journal article·2025-11Open access

A review of electrode poisoning in fuel Cells: Strategies for mitigation and performance enhancement

Timileyin Aworinde, Wenkai Yang, Lakshya Mathur, Vallimanalan Ashokan, Sivaprakash Sengodan

Abstract

Fuel cells present a hopeful future to produce clean energy in a range of applications, but their effectiveness is frequently affected by electrode poisoning. This article investigates some common types of electrodes poisoning that can occur in fuel cell systems, such as carbon, sulfur, hydrogen (in ammonia fuel cells), and chromium poisoning. We investigate the causes, effects and methods of reducing the harm for the forms of poisoning highlighted above, emphasizing the difficulties they present, and the approaches used to address them. This review seeks to gain insights into the phenomena of electrode poisoning and offer new directions for future research and development by collating newly emerging and already knowledge. By tackling the difficulties caused by electrode poisoning, we may enhance the dependability, effectiveness, and profitability of fuel cell technology, thereby contributing to a sustainable energy future. • Reviews electrode poisoning types in PEMFCs and SOFCs in detail. • Highlights catalyst degradation due to carbon, sulfur, and chromium. • Explores hydrogen poisoning in ammonia-fed fuel cells and mitigation. • Discusses strategies to improve fuel cell durability and performance.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fuel Cells and Related Materials · Advancements in Solid Oxide Fuel Cells · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Challenges in using perovskite-based anode materials for solid oxide fuel cells with various fuels: a review10.1016/j.ijhydene.2022.12.192 ↗
2. Ren · 2017 · 35
3. Reviews on the effects of contaminations and research methodologies for PEMFC10.1016/j.ijhydene.2020.06.145 ↗
4. Analysis of sulfur poisoning on a PEM fuel cell electrode10.1016/j.electacta.2010.05.004 ↗
5. Direct ammonia solid-oxide fuel cells: a review of progress and prospects10.1016/j.ijhydene.2021.08.092 ↗
6. Comprehensive review of chromium deposition and poisoning of solid oxide fuel cells (SOFCs) cathode materials10.1016/j.rser.2020.110320 ↗
7. A review of PEM hydrogen fuel cell contamination: impacts, mechanisms, and mitigation10.1016/j.jpowsour.2006.12.012 ↗
8. PEMFC contaminant tolerance limit—CO in H210.1016/j.electacta.2010.02.061 ↗
9. Adsorption behavior of low concentration carbon monoxide on polymer electrolyte fuel cell anodes for automotive applications10.1016/j.jpowsour.2016.03.104 ↗
10. Behavior of a proton exchange membrane fuel cell in reformate gas10.1016/j.egypro.2012.09.009 ↗
11. Dynamic behavior of a PEM fuel cell during electrochemical CO oxidation on a PtRu anode10.1007/s11244-008-9117-9 ↗
12. Effects of concentrated CO2 on the performance of a PBI/H3PO4 high temperature proton exchange membrane fuel cell10.1016/j.jpowsour.2024.235053 ↗
13. Improved CO tolerance of Pt nanoparticles on polyaniline-modified carbon for PEMFC anode10.1016/j.fuel.2024.133239 ↗
14. Surface anion promotes Pt electrocatalysts with high CO tolerance in fuel-cell performance10.1021/jacs.2c09147 ↗
15. Nature of CO adsorption during H2 oxidation in relation to modeling for CO poisoning of a fuel cell anode10.1149/1.2100333 ↗
16. Experimental evaluation of CO poisoning on the performance of a high temperature proton exchange membrane fuel cell10.1016/j.jpowsour.2009.04.021 ↗
17. Quantitative analysis of the performance impact of low-level carbon monoxide exposure in proton exchange membrane fuel cells10.1016/j.jpowsour.2012.11.062 ↗
18. Electroseparation of actinides from lanthanides on solid aluminum electrode in LiCl-KCl eutectic melts10.1149/1.1859812 ↗
19. Numerical simulations of carbon monoxide poisoning in high temperature proton exchange membrane fuel cells with various flow channel designs10.1016/j.apenergy.2012.10.059 ↗
20. Effects of reformate on performance of PBI/H3PO4 proton exchange membrane fuel cell stack10.1016/j.ijhydene.2020.03.219 ↗
21. Change of electrochemical impedance spectra during CO poisoning of the Pt and Pt–Ru anodes in a membrane fuel cell (PEFC)10.1016/S0013-4686(03)00528-0 ↗
22. High temperature PEM fuel cell performance characterisation with CO and CO2 using electrochemical impedance spectroscopy10.1016/j.ijhydene.2011.04.076 ↗
23. Analyzing characteristic and modeling of high-temperature proton exchange membrane fuel cells with CO poisoning effect10.1016/j.energy.2023.128305 ↗
24. Three-dimensional non-isothermal modeling of carbon monoxide poisoning in high temperature proton exchange membrane fuel cells with phosphoric acid doped polybenzimidazole membranes10.1016/j.fuel.2010.10.018 ↗
25. A CO poisoning model for high-temperature proton exchange membrane fuel cells comprising phosphoric acid-doped polybenzimidazole membranes10.1016/j.ijhydene.2014.06.101 ↗
26. Spatial analysis of CO poisoning in high temperature polymer electrolyte membrane fuel cells10.1016/j.ijhydene.2020.12.001 ↗
27. Recent advances in carbon-resistant anodes for solid oxide fuel cells10.1039/D2QM01366E ↗
28. La0.6Sr0.4Co0.2Fe0.8O3 perovskite: a stable anode catalyst for direct methane solid oxide fuel cells10.3390/catal4020146 ↗
29. Highly carbon– and sulfur–tolerant Sr2TiMoO6−δ double perovskite anode for solid oxide fuel cells10.1016/j.ijhydene.2019.06.023 ↗
30. Poisoning of SOFC anodes by various fuel impurities10.1016/j.ssi.2008.02.062 ↗
31. Degradation mechanisms of metal-supported solid oxide cells and countermeasures: a review10.3390/ma14113139 ↗
32. Enhanced performance of solid oxide fuel cells with Ni/CeO2 modified La0.75Sr0.25Cr0.5Mn0.5O3−δ anodes10.1016/j.jpowsour.2009.01.035 ↗
33. Carbon monoxide poisoning and mitigation strategies for polymer electrolyte membrane fuel cells–A review10.1016/j.pecs.2020.100842 ↗
34. Catalytic performance of the Pt/TiO2 catalysts in reverse water gas shift reaction: controlled product selectivity and a mechanism study10.1016/j.cattod.2016.03.020 ↗
35. Analysis of reaction kinetics for carbon monoxide and carbon dioxide on polycrystalline platinum relative to fuel cell operation10.1021/ie950580m ↗
36. Main degradation mechanisms of polymer electrolyte membrane fuel cell stacks–Mechanisms, influencing factors, consequences, and mitigation strategies10.1016/j.ijhydene.2023.06.215 ↗
37. Poisoning of proton exchange membrane fuel cells by contaminants and impurities: review of mechanisms, effects, and mitigation strategies10.1016/j.jpowsour.2019.03.097 ↗
38. Analysing carbon deposition on Ni/YSZ anode tested in an solid oxide fuel cell (SOFC)
39. Effect of carbon monoxide on the electrooxidation of hydrogen by tungsten carbide10.1016/S0378-7753(01)00987-9 ↗
40. Enhancing carbon monoxide tolerance in low-temperature PEM fuel cells through carbon nitride surface modification10.1021/acsami.4c15487 ↗
41. The role of electronic properties of Pt and Pt alloys for enhanced reformate electro-oxidation in polymer electrolyte membrane fuel cells10.1016/j.electacta.2013.06.026 ↗
42. Effect of the mesopores of carbon supports on the CO tolerance of Pt2Ru3 polymer electrolyte fuel cell anode catalyst10.1016/j.ijhydene.2016.05.272 ↗
43. Highly CO tolerant PtRu/PtNi/C catalyst for polymer electrolyte membrane fuel cell10.1039/C6RA28198B ↗
44. Incorporation of platinum and gold partially reduced graphene oxide into polymer electrolyte membrane fuel cells for increased output power and carbon monoxide tolerance10.1557/adv.2016.235 ↗
45. New non-platinum Ir–V–Mo electro-catalyst, catalytic activity and CO tolerance in hydrogen oxidation reaction10.1016/j.ijhydene.2012.09.165 ↗
46. Single-atom catalysts for proton exchange membrane fuel cell: anode anti-poisoning & characterization technology10.1016/j.electacta.2023.142120 ↗
47. High performance platinum single atom electrocatalyst for oxygen reduction reaction
48. Pt single atoms on CrN nanoparticles deliver outstanding activity and CO tolerance in the hydrogen oxidation reaction
49. Tackling CO poisoning with single-atom alloy catalysts10.1021/jacs.6b03339 ↗
50. “One stone three birds” of a synergetic effect between Pt single atoms and clusters makes an ideal anode catalyst for fuel cells10.1039/D3TA01313H ↗
51. Carbon monoxide powered fuel cell towards H2-onboard purification
52. Proton exchange membrane fuel cells powered with both CO and H2
53. Single atom sites as CO scavenger to allow for crude hydrogen usage in PEMFC
54. CO‐tolerant PEMFC anodes enabled by synergistic catalysis between iridium single‐atom sites and nanoparticles10.1002/anie.202110900 ↗
55. 2025
56. 2024
57. 2025
58. Review of polybed pressure swing adsorption for hydrogen purification10.1016/j.ijhydene.2022.01.147 ↗
59. Liu · 2010
60. A review on the metal hydride based hydrogen purification and separation technology
61. YW, enhancing the hydrogen storage properties of AxBy intermetallic compounds by partial substitution: a short review10.3390/hydrogen1010004 ↗
62. Poisoning-tolerant metal hydride materials and their application for hydrogen separation from CO2/CO containing gas mixtures10.1016/j.ijhydene.2013.05.102 ↗
63. Separation and purification of syngas-derived hydrogen: a comparative evaluation of membrane-and cryogenic-assisted approaches10.1016/j.chemosphere.2022.137420 ↗
64. A novel integrated structure for hydrogen purification using the cryogenic method10.1016/j.jclepro.2020.123872 ↗
65. Key technologies for polymer electrolyte membrane fuel cell systems fueled impure hydrogen10.1016/j.pnsc.2020.08.015 ↗
66. Exsolved NiRu bimetallic nanoparticles induced by Ru doping in LaBaMn1.6Ni0.3Ru0.1O5+δ as a coking resistant anode catalyst layer for direct-methane solid oxide fuel cells10.1016/j.ijhydene.2024.07.358 ↗
67. Sr2Fe1. 5Mo0.4Ti0.1O6-δ perovskite anode for high-efficiency coal utilization in direct carbon solid oxide fuel cells10.1016/j.jpowsour.2022.232562 ↗
68. Understanding the mechanism of carbon deposition on perovskite structured LaCo0.2Fe0.8-yMyO3-δ anodes of solid oxide fuel cells: a first principle study10.1016/j.apsusc.2024.159676 ↗
69. Co-Ru bimetallic nanoparticles/oxygen deficient perovskite oxides as a highly efficient anode catalyst layer for direct-methane solid oxide fuel cells
70. Degradation mechanisms and mitigation strategies of direct methane solid oxide fuel cells10.1016/j.apenergy.2023.122609 ↗
71. The poisoning effect of sulfur-containing impurity gas on a SOFC anode: part I. Dependence on temperature, time, and impurity concentration10.1016/S0167-2738(00)00653-6 ↗
72. A model for hydrogen sulfide poisoning in proton exchange membrane fuel cells10.1016/j.jpowsour.2008.06.082 ↗
73. The impact of impurities on long-term PEMFC performance10.1149/1.3210713 ↗
74. Evaluating sulfur-tolerance of metal/Ce0.80Gd0.20O1.90 co-impregnated La0.20 Sr0.25Ca0.45TiO3 anodes for solid oxide fuel cells10.1016/j.ssi.2020.115254 ↗
75. Mitigation studies of sulfur contaminated electrodes for PEMFC10.1016/j.ijhydene.2014.06.011 ↗
76. Determination of factors governing surface composition and degradation of La0.6Sr0.4Co0.2Fe0.8O3-δ electrode under sulfur-contained air10.1149/2.0091906jes ↗
77. Characterization of sulfur poisoning of Ni–YSZ anodes for solid oxide fuel cells using in situ Raman microspectroscopy10.1016/j.ssi.2007.04.004 ↗
78. Sulfur poisoning of SOFC cathodes10.1149/1.3090169 ↗
79. The influence of water vapor and SO on the durability of solid oxide fuel cell10.1149/1.3205850 ↗
80. Sulfur poisoning on La0.6Sr0.4Co0.2Fe0.8O3 cathode for SOFCs10.1149/2.059111jes ↗
81. Atomic-resolution analysis of degradation phenomena in SOFCS: a case study of SO2 poisoning in LSM cathodes10.1016/j.ijhydene.2016.05.216 ↗
82. Resisting coking and sulfur poisoning of double perovskite Sr2TiFe0.5Mo0.5O6–δ anode material for solid oxide fuel cells10.1016/j.ijhydene.2017.12.134 ↗
83. Effect of SO poisoning on the electrochemical activity of La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes of solid oxide fuel cells
84. Determination of factors governing surface composition and degradation of La0.6Sr0.4Co0.2Fe0.8O3-δ electrode under sulfur-contained air10.1149/2.0091906jes ↗
85. A review on solid oxide fuel cell durability: latest progress, mechanisms, and study tools
86. Mathematical modeling of solid oxide fuel cells: a review10.1016/j.rser.2010.12.011 ↗
87. Sr-and Mo-deficiency Sr1.95TiMo1−xO6–δ double perovskites as anodes for solidoxide fuel cells using H2S-containing syngas10.1016/j.ijhydene.2020.06.115 ↗
88. Sulfur deposition and poisoning of La0.6Sr0.4Co0.2Fe0.8O3-δ cathode materials of solid oxide fuel cells10.1149/2.0041412jes ↗
89. Huang · 2009 · 197
90. Reviews on the effects of contaminations and research methodologies for PEMFC10.1016/j.ijhydene.2020.06.145 ↗
91. Adsorption and oxidation of sulphur and of sulphur dioxide at the platinum electrode10.1016/S0022-0728(71)80162-6 ↗
92. PEMFC poisoning with H2S: dependence on operating conditions10.1149/1.2780996 ↗
93. Mitigation studies of sulfur contaminated electrodes for PEMFC10.1016/j.ijhydene.2014.06.011 ↗
94. The effect of H2S and CO mixtures on PEMFC performance10.1016/j.ijhydene.2007.06.029 ↗
95. Poisoning mechanism of the CO and H2S mixture on the anode of polymer electrolyte membrane fuel cell10.1002/celc.202300828 ↗
96. Impurity poisoning of SOFCs10.1149/1.3570280 ↗
97. A high-performance and anti-sulfur poisoning oxygen reduction reaction catalysts derive from molybdenum-doping on PtCo alloy nanoparticles surface10.1016/j.electacta.2023.142658 ↗
98. Hydrogen sulfide tolerance of palladium–copper catalysts for PEM fuel cell anode applications10.1016/j.ijhydene.2011.07.126 ↗
99. High CO and sulfur tolerant proton exchange membrane fuel cell anodes enabled by “work along both lines” mechanism of 2, 6-dihydroxymethyl pyridine molecule blocking layer10.1016/j.jcis.2023.09.076 ↗
100. Advanced Ru/Ti4O7 catalyst for tolerating CO and H2S poisoning to hydrogen oxidation reaction10.1016/j.ijhydene.2024.04.031 ↗