A way to limit the long-term degradation of solid oxide fuel cell cathode by decorating the surface with K2NiF4-Structure Pr4Ni3O10+δ phase
Source abstract
Abstract
Prolonged annealing of La0.6Sr0.4Co0.2Fe0.8O3-8 (LSCF) at 700 degrees C for 1000 h resulted in phase segregation on the surface in the form of submicron-sized SrO on the grains and micron-sized CoFe2O4 particles near the grain boundaries during electrical conductivity relaxation (ECR) measurements. The presence of segregated particles results in a substantial decrease in the surface exchange coefficient, kchem. To mitigate this issue, the LSCF electrodes underwent a systematic coating process with the K2NiF4-structure Pr4Ni3O10+8 (PNO), while varying the loading content, thickness, and porosity. This is achieved by adjusting the gap between the nozzle exit and LSCF surface, ranging from 2 cm to 9 cm, coupled with the application of ultrasonic vibration of the nozzle chamber operating between 40 kHz and 180 kHz. Optimal surface coverage with a loading content of 0.28 mg cm-2 referred to as PNO5 results in a significant increase in kchem by up to one and a half order of magnitude compared to bare LSCF. The PNO coating effectively suppresses phase segregation during prolonged exposure, resulting in a substantial decrease in degradation. The improved performance is attributed to the optimal surface coverage of coated particulates, which enhances the active sites for oxygen reduction reaction (ORR) and the triple phase boundary (TPB) area. These exceptional characteristics position PNO coated LSCF as a highly promising cathode option for low temperature solid oxide fuel cells (SOFCs).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Impact of fuel cells on hydrogen energy pathways in a sustainable energy economy10.1039/D2SE00923D ↗
2. Solid oxide fuel cell: decade of progress, future perspectives and challenges10.1016/j.ijhydene.2021.06.020 ↗
3. Recent advances, practical challenges, and perspectives of intermediate temperature solid oxide fuel cell cathodes10.1039/D1TA08475E ↗
4. Degradation and recovery of solid oxide fuel cell performance by control of cathode surface acidity: case study – impact of Cr followed by Ca infiltration10.1016/j.jpowsour.2022.232589 ↗
5. Enhanced diffusion barrier layers for avoiding degradation in SOFCs aged for 14000 h during 2 years10.1016/j.jpowsour.2022.232400 ↗
6. Surface chemistry and porosity engineering through etching reveal ultrafast oxygen reduction kinetics below 400 °C in B-site exposed (La,Sr)(Co,Fe)O3 thin-films10.1016/j.jpowsour.2022.230983 ↗
7. An improved oxygen reduction reaction activity and CO2-tolerance of La0.6Sr0.4Co0.2Fe0.8O3-δ achieved by a surface modification with barium cobaltite coatings10.1016/j.jpowsour.2021.230573 ↗
8. Validating the application of semiconductor-ionic conductor in solid oxide fuel cells as electrolyte membrane10.1016/j.jpowsour.2021.229963 ↗
9. Strongly coupled oxygen reservoir enabled highly efficient solid oxide fuel cell cathode operation under harsh conditions10.1016/j.jpowsour.2021.230933 ↗
10. Tailoring cobalt‐free La 0.5 Sr 0.5 FeO 3‐δ cathode with a nonmetal cation‐doping strategy for high‐performance proton‐conducting solid oxide fuel cells10.1002/sus2.79 ↗
11. Nanofibrous La0.7Sr0.3FeO3-δ-SDC cobalt-free composite cathode for proton-conducting solid oxide fuel cell10.1016/j.matlet.2022.133687 ↗
12. Comparison of chromium poisoning between lanthanum strontium manganite and lanthanum strontium ferrite composite cathodes in solid oxide fuel cells10.1016/j.jpowsour.2020.228743 ↗
13. Improving oxygen incorporation rate on (La0.6Sr0.4)0.98FeO3-δ via Pr2Ni1-xCuxO4+δ surface decoration10.1016/j.jpowsour.2020.228035 ↗
14. Defect chemistry and transport properties of perovskite-type oxides La1−xCaxFeO3−δ10.1039/D0TA07508F ↗
15. Understanding the favorable CO2 tolerance of Ca-doped LaFeO3 perovskite cathode for solid oxide fuel cells10.1016/j.jpowsour.2021.230907 ↗
16. Impact of SO2 on the oxygen exchange kinetics of the promising SOFC/SOEC air electrode material La0.8Ca0.2FeO3-δ10.1149/2.0041710jes ↗
17. A review on recent advances and trends in symmetrical electrodes for solid oxide cells10.1016/j.jpowsour.2021.230852 ↗
18. Ab initio investigation of O2 adsorption on Ca-doped LaMnO3 cathodes in solid oxide fuel cells10.1039/C8CP02137F ↗
19. Microwave assisted synthesis of La1−xCaxMnO3 (x = 0, 0.2 and 0.4): structural and capacitance properties10.1016/j.ceramint.2017.08.182 ↗
20. Development of lanthanum strontium cobalt ferrite perovskite electrodes of solid oxide fuel cells – a review10.1016/j.ijhydene.2019.01.212 ↗
21. Coating internal surface of porous electrode for decreasing the ohmic resistance and shifting oxygen reduction reaction pathways in solid oxide fuel cells10.1016/j.jpowsour.2021.229854 ↗
22. Effect of stoichiometry on (La0.6Sr0.4)xCo0.2Fe0.8O3 cathode evolution in solid oxide fuel cells10.1016/j.jpowsour.2014.05.114 ↗
23. From powder properties to fuel cell performance – a holistic approach for SOFC cathode development10.1016/j.ssi.2007.11.037 ↗
24. Effects of surface chemical potentials on cation segregation10.1039/D0TA08850A ↗
25. Mechanism of La0.6Sr0.4Co0.2Fe0.8O3 cathode degradation10.1557/jmr.2012.222 ↗
26. Factors that influence cation segregation at the surfaces of perovskite oxides10.1149/05701.2115ecst ↗
27. Cation size mismatch and charge interactions drive dopant segregation at the surfaces of manganite perovskites10.1021/ja3125349 ↗
28. Investigation of surface Sr segregation in model thin film solid oxide fuel cell perovskite electrodes10.1039/C1EE02762J ↗
29. Suppressed Sr segregation and performance of directly assembled La0.6Sr0.4Co0.2Fe0.8O3-δ oxygen electrode on Y2O3-ZrO2 electrolyte of solid oxide electrolysis cells10.1016/j.jpowsour.2018.02.082 ↗
30. Correlation of time-dependent oxygen surface exchange kinetics with surface chemistry of La0.6Sr0.4Co0.2Fe0.8O3-δ catalysts10.1021/acsami.9b06569 ↗
31. Oxygen reduction and transport on the La1−xSrxCo1−yFeyO3−δ cathode in solid oxide fuel cells: a first-principles study10.1039/c3ta11554b ↗
32. Suppression of Sr surface segregation in La(1-x)Sr(x)Co(1-y)Fe(y)O(3-δ): a first principles study10.1039/C2CP43148C ↗
33. Performance stability and degradation mechanism of La0.6Sr0.4Co0.2Fe0.8O3−δ cathodes under solid oxide fuel cells operation conditions10.1016/j.ijhydene.2014.03.077 ↗
34. Recent progress in nanostructured electrodes for solid oxide fuel cells deposited by spray pyrolysis10.1016/j.jpowsour.2021.230277 ↗
35. Precision surface modification of solid oxide fuel cells via layer-by-layer surface sol–gel deposition10.1039/D2TA00458E ↗
36. A review on infiltration techniques for energy conversion and storage devices: from fundamentals to applications10.1039/D1SE00878A ↗
37. Boosting solid oxide fuel cell performance via electrolyte thickness reduction and cathode infiltration10.1039/D0TA04280C ↗
38. Optimization of electrode-electrolyte interface structure for solid oxide fuel cell cathode10.1016/j.jpowsour.2019.227565 ↗
39. Oxygen surface exchange properties of La0.6Sr0.4Co0.8Fe0.2O3 − δ coated with SmxCe1 − xO2 − δ10.1016/j.jpowsour.2012.07.004 ↗
40. La0.6Sr0.4Co0.2Fe0.8O3 cathodes incorporated with Sm0.2Ce0.8O2 by three different methods for solid oxide fuel cells10.1016/j.jpowsour.2015.07.060 ↗
41. Influence of ionic conductivity of the nano-particulate coating phase on oxygen surface exchange of La0.58Sr0.4Co0.2Fe0.8O3−δ10.1039/C6TA10954C ↗
42. Determination of relevant factors affecting the surface oxygen exchange coefficient of solid oxide fuel cell cathode with ionic conducting oxide coating10.1016/j.ssi.2020.115372 ↗
43. Effect of hetero-structured nano-particulate coating on the oxygen surface exchange properties of La0.6Sr0.4Co0.2Fe0.8O3-δ10.1016/j.ijhydene.2019.01.107 ↗
44. Enhancement of La0.6Sr0.4Co0.2Fe0.8O3-δ durability and surface electrocatalytic activity by La0.85Sr0.15MnO3±δ investigated using a new test electrode platform10.1039/c1ee01188j ↗
45. Enhanced performance of LSCF cathode through surface modification10.1016/j.ijhydene.2012.02.139 ↗
46. Pr4Ni3O10+δ: a new promising oxygen electrode material for solid oxide fuel cells10.1016/j.jpowsour.2016.03.012 ↗
47. Comparison of Pr-based cathodes for IT-SOFCs in the ruddlesden-popper family10.1149/07801.0655ecst ↗
48. Atomistic computer simulation of oxygen ion conduction mechanisms in La2NiO410.1016/j.ssi.2008.04.013 ↗
49. Anisotropic oxygen diffusion in tetragonal La2NiO4+δ: molecular dynamics calculations10.1039/B917118E ↗
50. Oxygen exchange and diffusion coefficients of strontium‐doped lanthanum ferrites by electrical conductivity relaxation10.1149/1.1837531 ↗
51. Reactor flush time correction in relaxation experiments10.1149/1.1337604 ↗
52. Oxygen surface exchange kinetics of erbia-stabilized bismuth oxide10.1007/s10008-010-1168-8 ↗
53. Dispersions of oxide powders in organic liquids10.1007/BF00585744 ↗
54. The thermal degradation kinetics and morphology of poly (vinyl butyral) cast films prepared using different organic solvents10.1063/5.0028453 ↗
55. Enhancing oxygen exchange kinetics of solid oxide fuel cell cathode: unleashing the potential of higher order Ruddlesden-Popper phase surface modification10.1016/j.jpowsour.2023.233607 ↗
56. Stability of La0.6Sr0.4Co0.2Fe0.8O3-δ as SOFC cathode10.1149/2.063210jes ↗
57. Strong performance improvement of La0.6Sr0.4Co0.8Fe0.2O3 − δ SOFC cathodes by electrochemical activation10.1149/1.2034529 ↗
58. Raman spectroscopy study of chromium deposition on La0.6Sr0.4Co0.2Fe0.8O3-δ cathode of solid oxide fuel cells10.1149/2.018406jes ↗
59. A kinetic study of catalytic activity degradation of La0.6Sr0.4Co0.2Fe0.8O3-δ
60. Long-term operation of a La0.58Sr0.4Co0.2Fe0.8O3−δ-membrane for oxygen separation10.1016/j.memsci.2010.01.022 ↗
61. Kinetic decomposition of La0.3Sr0.7CoO3−δ perovskite membranes during oxygen permeation10.1016/S0167-2738(98)00191-X ↗
62. Kinetic demixing and decomposition of oxygen permeable membranes10.1016/j.ssi.2006.03.001 ↗
63. Degradation mechanisms of La – Sr – Co – Fe – O3 SOFC cathodes10.1149/1.2266160 ↗
64. Relationship between cation segregation and the electrochemical oxygen reduction kinetics of La0.6Sr0.4CoO3−δ thin film electrodes10.1149/1.3581114 ↗
65. Evidence for strontium segregation in La0.7Sr0.3MnO3 thin films grown by pulsed laser deposition: consequences for tunnelling junctions10.1016/S0039-6028(02)01546-7 ↗
66. Chemical heterogeneities on La0.6Sr0.4CoO3−δ thin films—correlations to cathode surface activity and stability10.1021/cm203501u ↗
67. Evidence that surface-segregated Sr phases can Be removed in LSCF via ceria pre-infiltration, are less apt to form in SSC
68. A novel core-shell LSCF perovskite structured electrocatalyst with local hetero-interface for solid oxide fuel cells10.1016/j.ijhydene.2020.02.130 ↗
69. La2NiO4+δ infiltration of plasma-sprayed LSCF coating for cathode performance improvement10.1007/s11666-015-0369-1 ↗
70. Influence of annealing at intermediate temperature on oxygen transport kinetics of Pr2NiO4+δ10.1039/C7TA08885J ↗