Abstract

Abstract The spherical Li[Ni 1/3 Co 1/3 Mn 1/3 ]O 2 powders with appropriate porosity, small particle size and good particle size distribution were successfully prepared by a slurry spray drying method. The Li[Ni 1/3 Co 1/3 Mn 1/3 ]O 2 powders were characterized by XRD, SEM, ICP, BET, EIS and galvanostatic charge/discharge testing. The material calcined at 950 °C had the best electrochemical performance. Its initial discharge capacity was 188.9 mAh g −1 at the discharge rate of 0.2 C (32 mA g −1 ), and retained 91.4% of the capacity on going from 0.2 to 4 C rate. From the EIS result, it was found that the favorable electrochemical performance of the Li[Ni 1/3 Co 1/3 Mn 1/3 ]O 2 cathode material was primarily attributed to the particular morphology formed by the spray drying process which was favorable for the charge transfer during the deintercalation and intercalation cycling.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Electrical and Thermal Properties of Materials · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Ohzuku · Chem. Lett. · 2001 · 30 · 64210.1246/cl.2001.642 ↗
2. Yabuuchi · J. Power Sources · 2003 · 119–121 · 17110.1016/S0378-7753(03)00173-3 ↗
3. Belharouak · J. Power Sources · 2003 · 123 · 24710.1016/S0378-7753(03)00529-9 ↗
4. Li · J. Power Sources · 2004 · 132 · 15010.1016/j.jpowsour.2004.01.016 ↗
5. Shaju · Electrochim. Acta · 2002 · 48 · 14510.1016/S0013-4686(02)00593-5 ↗
6. Kim · Electrochim. Acta · 2004 · 49 · 93710.1016/j.electacta.2003.10.005 ↗
7. Patoux · Electrochem. Commun. · 2004 · 6 · 76710.1016/j.elecom.2004.05.024 ↗
8. Lee · Electrochim. Acta · 2004 · 50 · 93910.1016/j.electacta.2004.07.038 ↗
9. Myung · Chem. Lett. · 2004 · 33 · 138810.1246/cl.2004.1388 ↗
10. Choi · Electrochem. Solid-Sate Lett. · 2004 · 7 · A36510.1149/1.1792271 ↗
11. Cho · Chem. Lett. · 2004 · 33 · 70410.1246/cl.2004.704 ↗
12. Cho · J. Power Sources · 2005 · 142 · 30610.1016/j.jpowsour.2004.10.016 ↗
13. Park · Chem. Mater. · 2005 · 17 · 610.1021/cm048433e ↗
14. Park · Electrochim. Acta · 2004 · 49 · 55710.1016/j.electacta.2003.09.009 ↗
15. Hwang · Chem. Mater. · 2003 · 15 · 367610.1021/cm030299v ↗
16. Nakahara · J. Power Sources · 2003 · 117 · 13110.1016/S0378-7753(03)00169-1 ↗
17. Wen · J. Power Sources · 2005 · 146 · 67010.1016/j.jpowsour.2005.03.065 ↗
18. Mahdjoub · J. Eur. Ceram. Soc. · 2003 · 23 · 163710.1016/S0955-2219(02)00412-0 ↗
19. Gao · Electrochem. Solid-Sate Lett. · 1998 · 1 · 11710.1149/1.1390656 ↗
20. Yabuuchi · J. Electrochem. Soc. · 2005 · 152 · A143410.1149/1.1924227 ↗
21. Shaju · J. Electrochem. Soc. · 2004 · 151 · A133210.1149/1.1775218 ↗
22. Sun · J. Electrochem. Soc. · 2007 · 154 · A16810.1149/1.2422890 ↗
23. Cho · J. Electrochem. Soc. · 1999 · 146 · 357110.1149/1.1392516 ↗