journal article·2015-01

Electrochemical properties of non-nano-silicon negative electrodes prepared with a polyimide binder

Satoshi Uchida, Megumi Mihashi, Masaki Yamagata, Masashi Ishikawa

Publisher page

Abstract

Abstract We successfully improved the cycle stability of a silicon (Si) negative electrode that consisted of untreated, conventional micro-sized Si particles by applying polyimide (PI) with a low breaking elongation percentage and a high tensile strength as a binder. The strong adhesion of the PI binder suppresses the collapse of the Si negative electrode undergoing the expansion/contraction of Si particles during lithiation/delithiation so that the PI-Si electrode maintains a discharge capacity of 800 mAh g −1 during 195 cycles at a current density of 800 mA g −1 . The electrodes prepared in this study contain a PI binder of 15 wt.% to maintain the electrode structure. Such a comparatively large amount of PI binder may prevent Li-ion access into Si particles. Nevertheless, the present Si negative electrode with sufficient electronic conductivity maintains a discharge capacity of 800 mAh g −1 during 167 cycles even at a high rate (1600 mA g −1 ). Perhaps the PI binder does not hinder Li-ion access to Si particles. The cell containing a highly porous polyolefin film coated with ceramic as a separator for a facile supply of Li ion from a bulk electrolyte shows excellent cycle stability and maintains a discharge capacity of 800 mAh g −1 during 300 cycles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Karden · J. Power Sources · 2007 · 168 · 210.1016/j.jpowsour.2006.10.090 ↗
3. Aurbach · Electrochim. Acta · 1999 · 45 · 6710.1016/S0013-4686(99)00194-2 ↗
4. Huggins · J. Power Sources · 1999 · 81-82 · 1310.1016/S0378-7753(99)00124-X ↗
5. Boukamp · J. Electrochem. Soc. · 1981 · 128 · 72510.1149/1.2127495 ↗
6. Beaulieu · Solid-State Lett. · 2001 · 4 · A13410.1149/1.1388178 ↗
7. Oumellal · J. Mater. Chem. · 2011 · 21 · 620110.1039/c1jm10213c ↗
8. Ryu · Solid-State Lett. · 2004 · 7 · A30610.1149/1.1792242 ↗
9. Pal · ECS Trans. · 2012 · 41 · 8710.1149/1.3687394 ↗
10. Kim · Angew. Chem. Int. Ed. · 2010 · 49 · 214610.1002/anie.200906287 ↗
11. Chan · Nat. Nanotechnol. · 2008 · 3 · 3110.1038/nnano.2007.411 ↗
12. Cui · Nano Lett. · 2009 · 9 · 337010.1021/nl901670t ↗
13. Chan · J. Power Sources · 2009 · 189 · 3410.1016/j.jpowsour.2008.12.047 ↗
14. Komaba · J. Phys. Chem. C · 2011 · 115 · 1348710.1021/jp201691g ↗
15. Kovalenko · Science · 2011 · 334 · 7510.1126/science.1209150 ↗