.joule.2019.11.018 ↗
7. Micro-mesoporous carbons from cyclodextrin nanosponges enabling high-capacity silicon anodes and sulfur cathodes for lithiated Si-S batteries10.1002/chem.202104201 ↗
8. Modeling of a commercial graphite/LiFePO4 cell10.1149/1.3567007 ↗
9. Life simulation of a graphite/LiFePO4 cell under cycling and storage10.1149/2.049208jes ↗
10. Analysis and modeling of calendar aging of a commercial LiFePO4/graphite cell10.1016/j.est.2018.01.019 ↗
11. Systematic aging of commercial LiFePO4 | graphite cylindrical cells including a theory explaining rise of capacity during aging10.1016/j.jpowsour.2017.01.133 ↗
12. Multi-scale thermo-electrochemical modeling of performance and aging of a LiFePO4/graphite lithium-ion cell10.1149/2.0761702jes ↗
13. A simplified electrochemical and thermal aging model of LiFePO4-graphite Li-ion batteries: Power and capacity fade simulations10.1149/2.053304jes ↗
14. Effect of lithium bis (trifluoromethylsulfonyl) imide salt-doped UV-cured glycidyl methacrylate10.1007/s10008-015-2910-z ↗
15. Recent progress in sustainable recycling of LiFePO4-type lithium-ion batteries: Strategies for highly selective lithium recovery10.1016/j.cej.2021.133993 ↗
16. Degradation mechanisms of C6/LiFePO4 batteries: Experimental analyses of cycling-induced aging10.1016/j.electacta.2016.05.091 ↗
17. An accelerated calendar and cycle life study of Li-ion cells10.1016/S0378-7753(01)00783-2 ↗
18. Aging mechanism in Li ion cells and calendar life predictions10.1016/S0378-7753(01)00722-4 ↗
19. A simple route toward next-gen green energy storage concept by nanofibres-based self-supporting electrodes and a solid polymeric design10.1016/j.carbon.2016.06.076 ↗
20. Failure statistics for commercial lithium ion batteries: A study of 24 pouch cells10.1016/j.jpowsour.2016.12.083 ↗
21. Prognostics of lithium-ion batteries based on Dempster–Shafer theory and the Bayesian Monte Carlo method10.1016/j.jpowsour.2011.08.040 ↗
22. Rational design of fly ash-based composites for sustainable lithium-ion battery anodes10.1016/j.electacta.2022.140035 ↗
23. Improvement of natural graphite as a lithium-ion battery anode material, from raw flake to carbon-coated sphere10.1039/b316702j ↗
24. Aqueous processing of natural graphite particulates for lithium-ion battery anodes and their electrochemical performance10.1016/j.jpowsour.2005.01.022 ↗
25. A review of the features and analyses of the solid electrolyte interphase in li-ion batteries10.1016/j.electacta.2010.05.072 ↗
26. Lithium ion battery graphite solid electrolyte interphase revealed by microscopy and spectroscopy10.1021/jp3118055 ↗
27. Data-driven prediction of battery cycle life before capacity degradation10.1038/s41560-019-0356-8 ↗
28. Simplified electrochemical and thermal model of LiFePO4-graphite li-ion batteries for fast charge applications10.1149/2.064209jes ↗
29. Cycle-life model for graphite-LiFePO4 cells10.1016/j.jpowsour.2010.11.134 ↗
30. Cycle ageing analysis of a LiFePO4/graphite cell with dynamic model validations: Towards realistic lifetime predictions10.1016/j.jpowsour.2014.10.153 ↗
31. Calendar aging of commercial graphite/LiFePO4 cell–predicting capacity fade under time dependent storage conditions10.1016/j.jpowsour.2013.11.098 ↗
32. Semi-empirical long-term cycle life model coupled with an electrolyte depletion function for large-format graphite/LiFePO4 lithium-ion batteries10.1016/j.jpowsour.2017.08.094 ↗
33. Design and parametrization analysis of a reduced-order electrochemical model of graphite/LiFePO4 cells for SOC/SOH estimation10.1016/j.jpowsour.2012.12.120 ↗
34. Physically-based reduced-order capacity loss model for graphite anodes in Li-ion battery cells10.1016/j.jpowsour.2016.12.099 ↗
35. A physically-based equivalent circuit model for the impedance of a LiFePO4/Graphite 26650 cylindrical cell10.1149/2.1071709jes ↗
36. Heterogeneous behavior modeling of a LiFePO4-graphite cell using an equivalent electrical circuit10.1016/j.est.2017.04.014 ↗
37. A data-driven multi-scale extended Kalman filtering based parameter and state estimation approach of lithium-ion polymer battery in electric vehicles10.1016/j.apenergy.2013.07.061 ↗
38. Battery safety: Data-driven prediction of failure10.1016/j.joule.2019.10.013 ↗
39. Mathematical modeling of the capacity fade of Li-ion cells10.1016/S0378-7753(03)00531-7 ↗
40. Development of first principles capacity fade model for Li-ion cells10.1149/1.1634273 ↗
41. Simulation-based analysis of aging phenomena in a commercial graphite/LiFePO4 cell10.1149/2.103112jes ↗
42. A single particle model for lithium-ion batteries with electrolyte and stress-enhanced diffusion physics10.1149/2.1541704jes ↗
43. A single particle model with chemical/mechanical degradation physics for lithium ion battery state of health (SOH) estimation10.1016/j.apenergy.2018.01.011 ↗
44. A comprehensive single-particle-degradation model for battery state-of-health prediction10.1016/j.jpowsour.2020.227950 ↗
45. Identify capacity fading mechanism in a commercial LiFePO4 cell10.1016/j.jpowsour.2009.05.036 ↗
46. A comprehensive capacity fade model and analysis for Li-ion batteries10.1149/2.040310jes ↗
47. Evolution of the solid–electrolyte interphase on carbonaceous anodes visualized by atomic-resolution cryogenic electron microscopy10.1021/acs.nanolett.9b01515 ↗
48. A high precision coulometry study of the SEI growth in Li/graphite cells10.1149/1.3557892 ↗
49. Electrochemical kinetics of SEI growth on carbon black: Part I. Experiments10.1149/2.0231904jes ↗
50. Electrochemical kinetics of SEI growth on carbon black: Part II. Modeling10.1149/2.0241904jes ↗
51. Theory of SEI formation in rechargeable batteries: Capacity fade, accelerated aging and lifetime prediction10.1149/2.044302jes ↗
52. Solvent diffusion model for aging of lithium-ion battery cells10.1149/1.1644601 ↗
53. The electrochemical behavior of alkali and alkaline earth metals in nonaqueous battery systems – The solid electrolyte interphase model10.1149/1.2128859 ↗
54. Modeling side reactions in composite LiyMn2O4 electrodes10.1149/1.1838376 ↗
55. Review on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries10.1038/s41524-018-0064-0 ↗
56. Mixed mode growth model for the solid electrolyte interface (SEI)10.1149/2.1101902jes ↗
57. A mathematical model for the lithium-ion negative electrode solid electrolyte interphase10.1149/1.1804812 ↗
58. Balluffi · 2005
59. Studying lithium intercalation into graphite particles via in situ Raman spectroscopy and confocal microscopy10.1007/s10008-004-0563-4 ↗
60. In situ, time-resolved Raman spectromicrotopography of an operating lithium-ion battery10.1149/1.1627972 ↗
61. In situ characterization of a graphite electrode in a secondary lithium-ion battery using Raman microscopy10.1366/0003702991945650 ↗
62. Kinetic Monte Carlo simulation of surface heterogeneity in graphite anodes for lithium-ion batteries: Passive layer formation10.1149/1.3548526 ↗
63. Mesoscale elucidation of solid electrolyte interphase layer formation in Li-ion battery anode10.1021/acs.jpcc.7b09465 ↗
64. Multi-scale simulation of heterogeneous surface film growth mechanisms in lithium-ion batteries10.1149/2.0241711jes ↗
65. Microstructure-resolved degradation simulation of lithium-ion batteries in space applications10.1016/j.powera.2022.100083 ↗
66. A four parameter model for the solid-electrolyte interphase to predict battery aging during operation10.1016/j.jpowsour.2022.231560 ↗
67. Threefold increase in the Young’s modulus of graphite negative electrode during lithium intercalation10.1149/1.3327913 ↗
68. Examination of graphite particle cracking as a failure mode in lithium-ion batteries: A model-experimental study10.1149/2.0281504jes ↗
69. Mechanical degradation of graphite/PVDF composite electrodes: A model-experimental study10.1149/2.0271603jes ↗
70. “Electrochemical shock” of intercalation electrodes: A fracture mechanics analysis10.1149/1.3464773 ↗
71. Modeling diffusion-induced stress in nanowire electrode structures10.1016/j.jpowsour.2010.02.021 ↗
72. A critical analysis of crack propagation laws10.1115/1.3656900 ↗
73. Life prediction model for grid-connected Li-ion battery energy storage system
74. Understanding anomalous behavior in coulombic efficiency measurements on li-ion batteries10.1149/2.0191503jes ↗
75. A study of the relationship between coulombic efficiency and capacity degradation of commercial lithium-ion batteries10.1016/j.energy.2017.12.144 ↗
76. Lithium-ion battery performance improvement based on capacity recovery exploitation10.1016/j.electacta.2013.10.101 ↗
77. Investigation of significant capacity recovery effects due to long rest periods during high current cyclic aging tests in automotive lithium ion cells and their influence on lifetime10.1016/j.est.2019.02.015 ↗
78. Lithium dendrite growth mechanisms in liquid electrolytes10.1016/j.nanoen.2017.08.056 ↗
79. Dendrite-separator interactions in lithium-based batteries10.1016/j.jpowsour.2014.11.056 ↗
80. Transition of lithium growth mechanisms in liquid electrolytes10.1039/C6EE01674J ↗
81. Electrochemomechanics of lithium dendrite growth10.1039/C9EE01864F ↗
82. Capacity fade mechanisms and side reactions in lithium-ion batteries10.1149/1.1838857 ↗
83. In-situ measurement of current distribution in a Li-ion cell10.1149/2.046304jes ↗
84. Effects of inhomogeneities–nanoscale to mesoscale–on the durability of Li-ion batteries10.1021/jp311431z ↗
85. Chemistry, impedance, and morphology evolution in solid electrolyte interphase films during formation in lithium ion batteries10.1021/jp4111019 ↗
86. Tracking inhomogeneity in high-capacity lithium iron phosphate batteries10.1016/j.jpowsour.2014.11.035 ↗
87. Heterogeneous damage in Li-ion batteries: Experimental analysis and theoretical modeling10.1016/j.jmps.2019.05.003 ↗
88. Quantification of heterogeneous degradation in Li-ion batteries10.1002/aenm.201900674 ↗
89. Influences of graphite electrode on degradation induced by accelerated charging-discharging cycling in lithium-ion battery10.1080/15421406.2018.1468135 ↗
90. Microstructural design considerations for Li-ion battery systems10.1016/j.cossms.2012.03.002 ↗
91. Fracture of electrodes in lithium-ion batteries caused by fast charging10.1063/1.3492617 ↗
92. In situ observation of strains during lithiation of a graphite electrode10.1149/1.3377130 ↗
93. Particle size polydispersity in Li-ion batteries10.1149/2.097403jes ↗
94. An analytical method to determine tortuosity in rechargeable battery electrodes10.1149/2.jes113224 ↗
95. Validity of the Bruggeman relation for porous electrodes10.1088/0965-0393/21/7/074009 ↗
96. Tortuosity anisotropy in lithium-ion battery electrodes10.1002/aenm.201301278 ↗
97. Physical, on the fly, capacity degradation prediction of LiNiMnCoO2-graphite cells10.1016/j.jpowsour.2019.02.073 ↗
98. Solid–electrolyte interphase during battery cycling: theory of growth regimes10.1002/cssc.202000867 ↗
99. Direct calculation of Li-ion transport in the solid electrolyte interphase10.1021/ja305366r ↗
100. Transport properties of LiPF6-based Li-ion battery electrolytes10.1149/1.1872737 ↗