Synthesis of pure phase disordered LiMn1.45Cr0.1Ni0.45O4 by a post-annealing method
Source abstract
Abstract
A post-annealing strategy at 600 C was used to modify the oxygen deficiency during synthesis of a spinel LiMn1.45Cr0.1Ni0.45O4 cathode for lithium-ion batteries. Structural analyses revealed that postannealing is an effective way to eliminate the impurity phase without changing the Fd3m space group. The substitution of a small amount of Cr leads to better rate performance along with cyclability at room temperature, compared to the commercial LiMn1.5Ni0.5O4. LiMn1.45Cr0.1Ni0.45O4 delivered a reversible capacity of w115, 104, 95 and 40 mAh g 1 at 0.2C, 1C, 2C and 5C, respectively. While commercial LiMn1.5Ni0.5O4 offered a lower reversible capacity of w110, 98, 85 and 20 mAh g 1 at the same C rates. After 125 cycles, about 99% of reversible capacity was retained for the LiMn1.45Cr0.1Ni0.45O4, while about 6% of capacity loss was obtained after 125 cycles for the commercial LiMn1.5Ni0.5O4. Electrochemical impedance spectroscopy measurements revealed that the LiMn1.45Cr0.1Ni0.45O4 had a smaller surface resistance, which may be due to the segregation of Ni from the surface to the bulk.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Semiconductor materials and devices · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Sawa · J. Power Sources · 2001 · 97-98 · 43010.1016/S0378-7753(01)00631-0 ↗
2. Ruffo · Ionics · 2005 · 11 · 21310.1007/BF02430379 ↗
3. Kim · Chem. Mater. · 2004 · 16 · 90610.1021/cm035050s ↗
4. Takahashi · J. Electrochem. Soc. · 2004 · 151 · A17310.1149/1.1633267 ↗
5. Kunduraci · Chem. Mater. · 2006 · 18 · 358510.1021/cm060729s ↗
6. Amdouni · Ionics · 2006 · 12 · 11710.1007/s11581-006-0021-7 ↗
7. 2005 · 101
8. Kim · Electrochem. Solid-State Lett. · 2004 · 7 · A21610.1149/1.1753252 ↗
9. Kunduraci · J. Electrochem. Soc. · 2006 · 153 · A134510.1149/1.2198110 ↗
10. Arunkumar · Electrochim. Acta · 2005 · 50 · 556810.1016/j.electacta.2005.03.033 ↗
11. Zhong · J. Power Sources · 2012 · 205 · 38510.1016/j.jpowsour.2011.12.037 ↗
12. Liu · J. Electrochem. Soc. · 2010 · 157 · A126910.1149/1.3491365 ↗
13. Shin · Electrochem. Commun. · 2011 · 13 · 121310.1016/j.elecom.2011.08.041 ↗
14. Liu · J. Power Sources · 2010 · 195 · 291810.1016/j.jpowsour.2009.11.024 ↗
15. Ma · J. Electrochem. Soc. · 2010 · 157 · A92510.1149/1.3439678 ↗
16. Goodenough · 1963
17. Amdouni · J. Mag. Mater. · 2007 · 309 · 10010.1016/j.jmmm.2006.06.018 ↗
18. Liu · J. Phys. Chem. C · 2009 · 113 · 1507310.1021/jp904276t ↗
19. Kunduraci · J. Power Sources · 2007 · 165 · 35910.1016/j.jpowsour.2006.11.051 ↗
20. Ooms · Solid State Ionics · 2002 · 152 · 14310.1016/S0167-2738(02)00368-5 ↗
21. Liu · J. Electrochem. Soc. · 2009 · 156 · A83310.1149/1.3206590 ↗