Grain boundary complexion modification for interface stability in garnet based solid-state Li batteries
Source abstract
Abstract
The garnet type solid-state electrolyte (SSE) encounters challenges related to poor interfacial contact with Li metal and dendrite penetration problem. This study addresses these issues by manipulating the surface property of garnet-based LLZTO (Li6.5La3Zr1.6Ta0.4O12) SSE. The manipulation is achieved by varying thickness of Al2O3 atomic layer deposition (ALD), followed by sintering. Research results show that the relative density, ionic conductivity, and hardness of LLZTO are improved while electronic conductivity is reduced due to the formation of multiple complexions at grain boundary (GB). The SSE pellets also demonstrate improved wettability with Li metal, leading to stable galvanostatic Li plating/stripping cycling with low polarization, which allows for batter battery performance than pristine one. The concept of modifying SSE through the grain boundary complexion modification by thin ALD coating for enhancing the dendrite tolerance with better electrochemical properties of SSE may open a new direction for solid state battery research.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. All-ceramic Li batteries based on garnet structured Li7La3Zr2O1210.1080/10667857.2020.1746539 ↗
2. Instability of Ga-substituted Li7La3Zr2O12 toward metallic Li10.1039/D1TA10215J ↗
3. Li2CO3: a critical issue for developing solid garnet batteries10.1021/acsenergylett.9b02401 ↗
4. Surface chemistry mechanism of ultra-low interfacial resistance in the solid-state electrolyte Li7La3Zr2O1210.1021/acs.chemmater.7b03002 ↗
5. Local electronic structure variation resulting in Li 'filament' formation within solid electrolytes10.1038/s41563-021-01019-x ↗
6. Revealing atomic-scale ionic stability and transport around grain boundaries of garnet Li7La3Zr2O12 solid electrolyte10.1002/aenm.202102151 ↗
7. Local electronic structure variation resulting in Li ‘filament’ formation within solid electrolytes10.1038/s41563-021-01019-x ↗
8. Inhibiting formation and reduction of Li2CO3 to LiCx at grain boundaries in garnet electrolytes to prevent Li penetration10.1002/adma.202208951 ↗
9. Building a better Li-garnet solid electrolyte/metallic Li interface with antimony10.1002/aenm.202102086 ↗
10. Conformal, nanoscale ZnO surface modification of garnet-based solid-state electrolyte for lithium metal anodes10.1021/acs.nanolett.6b04695 ↗
11. Revealing the short-circuiting mechanism of garnet-based solid-state electrolyte
12. Li7La3Zr2O12 interface modification for Li dendrite prevention10.1021/acsami.6b00831 ↗
13. Grain boundary complexion transitions10.1146/annurev-matsci-081619-114055 ↗
14. Review of grain boundary complexion engineering: know your boundaries
15. Complexion time-temperature-transformation (TTT) diagrams: opportunities and challenges10.1016/j.cossms.2016.05.004 ↗
16. Nano‐scale complexions facilitate Li dendrite‐free operation in LATP solid‐state electrolyte
17. Crystal chemistry and stability of Li7La3Zr2O12 garnet: a fast lithium-ion conductor10.1021/ic101914e ↗
18. Structure and dynamics of the fast lithium ion conductor “Li7La3Zr2O1210.1039/c1cp22108f ↗
19. Effect of Al2O3 on the sintering of garnet-type Li6.5La3Zr1.5Ta0.5O1210.1016/j.ssi.2016.06.013 ↗
20. Low-temperature densification of Al-doped Li7La3Zr2O12: a reliable and controllable synthesis of fast-ion conducting garnets10.1039/C6TA06961D ↗
21. Al-doped Li7La3Zr2O12 synthesized by a polymerized complex method10.1016/j.jpowsour.2011.05.065 ↗
22. Unveiling the roles of alumina as a sintering aid in Li-Garnet solid electrolyte10.1002/er.5562 ↗
23. Organic nanowire-templated fabrication of alumina nanotubes by atomic layer deposition10.1021/nl070404q ↗
24. Conformality in atomic layer deposition: current status overview of analysis and modelling10.1063/1.5060967 ↗
25. Electrochemical and structural investigation on ultra-thin ALD ZnO and TiO2 coated lithium-rich layered oxide cathodes10.1021/acssuschemeng.8b04285 ↗
26. Ultrathin artificial solid electrolyte layer coated biomass derived hard carbon as anode for sodium-ion batteries10.1021/acsaem.1c03425 ↗
27. Nanolaminated ZnO–TiO2 coated lithium-rich layered oxide cathodes by atomic layer deposition for enhanced electrochemical performances10.1016/j.jallcom.2020.155845 ↗
28. Low temperature sintering of fully inorganic all-solid-state batteries – impact of interfaces on full cell performance10.1016/j.jpowsour.2020.228905 ↗
29. High conductivity of mixed phase Al-substituted Li7La3Zr2O1210.1007/s10832-015-9988-7 ↗
30. From ultrasoft pseudopotentials to the projector augmentedwave method10.1103/PhysRevB.59.1758 ↗
31. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
32. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
33. Ab initio phase stability and electronic conductivity of the doped-Li4Ti5O12 anode for Li-ion batteries10.1016/j.actamat.2019.06.014 ↗
34. Thermal recovery of the electrochemically degraded LiCoO2/Li7La3Zr2O12:Al,Ta interface in an all-solid-state lithium battery10.1021/acsami.2c20004 ↗
35. Synthesis and Raman micro-spectroscopy investigation of Li7La3Zr2O1210.1016/j.ssi.2012.10.021 ↗
36. Tetragonal vs. cubic phase stability in Al – free Ta doped Li7La3Zr2O12 (LLZO)10.1039/C4TA02099E ↗
37. A garnet structure-based all-solid-state Li battery without interface modification: resolving incompatibility issues on positive electrodes10.1039/C8SE00436F ↗
38. Dual substitution strategy to enhance Li+ ionic conductivity in Li7La3Zr2O12 solid electrolyte10.1021/acs.chemmater.6b05369 ↗
39. Li ion diffusion in LiAlO2 investigated by Raman spectroscopy10.1016/j.solidstatesciences.2014.08.017 ↗
40. Pankratz · 1982
41. Interfacial kinetic engineering: how far have we come since kingery's inaugural sosman address?10.1111/j.1551-2916.2009.03545.x ↗
42. Demystifying the role of sintering additives with “complexion”10.1016/j.jeurceramsoc.2007.12.018 ↗
43. Thermodynamic optimization of lithia–alumina10.1111/j.1551-2916.2008.02753.x ↗
44. Grain boundary complexions10.1016/j.actamat.2013.07.037 ↗
45. The origin of high electrolyte-electrode interfacial resistances in lithium cells containing garnet type solid electrolytes10.1039/C4CP02921F ↗
46. Densification and ionic-conduction improvement of lithium garnet solid electrolytes by flowing oxygen sintering10.1016/j.jpowsour.2013.09.140 ↗
47. An efficient multi-doping strategy to enhance Li ion conductivity in the garnet-type solid electrolyte Li7La3Zr2O1210.1039/C9TA00417C ↗
48. Shin · Sci. Rep. · 2015 · 5
49. Reducing Interfacial resistance between garnet-structured solid-state electrolyte and Li-metal anode by a germanium layer10.1002/adma.201606042 ↗
50. Interfacial study on solid electrolyte interphase at Li metal anode: implication for Li dendrite growth10.1149/2.0151605jes ↗
51. Physicochemical concepts of the lithium metal anode in solid-state batteries10.1021/acs.chemrev.0c00431 ↗
52. The natural critical current density limit for Li7La3Zr2O12 garnets10.1039/C9TA14177D ↗
53. Critical current density measurements of argyrodite Li6PS5Cl solid electrolyte at ambient pressure10.1149/1945-7111/ad01e3 ↗
54. Hybrid electrolyte with dual-anion-aggregated solvation sheath for stabilizing high-voltage lithium-metal batteries10.1002/adma.202007945 ↗