Mitigation of chromium poisoning of cathodes in solid oxide fuel cells employing CuMn1.8O4 spinel coating on metallic interconnect
Source abstract
Abstract
Abstract Chromium poisoning is one of the major reasons for cathode performance degradation in solid oxide fuel cells (SOFCs). To mitigate the effect of Cr-poisoning, a protective coating on the surface of interconnect for suppressing Cr vaporization is necessary. Among the various coating materials, Cu-Mn spinel coating is considered to be a potential candidate due to their good thermal compatibility, high stability and good electronic conductivity at high temperature. In this study, Crofer 22 H meshes with no protective coating, those with commercial CuMn2O4 spinel coating and the ones with lab-developed CuMn1.8O4 spinel coating were investigated. The lab-developed CuMn1.8O4 spinel coating were deposited on Crofer 22 H mesh by electrophoretic deposition and densified by a reduction and re-oxidation process. With these different Crofer 22 H meshes (bare, CuMn2O4-coated, and CuMn1.8O4-coated), anode-supported SOFCs with Sr-doped LaMnO3-based cathode were electrochemically tested at 800 °C for total durations of up to 288 h. Comparing the mitigating effects of the two types of Cu-Mn spinel coatings on Cr-poisoning, it was found that the performance of the denser lab-developed CuMn1.8O4 spinel coating was distinctly better, showing no degradation in the cell electrochemical performance and significantly less Cr deposition near the cathode/electrolyte interface after the test.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Electrocatalysts for Energy Conversion
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Interaction between chromia forming alloy interconnects and air electrode of solid oxide fuel cells10.1016/S0167-2738(97)00247-6 ↗
2. Dependence of SOFC cathode degradation by chromium-containing alloy on compositions of electrodes and electrolytes10.1149/1.1339869 ↗
3. Development of interconnect materials for solid oxide fuel cells10.1016/S0921-5093(02)00736-0 ↗
4. Metallic interconnects for solid oxide fuel cells10.1016/j.msea.2005.02.047 ↗
5. Lowering the temperature of solid oxide fuel cells10.1126/science.1204090 ↗
6. A fundamental study of chromium deposition and poisoning at (La0.8Sr0.2)0.95(Mn1−xCox)O3±δ (0.0≤x≤1.0) cathodes of solid oxide fuel cells10.1016/j.ijhydene.2010.09.087 ↗
7. A review of recent progress in coatings, surface modifications and alloy developments for solid oxide fuel cell ferritic stainless steel interconnects10.1016/j.jpowsour.2009.09.069 ↗
8. Metallic interconnects for solid oxide fuel cell: a review on protective coating and deposition techniques10.1016/j.ijhydene.2016.03.195 ↗
9. Degradation phenomena in the cathode of a solid oxide fuel cell with an alloy separator10.1016/0378-7753(94)02172-Y ↗
10. Chromium vapor species over solid oxide fuel cell interconnect materials and their potential for degradation processes10.1149/1.1837264 ↗
11. Chromium vaporization of bare and of coated iron–chromium alloys at 1073 K10.1016/j.ssi.2006.12.010 ↗
12. Effect of cathode and electrolyte transport properties on chromium poisoning in solid oxide fuel cells10.1016/j.ijhydene.2006.08.005 ↗
13. Roles of humidity and cathodic current in chromium poisoning of Sr-doped LaMnO3-based cathodes in solid oxide fuel cells10.1016/j.jpowsour.2017.06.005 ↗
14. A comparative investigation of chromium deposition at air electrodes of solid oxide fuel cells10.1016/S0955-2219(01)00280-1 ↗
15. Chromium deposition and poisoning of cathodes of solid oxide fuel cells–a review10.1016/j.ijhydene.2013.10.042 ↗
16. Chromium poisoning and degradation at (La,Sr)MnO3 and (La,Sr)FeO3 cathodes for solid oxide fuel cells10.1149/1.3322103 ↗
17. Correlation between degradation of cathode performance and chromium concentration in (La,Sr)MnO3 cathode10.1016/j.ssi.2012.02.048 ↗
18. The effect of chromium oxyhydroxide on solid oxide fuel cells10.1149/1.3266930 ↗
19. Recent results in Jülich solid oxide fuel cell technology development10.1016/j.jpowsour.2013.04.110 ↗
20. Degradation of anode supported cell (ASC) performance by Cr-poisoning10.1016/j.jpowsour.2010.10.033 ↗
21. Formation of chromium containing impurities in (La,Sr)MnO3 solid-oxide-fuel-cell cathodes under stack operating conditions and its effect on performance10.1016/j.ceramint.2016.03.010 ↗
22. Effect of humidity and cathodic current on chromium poisoning of Sr-doped LaMnO3-based cathode in anode-supported solid oxide fuel cells10.1149/07542.0061ecst ↗
23. Chromium poisoning effects on performance of (La,Sr)MnO3-based cathode in anode-supported solid oxide fuel cells10.1149/2.0441707jes ↗
24. Chromium poisoning of cathodes in solid oxide fuel cells and its mitigation employing CuMn1.8O4 spinel coatings on interconnects10.1149/07801.1665ecst ↗
25. Development of high strength ferritic steel for interconnect application in SOFCs10.1016/j.jpowsour.2007.12.028 ↗
26. Effect of Laves phase strengthening on the mechanical properties of high Cr ferritic steels for solid oxide fuel cell interconnect application10.1016/j.msea.2011.03.112 ↗
27. The effect of dual atmosphere conditions on the corrosion of Sandvik Sanergy HT10.1016/j.ijhydene.2011.10.096 ↗
28. Evaluation of Fe-Cr alloys as interconnects for reduced operation temperature SOFCs10.1149/1.1539498 ↗
29. Structure and conductivity of thermally grown scales on ferritic Fe-Cr-Mn steel for SOFC interconnect applications10.1149/1.1797031 ↗
30. Chromium vaporization from high-temperature alloys I. Chromia-forming steels and the influence of outer oxide layers10.1149/1.2434690 ↗
31. Evaluation of the oxidation and Cr evaporation properties of selected FeCr alloys used as SOFC interconnects10.1016/j.ijhydene.2013.09.044 ↗
32. The effect of temperature on chromium vaporization and oxide scale growth on interconnect steels for Solid Oxide Fuel Cells10.1016/j.jpowsour.2015.04.040 ↗
33. Thermal growth and performance of manganese cobaltite spinel protection layers on ferritic stainless steel SOFC interconnects10.1149/1.1990462 ↗
34. Mn1.5Co1.5O4 spinel protection layers on ferritic stainless steels for SOFC interconnect applications10.1149/1.1854122 ↗
35. (Mn,Co)3O4 spinel coatings on ferritic stainless steels for SOFC interconnect applications10.1016/j.ijhydene.2006.08.048 ↗
36. Thermally oxidized Mn-Co thin films as protective coatings for SOFC interconnects10.1149/1.3240597 ↗
37. Electrophoretic deposition of (Mn,Co)3O4 spinel coating for solid oxide fuel cell interconnects10.1016/j.jpowsour.2011.05.053 ↗
38. The performance of solid oxide fuel cells with Mn-Co electroplated interconnect as cathode current collector10.1016/j.jpowsour.2008.12.079 ↗
39. Highly dense Mn-Co spinel coating for protection of metallic interconnect of solid oxide fuel cells10.1149/2.0541414jes ↗
40. Effect of coating density on oxidation resistance and Cr vaporization from solid oxide fuel cell interconnects10.1016/j.jpowsour.2017.04.023 ↗
41. Electrical conductivity and thermal expansion of spinels at elevated temperatures10.1111/j.1551-2916.2007.01522.x ↗
42. Spinel coatings for UNS 430 stainless steel interconnects10.1016/j.surfcoat.2006.10.011 ↗
43. Evaluation of electrophoretically deposited CuMn1.8O4 spinel coatings on Crofer 22 APU for solid oxide fuel cell interconnects10.1149/1.2975367 ↗
44. (Mn,Cu)3O4-based conductive coatings as effective barriers to high-temperature oxidation of metallic interconnects for solid oxide fuel cells10.1007/s10008-013-2245-6 ↗
45. Evaluating electrophoretically deposited Cu-Mn-O spinel coatings on stainless steel substrates used in solid oxide fuel cell interconnects
46. Development of Cu1.3Mn1.7O4 spinel coating on ferritic stainless steel for solid oxide fuel cell interconnects10.1016/j.jpowsour.2014.10.017 ↗
47. Cu1.3Mn1.7O4 spinel coatings deposited by electrophoretic deposition on Crofer 22 APU substrates for solid oxide fuel cell applications10.1016/j.surfcoat.2016.09.028 ↗
48. Redox anode supported cell performances tested with different cathode materials10.1149/05701.0867ecst ↗
49. Cathode materials for solid oxide fuel cells: a review10.1007/s10008-009-0932-0 ↗
50. Effect of polarization on and implications for characterization of LSM-YSZ composite cathodes10.1149/1.1667792 ↗
51. A mechanistic study on the activation process of (La, Sr)MnO3 electrodes of solid oxide fuel cells10.1016/j.ssi.2006.05.022 ↗
52. Chemical analysis of activation process of LSM thin film electrode10.1149/07801.0701ecst ↗
53. Electrochemical properties of a SOFC cathode in contact with a chromium-containing alloy separator10.1016/S0167-2738(00)00654-8 ↗
54. Deposition of chromium species at Sr-doped LaMnO3 electrodes in solid oxide fuel cells II. Effect on O2 reduction reaction10.1149/1.1393883 ↗
55. Chromium deposition and poisoning in dry and humidified air at (La0.8Sr0.2)0.9MnO3+δ cathodes of solid oxide fuel cells10.1016/j.ijhydene.2009.12.185 ↗
56. Microstructural degradation of (La,Sr)MnO3/YSZ cathodes in solid oxide fuel cells with uncoated E-brite interconnects10.1149/1.3515073 ↗
57. A fundamental study of chromium deposition on solid oxide fuel cell cathode materials10.1016/j.jpowsour.2006.02.017 ↗
58. Chromium transport by solid state diffusion on solid oxide fuel cell cathode10.1016/j.jpowsour.2010.06.017 ↗
59. Chromium deposition and poisoning at La0.6Sr0.4Co0.2Fe0.8O3−δ oxygen electrodes of solid oxide electrolysis cells10.1039/C4CP05110F ↗