journal article·2024-09

How to perform corrosion experiments for proton exchange membrane water electrolysis bipolar plates

L.H. Prado, S. Virtanen, N. Weineck, A. Ghicov, F. Kessler

Publisher page

Abstract

Ex-situ corrosion experiments are very common to identify the suitability of metallic materials for various applications. While for proton exchange membrane (PEM) fuel cells the US Department of Energy (DoE) gives a clear guidance on how to perform corrosion experiments, no such guidance exists for PEM water electrolyzer (PEMWE) applications. For the latter, much higher anodic potentials (when compared to fuel cells) of up to +2 V vs. RHE must be considered for bipolar plates. Consequently, in aqueous electrolytes oxygen evolution via water splitting takes place in parallel and the two processes corrosion vs. oxygen evolution cannot easily be separated. We herein demonstrate how corrosion experiments for PEMWE applications can be performed and ascribe the contribution of oxygen evolution during such experiments. Together with the shown comprehensive surface analysis of the metallic sample and analysis of the electrolyte via ICP-MS a clear picture of the stability of 316L stainless steel under electrolysis conditions is given. The described method allows both, the evaluation of metals and alloys as well as coatings on different metals for electrolyzer applications.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Hybrid Renewable Energy Systems · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. A comprehensive review on PEM water electrolysis10.1016/j.ijhydene.2013.01.151 ↗
2. Corrosion of structural components of proton exchange membrane water electrolyzer anodes: a review10.1016/j.jpowsour.2022.232469 ↗
3. Review on bipolar plates for low-temperautre polymer electrolyte membrane water electrolyzers10.1002/er.7182 ↗
4. Materials for Proton Exchange Membrane water electrolyzer bipolar plates10.1016/j.ijhydene.2016.11.106 ↗
5. DOE, Technical Targets for Polymer Electrolyte Membrane Fuel Cell Components |, Department of Energy.
6. Stainless steel as biplar plate material for polymer electrolyte membrane fuel cells10.1016/S0378-7753(03)00023-5 ↗
7. Local measurement of current collector potential in a polymer electrolyte membrane water electrolyser10.1016/j.jpowsour.2019.227563 ↗
8. Carbon-coated stainless steel as a bipolar plate material in PEM water electrolyzers
9. Coated stainless steels evaluation for bipolar plates in PEM water electrolysis conditions10.1016/j.ijhydene.2021.03.100 ↗
10. Corrosion resistance of AISI 442 and AISI 446 ferritic stainless steels as a support for PEMWE bipolar plates10.3390/ma16041501 ↗
11. Characterization and corrosion behaviour of grade 2 titanium used in electrolyzers for hydrogen production10.1016/j.ijhydene.2019.04.093 ↗
12. Ta-ITO coated titanium bipolar plates for proton exchange membrane water electrolyzers10.1149/1945-7111/ac56a3 ↗
13. Bipolar plate development with additive manufacturing and protective coating for durable and high-efficiency hydrogen production10.1016/j.jpowsour.2018.06.078 ↗
14. A review of proton exchange membrane water electrolysis on degradation mechanisms and mitigation strategies10.1016/j.jpowsour.2017.09.006 ↗
15. Stability of bipolar plate materials for proton-exchange membrane water electrolyzers: dissolution of titanium and stainless steel in DI water and highly diluted acid10.1002/celc.202300373 ↗
16. Long-term operation of Nb-coated stainless steel bipolar plates for proton exchange membrane water electrolyzers10.1002/aesr.202200024 ↗
17. Impact of impurities on water electrolysis: a review10.1039/D2SE01517J ↗
18. Toward developing accelerated stress tests for proton exchange membrane electrolyzers10.1016/j.coelec.2020.02.024 ↗
19. Low-cost and durable bipolar plates for proton exchange membrane electrolyzers10.1038/srep44035 ↗
20. Standardization · 2021
21. Effect of halide anions and temperature on initiation of pitting in Cr–Mn–N and Cr–Ni steels10.1179/174327806X94027 ↗
22. Pitting corrosion of martensitic stainless steel in halide bearing solutions10.1016/j.corsci.2016.07.008 ↗
23. Metastable and stable pitting corrosion of titanium in halide solutions10.5006/1.3287839 ↗
24. The effect of halide ions on the anodic passivation of titanium10.2320/matertrans1960.5.198 ↗
25. Protective coatings on stainless steel bipolar plates for proton exchange membrane (PEM) electrolysers10.1016/j.jpowsour.2015.12.071 ↗
26. Coated stainless steel bipolar plates for proton exchange membrane electrolyzers10.1149/2.0141611jes ↗
27. Validation and characterization of suitable materials for bipolar plates in PEM-WE
28. Conductive polymer and nanoparticle-promoted polymer hybrid coatings for metallic bipolar plates in proton membrane exchange water electrolysis10.3390/app13031244 ↗
29. Evolution of nanoporosity in dealloying10.1038/35068529 ↗
30. Effects of Metallurgical Variables on dealloying corrosion
31. Hydriding of titanium: recent trends and perspectives in advanced characterization and multiscale modeling10.1016/j.cossms.2022.101020 ↗
32. Hydride formation on titanium surfaces by cathodic polarization10.1016/j.apsusc.2008.08.090 ↗
33. Hydrogen absorption into titanium under cathodic polarization: an in-situ neutron reflectometry and EIS study10.1149/2.020309jes ↗
34. Effect of pretreatments on the hydrogen evolution kinetics of pure titanium using impedance and SECM technologies10.1016/j.corsci.2021.109726 ↗
35. Electrochemical investigation and identification of titanium hydrides formed in mixed chloride sulfuric acid solution10.1149/2.0121911jes ↗
36. Structural evolution of titanium dioxide during reduction in high-pressure hydrogen10.1038/s41563-018-0135-0 ↗
37. In situ studies of hydrogen evolution kinetics on pure titanium surface: the effects of pre-reduction and dissolved oxygen10.1021/acs.jpcc.1c09818 ↗
38. Hydride formation during cathodic polarization of Ti—I. Effect of temperature and pH of solution on hydride growth10.1016/S0010-938X(72)80014-3 ↗
39. Hydride formation during cathodic polarization of Ti—II. Effect of temperature and pH of solution on hydride growth10.1016/S0010-938X(74)80063-6 ↗
40. Electrocatalytic oxygen evolution reaction (OER) on Ru, Ir, and Pt catalysts: a comparative study of nanoparticles and bulk materials10.1021/cs3003098 ↗
41. Electrocatalysis for the oxygen evolution reaction: recent development and future perspectives10.1039/C6CS00328A ↗
42. Pourbaix diagrams for the ternary system of iron-chromium-nickel10.5006/1.3283945 ↗
43. From Bacon to barriers: a review on the passivity of metals and alloys10.1007/s100080100219 ↗
44. Nature of the passive film on Fe–Cr alloys as studied by 18 O secondary ion mass spectrometry: reduction of the prior film and stability to ex situ surface analysis10.1039/FT9918701011 ↗
45. Pourbaix · 1974
46. In-situ analysis of passive films on high purity Fe-Cr alloys using ellipsometry and potential-modulated reflection spectroscopy10.2355/isijinternational.31.154 ↗
47. Evaluation of nitrided titanium separator plates for proton exchange membrane electrolyzer cells10.1016/j.jpowsour.2014.09.016 ↗
48. Effect of TIG welding on corrosion behavior of 316L stainless steel10.1016/j.matlet.2006.09.008 ↗
49. A single-step fabrication approach for development of antimicrobial surfaces10.1016/j.jmatprotec.2019.04.012 ↗
50. Crystallographic effects in corrosion of austenitic stainless steel 316L10.1002/maco.201408002 ↗
51. Passive films on stainless steels—chemistry, structure and growth10.1016/S0013-4686(02)00841-1 ↗
52. The secondary passive film for type 304 stainless steel in 0.5 M H2SO410.1149/1.1838078 ↗
53. The transpassive dissolution mechanism of highly alloyed stainless steels: I. Experimental results and modelling procedure10.1016/S0010-938X(02)00073-2 ↗
54. Transpassive dissolution of Cr and sputter-deposited Cr oxides studied by in situ X-ray near-edge spectroscopy10.1149/1.1837327 ↗