Promoted electrochemical performance of intermediate temperature solid oxide fuel cells with Pd0.95Mn0.05O-infiltrated (La0.8Sr0.2)0.95MnO3−δ–Y0.16Zr0.84O2 composite cathodes
Source abstract
Abstract
Abstract Pd 0.95 Mn 0.05 O-infiltrated (La 0.8 Sr 0.2 ) 0.95 MnO 3−δ –8 mol.% Y 2 O 3 stabilized ZrO 2 (LSM-YSZ) cathode is used to large size (11 × 11 × 0.1 cm) Ni-YSZ anode-supported planar cells for the first time and electrochemically evaluated in the intermediate temperature range from 650 to 800 °C with H 2 as the fuel and air as the oxidant. The initial open circuit voltage (OCV) of the cell is 1.15 V, and the achieved maximum power density increases from 328 to 734 mW cm −2 with the increase of testing temperatures from 600 to 800 °C, which is almost 2.6 times higher than that of the cell with conventional LSM-YSZ cathode. After each thermal cycle between 750 and 300 °C, the OCV remains almost unchanged and the cell voltage decreases less than 0.007 V, indicating that the cell is capable of thermal cycling. The cell voltage at 310 mA cm −2 and 750 °C declines linearly with testing time at a rate of 2.6 × 10 −4 V h −1 for the growth of the infiltrated Pd 0.95 Mn 0.05 O size, resulting in reduction of the total surface area of the particles. The mechanism of performance degradation of the cell with Pd 0.95 Mn 0.05 O-infiltrated LSM-YSZ composites cathode is discussed in detail.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Jacobson · Chem. Mater. · 2010 · 22 · 66010.1021/cm902640j ↗
2. Zhan · Science · 2005 · 308 · 84410.1126/science.1109213 ↗
3. Jiang · J. Mater. Sci. · 2008 · 43 · 679910.1007/s10853-008-2966-6 ↗
4. Sakaki · Solid State Ionics · 1999 · 118 · 18710.1016/S0167-2738(98)00440-8 ↗
5. Jiang · Solid State Ionics · 1998 · 110 · 11110.1016/S0167-2738(98)00111-8 ↗
6. Liang · Electrochem. Commun. · 2009 · 11 · 104810.1016/j.elecom.2009.03.009 ↗
7. Duan · Sci. Rep. · 2015 · 5 · 817410.1038/srep08174 ↗
8. Ai · Int. J. Hydrogen Energy · 2013 · 38 · 1656910.1016/j.ijhydene.2013.04.058 ↗
9. Liang · Electrochem. Solid-State Lett. · 2008 · 11 · B21310.1149/1.2987693 ↗
10. Sahibzada · Solid State Ionics · 1998 · 113–115 · 28510.1016/S0167-2738(98)00294-X ↗
11. Babaei · J. Alloys Compd. · 2011 · 509 · 478110.1016/j.jallcom.2011.01.157 ↗
12. Liang · Electrochem. Commun. · 2008 · 10 · 4210.1016/j.elecom.2007.10.016 ↗
13. Liang · Int. J. Hydrogen Energy · 2011 · 36 · 767010.1016/j.ijhydene.2011.03.132 ↗
14. Jiang · J. Electrochem. Soc. · 2005 · 152 · A139810.1149/1.1928167 ↗
15. Murray · Solid State Ionics · 2001 · 143 · 26510.1016/S0167-2738(01)00871-2 ↗
16. Liu · J. Energy Chem. · 2013 · 22 · 55510.1016/S2095-4956(13)60072-8 ↗
17. Liang · J. Power Sources · 2011 · 196 · 15310.1016/j.jpowsour.2010.07.011 ↗
18. Wang · Int. J. Hydrogen Energy · 2014 · 39 · 1442110.1016/j.ijhydene.2014.02.051 ↗
19. Liang · Fuel Cells · 2009 · 9 · 63610.1002/fuce.200800078 ↗
20. Zhang · Phys. B Condens. Matter · 2004 · 344 · 27810.1016/j.physb.2003.08.131 ↗
21. Lee · J. Electrochem. Soc. · 2006 · 153 · A2010.1149/1.2128101 ↗
22. Luo · J. Power Sources · 2013 · 224 · 3710.1016/j.jpowsour.2012.09.087 ↗
23. Larminie · 2003
24. Lee · Solid State Ionics · 2008 · 179 · 145410.1016/j.ssi.2008.01.093 ↗
25. Lang · ECS Trans. · 2007 · 7 · 8510.1149/1.2729077 ↗
26. Suzuki · Solid State Ionics · 2006 · 177 · 207110.1016/j.ssi.2005.12.016 ↗
27. Tsai · Solid State Ionics · 1997 · 93 · 20710.1016/S0167-2738(96)00524-3 ↗
28. Lang · Electrochim. Acta · 2008 · 53 · 750910.1016/j.electacta.2008.04.047 ↗
29. Wang · Int. J. Hydrogen Energy · 2013 · 38 · 64610.1016/j.ijhydene.2012.06.052 ↗
30. Jiang · J. Mater. Sci. · 2004 · 39 · 440510.1023/B:JMSC.0000034135.52164.6b ↗
31. Yong · 2006 · 450