Abstract
Abstract Samples of small particle size bismuth and electroplated Ni–Sn alloy were tested as anodes for lithium ion batteries to highlight the effects of volume changes during charge and discharge on the cycling life of the electrodes. Bismuth was used for its relatively “high” potential of Li–Bi alloys formation (0.8–0.6 V) which prevents other components within the electrode from being electrochemically active versus lithium in this potential window. Electrochemical tests have shown that the capacity fade during cycling is largely dependant of the amount of Bi in the electrode. Electroplated Ni–Sn alloys were directly used as anodes and do not need to be reground nor mixed with additives. Different electroplating conditions, leading to different morphology, highlight the leading role of the particle size of the active materials used in the lithium ion cells.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Winn · Mater. Res. Bull. · 1976 · 11 · 55910.1016/0025-5408(76)90239-7 ↗
2. Wittinghamn · Science · 1976 · 192 · 112610.1126/science.192.4244.1126 ↗
3. Py · Can. J. Phys. · 1993 · 61 · 7610.1139/p83-013 ↗
4. Y. Idota, M. Mishima, Y. Miyiaki, T. Kubota, T. Miyasaka, US Patent 5,618,641 (1997).
5. Idota · Science · 1997 · 276 · 139710.1126/science.276.5317.1395 ↗
6. Courtney · J. Electrochem. Soc. · 1997 · 144 · 204510.1149/1.1837740 ↗
7. Courtney · J. Electrochem. Soc. · 1997 · 144 · 294310.1149/1.1837941 ↗
8. Brousse · J. Electrochem Soc. · 1998 · 145 · 110.1149/1.1838201 ↗
9. Yang · Solid State Ionics · 1996 · 90 · 28110.1016/S0167-2738(96)00389-X ↗
10. Wen · J. Electrochem. Soc. · 1980 · 128 · 118110.1149/1.2127590 ↗
11. Crosnier · Ionics · 1999 · 5 · 31110.1007/BF02375855 ↗
12. Devaux · Nanostruct. Mater. · 1997 · 8 · 13710.1016/S0965-9773(97)00012-3 ↗
13. Parkinson · J. Electrodepositor’s Technol. Soc. · 1951 · 27 · 129
14. Schwitzgebel · Ber. Bunsenges. Phys. Chem. · 1997 · 101 · 174210.1002/bbpc.19971011140 ↗
15. Lo · J. Appl. Phys. · 1980 · 51 · 200710.1063/1.327918 ↗