journal article·2006-10

Pt/SiO2 catalyst as an addition to Nafion/PTFE self-humidifying composite membrane

L. Wang, D.M. Xing, Y.H. Liu, Y.H. Cai, Z.-G. Shao, Y.F. Zhai, H.X. Zhong, B.L. Yi, H.M. Zhang

Journal of Power Sources· Volume 161· Issue 1
Publisher page

Abstract

Abstract A novel self-humidifying reinforced composite membrane for the proton exchange membrane fuel cell (PEMFC) was developed. Pt/SiO 2 catalyst particles were dispersed uniformly into the Nafion resin, and then Pt–SiO 2 /Nafion/PTFE reinforced composite membrane was prepared using solution-cast method. Compared with the performance of the fuel cell with commercial Nafion ® NRE-212 membrane, the cell performance with the self-humidifying composite membrane was obviously improved under both humidified and dry conditions at 80–120 °C. The self-humidifying composite membrane could minimize membrane conductivity loss under dry conditions due to the presence of catalyst and hydrophilic Pt/SiO 2 particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Kong · J. Power Sources · 2002 · 108 · 18510.1016/S0378-7753(02)00028-9 ↗
2. Springer · 1991 · 209
3. Liu · J. Electrochem. Soc. · 2005 · 152 · A116510.1149/1.1904988 ↗
4. Healy · Fuel Cells · 2005 · 5 · 30210.1002/fuce.200400050 ↗
5. Alberti · J. Membr. Sci. · 2001 · 185 · 7310.1016/S0376-7388(00)00635-9 ↗
6. Yang · J. Power Sources · 2001 · 103 · 110.1016/S0378-7753(01)00812-6 ↗
7. Costamagna · Electrochim. Acta · 2002 · 47 · 102310.1016/S0013-4686(01)00829-5 ↗
8. Costamagna · Electrochim. Acta · 2002 · 47 · 102310.1016/S0013-4686(01)00829-5 ↗
9. Kim · Electrochim. Acta · 2004 · 50 · 64510.1016/j.electacta.2003.12.079 ↗
10. W.G. Grot, G. Rajendran, U.S. Patent 5, 919,583 (1999).
11. Sacca · J. Power Sources · 2005 · 152 · 1610.1016/j.jpowsour.2004.12.053 ↗
12. Si · J. Electrochem. Soc. · 2004 · 151 · A62310.1149/1.1651527 ↗
13. Watanabe · J. Electrochem. Soc. · 1996 · 143 · 384710.1149/1.1837307 ↗
14. Watanabe · J. Phys. Chem. B · 1998 · 192 · 312910.1021/jp973477e ↗
15. Uchida · J. Electrochem. Soc. · 2002 · 149 · A68210.1149/1.1471539 ↗
16. Ramani · J. Membr. Sci. · 2004 · 232 · 3110.1016/j.memsci.2003.11.016 ↗
17. Watanabe · J. Electroanal. Chem. · 1994 · 375 · 41510.1016/0022-0728(94)03619-5 ↗
18. Lee · Electrochim. Acta · 2004 · 50 · 76110.1016/j.electacta.2004.01.123 ↗
19. Liu · J. Power Sources · 2003 · 124 · 8110.1016/S0378-7753(03)00616-5 ↗
20. Xing · Electochem. Solid-State Lett. · 2004 · 7 · A31510.1149/1.1792274 ↗
21. Yang · J. Power Sources · 2002 · 106 · 32810.1016/S0378-7753(01)01025-4 ↗
22. Kwak · J. Power Sources · 2003 · 118 · 20010.1016/S0378-7753(03)00094-6 ↗
23. Zhu · Electochem. Solid-State Lett. · 2006 · 9 · A4910.1149/1.2142154 ↗
24. Liu · J. Power Sources · 2005 · 139 · 7310.1016/j.jpowsour.2004.07.012 ↗
25. Yu · Phys. Chem. Chem. Phys. · 2004 · 6 · 110.1016/j.chemphys.2004.06.047 ↗
26. Radmilovic · J. Catal. · 1995 · 154 · 9810.1006/jcat.1995.1151 ↗
27. Swanson · 1953 · vol. I
28. Liu · J. Membr. Sci. · 2003 · 212 · 21310.1016/S0376-7388(02)00503-3 ↗