Abstract

Aqueous zinc-ion battery suffers poor cycling stability due to uneven Zn2+ deposition and serious dendrite growth. To effectively protect the Zn metal anode, diglyme (G2) is added as the co-solvent. Adding G2 can reconstruct the Zn2+ solvation structure and reduce the water molecule content of [Zn(H2O)6]2+ sheath. Theoretical calculations confirm that by adding G2, the triflate group OTF− ion shows greater interaction with Zn, and the water molecules from the [Zn(H2O)6]2+ solvation structure are replaced by OTF− ions. Benefitted from this, an organic-inorganic SEI layer is formed on the Zn anode, which isolates the Zn anode from the bulk electrolyte, and allows/suppresses Zn2+ diffusion. As well, Zn corrosion and side reactions are inhibited in this system. This co-solvent electrolyte system has a high Coulombic efficiency of 99.7%. A long cycling life of 1000 cycles with capacity retention of 80% is demonstrated by Zn//iodine (I2) - Activated Carbon (AC) full cell at room temperature. Even under a low-temperature condition (−18 °C), Zn//I2 - AC full cell shows a long lifespan of 1000 cycles with capacity retention of 65%. This work demonstrates a new direction and unparalleled insight into electrolyte engineering with solvation structure regeneration and SEI player formation for aqueous zinc-ion batteries.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced battery technologies research · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Roadmap for advanced aqueous batteries: from design of materials to applications10.1126/sciadv.aba4098 ↗
2. Recent advances in aqueous zinc-ion batteries10.1021/acsenergylett.8b01426 ↗
3. Recent advances in Zn‐ion batteries10.1002/adfm.201802564 ↗
4. Long cyclic stability of acidic aqueous zinc-ion batteries achieved by atomic layer deposition: the effect of the induced orientation growth of the Zn anode
5. Boosting reversibility and stability of Zn anodes via Manipulation of electrolyte structure and interface with addition of Trace organic molecules
6. Ultrafast zinc–ion–conductor interface toward high‐rate and stable zinc metal batteries10.1002/aenm.202100186 ↗
7. Do zinc dendrites exist in neutral zinc batteries: a developed electrohealing strategy to in situ rescue in‐service batteries10.1002/adma.201903778 ↗
8. Diethyl ether as self-healing electrolyte additive enabled long-life rechargeable aqueous zinc ion batteries10.1016/j.nanoen.2019.05.042 ↗
9. Interfacial Double‐coordination effect Guiding uniform electrodeposition for reversible zinc metal anode10.1002/aenm.202302770 ↗
10. A low-cost separator enables a highly stable zinc anode by accelerating the de-solvation effect10.1016/j.cej.2023.147980 ↗
11. Stability Enhancement of zinc‐ion batteries using Non‐aqueous electrolytes
12. An in‐depth study of Zn metal surface chemistry for advanced aqueous Zn‐ion batteries10.1002/adma.202003021 ↗
13. Electrolyte engineering enables stable Zn-ion deposition for long-cycling life aqueous Zn-ion batteries10.1016/j.ensm.2021.11.003 ↗
14. Strategies of regulating Zn 2+ solvation structures for dendrite-free and side reaction-suppressed zinc-ion batteries10.1039/D1EE03377H ↗
15. Unveiling the X‐ray absorption chemistry of H3. 78V6O13 cathode for aqueous zinc‐ion batteries10.1002/adfm.202307270 ↗
16. Stabilizing zinc anode via a chelation and desolvation electrolyte additive
17. Challenges and strategies on Zn electrodeposition for stable Zn-ion batteries10.1016/j.ensm.2021.04.027 ↗
18. A dual‐functional organic electrolyte additive with regulating Suitable overpotential for building highly reversible aqueous zinc ion batteries
19. Hexaoxacyclooctadecane induced interfacial engineering to achieve dendrite-free Zn ion batteries10.1016/j.ensm.2021.11.015 ↗
20. Electrolyte strategies toward better zinc-ion batteries10.1021/acsenergylett.0c02684 ↗
21. Strategies of regulating Zn 2+ solvation structures for dendrite-free and side reaction-suppressed zinc-ion batteries
22. Concentrated dual-cation electrolyte strategy for aqueous zinc-ion batteries
23. Tuning Zn2+ coordination environment to suppress dendrite formation for high-performance Zn-ion batteries10.1016/j.nanoen.2020.105478 ↗
24. Dendrite-free zinc anode enabled by zinc-chelating chemistry10.1016/j.ensm.2021.06.026 ↗
25. Synergetic modulation on solvation structure and electrode interface enables a highly reversible zinc anode for zinc–iron flow batteries10.1021/acsenergylett.2c00560 ↗
26. Zinc anode-compatible in-situ solid electrolyte interphase via cation solvation modulation10.1038/s41467-019-13436-3 ↗
27. Reshaping the electrolyte structure and interface chemistry for stable aqueous zinc batteries10.1016/j.ensm.2022.02.019 ↗
28. High-donor electrolyte additive enabling stable aqueous zinc-ion batteries10.1016/j.ensm.2022.07.032 ↗
29. Non-concentrated aqueous electrolytes with organic solvent additives for stable zinc batteries
30. Solvation structure design for aqueous Zn metal batteries10.1021/jacs.0c09794 ↗
31. 2-methyl imidazole electrolyte additive enabling ultra-stable Zn anode10.1016/j.cej.2022.139465 ↗
32. Zn metal anodes stabilized by an intrinsically safe, dilute, and hydrous organic electrolyte10.1016/j.ensm.2022.10.043 ↗
33. A thin and uniform fluoride-based artificial interphase for the zinc metal anode enabling reversible Zn/MnO2 batteries10.1021/acsenergylett.1c01249 ↗
34. A Synergistic strategy of organic molecules Introduced a high Zn2+ Flux solid electrolyte interphase for stable aqueous zinc-ion batteries10.1021/acsami.2c12118 ↗
35. Electrolyte design for in situ construction of highly Zn2+‐conductive solid electrolyte interphase to enable high‐performance aqueous Zn‐ion batteries under practical conditions10.1002/adma.202007416 ↗
36. Solid electrolyte interface in zn-based battery systems10.1007/s40820-022-00939-w ↗
37. Diglyme based electrolytes for sodium-ion batteries10.1021/acsaem.8b00360 ↗
38. Origin of electrochemical, structural, and transport properties in nonaqueous zinc electrolytes10.1021/acsami.5b10024 ↗
39. Tuning the electrolyte solvation structure to suppress cathode dissolution, water reactivity, and Zn dendrite growth in zinc‐ion batteries10.1002/adfm.202104281 ↗
40. Dual-function electrolyte additive enabling simultaneous electrode interface and coordination environment regulation for zinc-ion batteries10.1016/j.ensm.2023.03.010 ↗
41. Design of a solid electrolyte interphase for aqueous Zn batteries10.1002/anie.202103390 ↗
42. Zinc anode stabilized by an organic-inorganic hybrid solid electrolyte interphase10.1016/j.ensm.2021.09.021 ↗
43. Fluorinated interphase enables reversible aqueous zinc battery chemistries10.1038/s41565-021-00905-4 ↗
44. Defect‐rich Hierarchical Porous Mn‐Doped CoP Hollow Microspheres Accelerate Polysulfide Conversion10.1002/adfm.202211124 ↗
45. Organic Eutectic salts‐Assisted Direct lithium regeneration for Extremely low state of Health Ni‐rich cathodes10.1002/aenm.202302987 ↗