A study on electrolyte interactions with graphite anodes exhibiting structures with various amounts of rhombohedral phase
Source abstract
Abstract
Abstract The lithium-ion battery anode performance of graphites with and without high amounts of rhombohedral phase in the structure has been investigated. A main outcome was that in addition to possible graphite bulk structure effects, there are also strong influences of the graphite surface and the graphite “sub-surface” (part of the graphite bulk at the border of the particle near the surface) on the solid electrolyte interphase (SEI) formation process and on the tendency to solvent co-intercalation into graphite. Using transmission electron microscopy with atomic resolution, we indeed could determine unique and also different surface and “sub-surface” morphologies for the two graphites. In case of the graphite without rhombohedral phase, unique convoluted graphene layers could be determined at the prismatic surfaces; in case of the graphite with a high rhombohedral phase content a strongly disordered, approximately 1 nm thick “sub-surface” layer could be determined. The anode performance depends primarily on these surface and “sub-surface” graphite properties and the used electrolytes. The differences in the “sub-surface” layer structure have a most significant influence on the performance in an ethylene carbonate/dimethyl carbonate electrolyte. The differences in surface structure and morphology are considered to have the highest impact in a propylene carbonate/ethylene sulfite-based electrolyte. For ethylene carbonate/diethyl carbonate electrolyte, the performance differences are small so that no strong dependence on surface or “sub-surface” structures could be observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Graphene research and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. O. Volher, G. Nutsch, G. Collin, F. von Sturm, E. Wege, W. Frohs, K.D. Henning, H. von Kienle, M. Voll, P. Kleinschmitt, in: Carbon–Graphite, Ullmann’s Encyclopedia of Industrial Chemistry, sixth ed., Electronic Release, 2002.10.1002/14356007.a05_095 ↗
2. Huang · Solid State Ionics · 1998 · 110 · 17310.1016/S0167-2738(98)00144-1 ↗
3. Guerin · J. Electrochem. Soc. · 1999 · 146 · 366010.1149/1.1392530 ↗
4. Flandrois · Mol. Cryst. Liq. Cryst. · 2000 · 340 · 49310.1080/10587250008025514 ↗
5. S. Flandrois, A. Fevrier, P. Biensan, B. Simon, US Patent No. 5 554 462 (1996).
6. Shi · J. Power Sources · 1997 · 68 · 29110.1016/S0378-7753(96)02562-1 ↗
7. Simon · Mol. Cryst. Liq. Cryst. · 1998 · 310 · 33310.1080/10587259808045358 ↗
8. Simon · J. Power Sources · 1999 · 81-82 · 31210.1016/S0378-7753(99)00211-6 ↗
9. Cao · J. Electrochem. Soc. · 2000 · 147 · 357910.1149/1.1393942 ↗
10. Shi · J. Electrochem. Soc. · 1996 · 143 · 346610.1149/1.1837238 ↗
11. Wrodnigg · J. Electrochem. Soc. · 1999 · 146 · 47010.1149/1.1391630 ↗
12. Besenhard · J. Power Sources · 1995 · 54 · 22810.1016/0378-7753(94)02073-C ↗
13. Winter · J. Electrochem. Soc. · 2000 · 147 · 242710.1149/1.1393548 ↗
14. Buqa · J. Power Sources · 2001 · 97-98 · 12210.1016/S0378-7753(01)00523-7 ↗
15. Buqa · Ionics · 2001 · 6 · 17210.1007/BF02374063 ↗