Safety and performance implications of lithium plating induced by sub-zero temperature cycling of lithium-ion batteries

Charles Kirchner-Burles, Arthur Fordham, Hamish T. Reid, Michael Johnson, Mark Buckwell, Francesco Iacoviello, Kofi Coke, Rhodri Jervis, Gareth Hinds, Paul R. Shearing, James B. Robinson

Abstract

The operation of lithium-ion cells at sub-zero temperatures can result in the deposition of metallic lithium onto the surface of the negative electrode. The resulting lithium deposits have substantial ramifications for the performance and safety of the cell, with rapid capacity fade and reduced thermal stability both exhibited in cells aged under these conditions. In this study, it is found that extending the cycling temperatures of these cells to sub-zero temperatures results in a change in plating behaviour, with cells cycled at −10 °C exhibiting reversible plating behaviour and cells cycled at −20 °C plating irreversibly instead. Additionally, the nature of the plating is observed to transition from reversible to irreversible with progressive ageing in the cells cycled at −10 °C. Using operando electrochemical analysis such as voltage relaxation and Coulombic efficiency (CE) measurement, characteristics of the degradation are revealed. Electrochemical impedance spectroscopy (EIS) is also employed between cycles to provide information on the changes in internal cell processes due to plating. Ex-situ investigations complement the analysis allowing images of electrode condition to be collected. In-situ X-ray computed tomography further highlights how lithium plating compromises the structural integrity of the internal cell architecture, leading to increased safety concerns. Testing the aged cells with accelerated rate calorimetry also shows that the presence of more strongly reductive metallic lithium within a cell results in lower onset temperatures for self-heating and thermal runaway, plus an increased potential for projectiles during failure. • Degradation and safety of Li-ion cells at low temperatures examined. • Influence of temperature on Li plating on safety explored. • Jelly roll collapse due to Li-plating observed. • Multi-technique characterisation details increased safety risk at low temperatures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. Lithium batteries: status, prospects and future10.1016/j.jpowsour.2009.11.048 ↗
2. Aurbach, D., Zinigrad, E., Cohen, Y. & Teller, H. A Short Review of Failure Mechanisms of Lithium Metal and Lithiated Graphite Anodes in Liquid Electrolyte Solutions.
3. Jaguemont · 2015
4. Challenges and development of lithium-ion batteries for low temperature environments10.1016/j.etran.2021.100145 ↗
5. Degradation diagnostics for lithium ion cells10.1016/j.jpowsour.2016.12.011 ↗
6. Electrode degradation in lithium-ion batteries10.1021/acsnano.9b04365 ↗
7. A review on the key issues of the lithium ion battery degradation among the whole life cycle10.1016/j.etran.2019.100005 ↗
8. Lithium ion battery degradation: what you need to know10.1039/D1CP00359C ↗
9. A review of safety-focused mechanical modeling of commercial lithium-ion batteries10.1016/j.jpowsour.2017.12.034 ↗
10. Tracking the lifecycle of a 21700 cell: a 4D tomography and digital disassembly study10.1149/1945-7111/acf412 ↗
11. A mechanical aging mechanism in lithium-ion batteries10.1149/2.1001410jes ↗
12. Lithium plating behavior in lithium-ion cells10.1149/1.3393860 ↗
13. Understanding undesirable anode lithium plating issues in lithium-ion batteries10.1039/C6RA19482F ↗
14. Lithium plating mechanism, detection, and mitigation in lithium-ion batteries10.1016/j.pecs.2021.100953 ↗
15. Nondestructive detection, characterization, and quantification of lithium plating in commercial lithium-ion batteries10.1016/j.jpowsour.2013.12.060 ↗
16. Mechanical collapse as primary degradation mode in mandrel-free 18650 Li-ion cells operated at 0 °C10.1016/j.jpowsour.2019.226820 ↗
17. Toward a safer battery management system: a critical review on diagnosis and prognosis of battery short circuit10.1016/j.isci.2020.101010 ↗
18. Internal short circuit mechanisms, experimental approaches and detection methods of lithium-ion batteries for electric vehicles: a review10.1016/j.rser.2021.110790 ↗
19. Research status and analysis for battery safety accidents in electric vehicles
20. (Zhengming). Analysis of internal short-circuit in a lithium ion cell10.1016/j.jpowsour.2009.05.002 ↗
21. Thermal runaway triggered by plated lithium on the anode after fast charging10.1021/acsami.9b16589 ↗
22. Low-temperature lithium plating/corrosion hazard in lithium-ion batteries: electrode rippling, variable states of charge, and thermal and nonthermal runaway10.1021/acsaem.0c00130 ↗
23. Investigating lithium-ion battery materials during overcharge-induced thermal runaway: an operando and multi-scale X-ray CT study10.1039/C6CP04251A ↗
24. Mitigating thermal runaway of lithium-ion batteries10.1016/j.joule.2020.02.010 ↗
25. Li plating as unwanted side reaction in commercial Li-ion cells – a review10.1016/j.jpowsour.2018.02.063 ↗
26. A comprehensive review of lithium-ion batteries used in hybrid and electric vehicles at cold temperatures10.1016/j.apenergy.2015.11.034 ↗
27. Aging of lithium-ion batteries10.1016/j.jpowsour.2003.09.008 ↗
28. Lithium plating in a commercial lithium-ion battery - a low-temperature aging study10.1016/j.jpowsour.2014.11.065 ↗
29. Suppression of lithium deposition at sub-zero temperatures on graphite by surface modification10.1016/j.elecom.2011.07.014 ↗
30. Lithium plating on the anode for lithium-ion batteries during long-term low temperature cycling10.1016/j.jpowsour.2020.229312 ↗
31. Cause and mitigation of lithium-ion battery failure—A review
32. Li · 2018
33. Zhao · 2019
34. In situ detection of lithium metal plating on graphite in experimental cells10.1016/j.jpowsour.2015.01.046 ↗
35. Voltage relaxation and impedance spectroscopy as in-operando methods for the detection of lithium plating on graphitic anodes in commercial lithium-ion cells10.1016/j.jpowsour.2015.11.044 ↗
36. Lithium plating in lithium-ion batteries investigated by voltage relaxation and in situ neutron diffraction10.1016/j.jpowsour.2016.12.032 ↗
37. In-Situ detection of lithium plating using high precision coulometry10.1149/2.0621506jes ↗
38. Detecting undesired lithium plating on anodes for lithium-ion batteries – a review on the in-situ methods10.1016/j.apenergy.2021.117386 ↗
39. Lithium plating in a commercial lithium-ion battery – a low-temperature aging study10.1016/j.jpowsour.2014.11.065 ↗
40. Electrochemical stability of copper in lithium-ion battery electrolytes10.1149/1.1393619 ↗
41. Heat generation in lithium-ion batteries with different nominal capacities and chemistries10.1016/j.applthermaleng.2017.07.126 ↗
42. Arrhenius plots for Li-ion battery ageing as a function of temperature, C-rate, and ageing state – an experimental study10.1016/j.jpowsour.2022.232129 ↗
43. Multimodal physics-based aging model for life prediction of Li-Ion batteries10.1149/1.3043429 ↗
44. Main aging mechanisms in Li ion batteries10.1016/j.jpowsour.2005.03.172 ↗
45. The effect of mud cracking on the performance of thick Li-ion electrodes10.1002/batt.202400260 ↗
46. Li-Ion cell operation at low temperatures10.1149/2.047304jes ↗
47. Understanding the role of SEI layer in low-temperature performance of lithium-ion batteries10.1021/acsami.1c23934 ↗
48. Overpotential analysis of graphite-based Li-ion batteries seen from a porous electrode modeling perspective10.1016/j.jpowsour.2021.230345 ↗
49. Minimum lithium plating overpotential control based charging strategy for parallel battery module prevents side reactions10.1016/j.jpowsour.2021.229772 ↗
50. Development of a voltage relaxation model for rapid open-circuit voltage prediction in lithium-ion batteries10.1016/j.jpowsour.2013.12.083 ↗
51. Review—lithium plating detection methods in Li-Ion batteries
52. Stress evolution in lithium-ion composite electrodes during electrochemical cycling and resulting internal pressures on the cell casing10.1149/2.0341514jes ↗
53. Stress and displacement of cylindrical lithium-ion power battery during charging and discharging
54. Virtual unrolling of spirally-wound lithium-ion cells for correlative degradation studies and predictive fault detection10.1039/C9SE00500E ↗
55. Thermal behavior of lithiated graphite with electrolyte in lithium-ion batteries you may also like study of various (‘Super iron’) MFeO 4 compounds in Li salt solutions as potential cathode materials for Li batteries maxim koltypin
56. Thermal runaway caused fire and explosion of lithium ion battery10.1016/j.jpowsour.2012.02.038 ↗
57. Spotnitz, R. & Franklin, J. Abuse Behavior of high-power, lithium-ion Cells.
58. Review on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries
59. Electrolyte decomposition on Li-metal surfaces from first-principles theory10.1063/1.4967810 ↗
60. Failure and hazard characterisation of high-power lithium-ion cells via coupling accelerating rate calorimetry with in-line mass spectrometry, statistical and post-mortem analyses10.1016/j.est.2023.107069 ↗
61. Fleischhammer · 2014
62. Effects of rest time after Li plating on safety behavior—Arc tests with commercial high-energy 18650 Li-ion cells10.1016/j.electacta.2017.02.036 ↗
63. In-operando high-speed tomography of lithium-ion batteries during thermal runaway